Abstract

Abstract Before the preparation of Si-Mo-Cr coating, blasting treatment of C/C composites and in-situ grown SiC nanowires were performed. Compared with the coated C/C composites without SiC nanowires, the bonding strength of Si-Mo-Cr coating was increased by 5.7%, and the mass loss per unit area was reduced by 46.39% after 30 thermal cycles between 1600 °C and room temperature. The performance enhancement can be attributed to the improved bonding strength and the alleviation of mismatch of thermal expansion coefficient between C/C substrate and Si-Mo-Cr coating, thereby decreasing the thermal stress during thermal cycles between high and low temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
2. High temperature tensile properties of 2D crossply carbon-carbon composites10.5185/amlett.2010.12189 ↗
3. Structural and compositional analyses of oxidised layers of ZrB2-based UHTCs10.1016/j.jeurceramsoc.2015.07.026 ↗
4. UHTC-carbon fibre composites: preparation, oxyacetylene torch testing and characterization10.1016/j.jeurceramsoc.2012.08.018 ↗
5. Anti-oxidation properties of a BN/SiC/Si3N4-ZrO2-SiO2 multilayer coating for carbon/carbon composites10.1016/j.surfcoat.2015.06.072 ↗
6. Long-term oxidation behavior of carbon/carbon composites with a SiC/B4C-B2O3-SiO2-Al2O3 coating at low and medium temperatures10.1016/j.corsci.2015.02.026 ↗
7. An AlPO4/SiC coating prepared by pulse arc discharge deposition for oxidation protection of carbon/carbon composites10.1016/j.corsci.2013.11.006 ↗
8. In-situ fabrication of ZrB2-SiC/SiC gradient coating on C/C composites10.1016/j.jallcom.2015.05.205 ↗
9. Hafnium carbide protective layer coatings on carbon/carbon composites deposited with a vacuum plasma spray coating method10.1016/j.jeurceramsoc.2016.01.032 ↗
10. Erosion resistance of Mo-Si-Cr coating-modified C/C composites in a wind tunnel at 1873K10.1016/j.jallcom.2014.10.189 ↗
11. Oxidation pre-treatment to improve the mechanical property and oxidation resistance of Si-Mo-Cr coated C/C composites10.1016/j.corsci.2014.02.008 ↗
12. Microstructure and mechanical properties of hot pressed Mo-Cr-Si-Ti in-situ composite, and oxidation behavior with silicide coatings10.1016/j.ijrmhm.2012.12.005 ↗
14. Direct observation of super-plasticity of beta-SiC nanowires at low temperature10.1002/adfm.200700162 ↗
15. Effect of the incorporation of SiC nanowire on mullite/SiC protective coating for carbon/carbon composites10.1016/j.corsci.2016.02.022 ↗
16. Oxidation pre-treatment and electrophoretic deposition of SiC nanowires to improve the thermal shock resistance of SiC coating for C/C composites10.1016/j.jallcom.2015.02.075 ↗
17. Carbon nanotube-toughened interlocking buffer layer to improve the adhesion strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites
18. Arc-jet testing of ultra-high-temperature-ceramics10.1016/j.ast.2009.12.004 ↗
19. Effects of LaB6 addition on arc-jet convectively heated SiC-containing ZrB2-based ultra-high temperature ceramics in high enthalpy supersonic airflows10.1016/j.corsci.2013.06.029 ↗
20. Pre-ablation treatment of carbon/carbon composites to improve the thermal shock resistance for SiC coating under oxyacetylene torch10.1016/j.apsusc.2015.07.161 ↗
21. Oxidation-protective and mechanical properties of SiC nanowire-toughened Si-Mo-Cr composite coating for C/C composites10.1016/j.corsci.2012.01.003 ↗
22. Effect of surface ablation products on the ablation resistance of C/C-SiC composites under oxyacetylene torch10.1016/j.corsci.2012.10.003 ↗
23. Delamination of multilayer thermal barrier coatings10.1016/S0167-6636(99)00016-2 ↗