journal article·2023-08

Comprehensive microstructural characterization and CMAS infiltration resistance of ytterbium disilicate coatings with lamellar and quasi-columnar structures

Haoyu Wang, Zhixin Luo, Luchao Sun, Jie Zhang, Jingyang Wang

Corrosion Science· Volume 221
Publisher page

Abstract

Degradation by CMAS deposits represents a considerable threat to the EBC service life. Current work contributes to understanding the response of Yb 2Si 2O 7 coatings with lamellar and quasi-columnar structures to CMAS attack. It is revealed that the dual-phase structure in APS coating drastically improved the overall coating resistance to CMAS infiltration by enhancing the apatite-forming capability. The amorphous silica in PS-PVD coatings limited the formation of apatite “sealing” layer. With a continuous degradation of sand-phobic morphology, molten CMAS rapidly penetrated inside the entire coating. This study highlights that microstructure modulation of Yb 2Si 2O 7 coating is a promising strategy for CMAS infiltration mitigation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
2. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
3. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
4. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
5. Interactions of water vapor with oxides at elevated temperatures10.1016/j.jpcs.2004.06.044 ↗
6. Yb2Si2O7 Environmental barrier coatings with reduced bond coat oxidation rates via chemical modifications for long life10.1111/jace.15978 ↗
7. Interaction of multicomponent disilicate (Yb0.2Y0.2Lu0.2Sc0.2Gd0.2)2Si2O7 with molten calcia-magnesia-aluminosilicate10.1007/s40145-021-0517-7 ↗
8. CMAS degradation of environmental barrier coatings10.1016/j.surfcoat.2007.06.045 ↗
9. Environmental degradation of high-temperature protective coatings for ceramic-matrix composites in gas-turbine engines10.1038/s41529-019-0075-4 ↗
10. (Ho0.25Lu0.25Yb0.25Eu0.25)2SiO5 high-entropy ceramic with low thermal conductivity, tunable thermal expansion coefficient, and excellent resistance to CMAS corrosion10.1007/s40145-022-0609-z ↗
11. High temperature viscosity of calcium-magnesium-aluminosilicate glass from synthetic sand10.1016/j.scriptamat.2016.07.020 ↗
12. Stability and CMAS resistance of ytterbium-silicate/hafnate EBCs/TBC for SiC composites10.1111/jace.13262 ↗
13. Plasma spray deposition of tri-layer environmental barrier coatings10.1016/j.jeurceramsoc.2014.04.027 ↗
14. Molten silicate reactions with plasma sprayed ytterbium silicate coatings10.1016/j.surfcoat.2015.12.053 ↗
15. Interaction of yttrium disilicate environmental barrier coatings with calcium-magnesium-iron alumino-silicate melts10.1016/j.actamat.2017.12.004 ↗
16. The influence of calcium-magnesium-aluminosilicate deposits on internal stresses in Yb2Si2O7 multilayer environmental barrier coatings10.1016/j.actamat.2015.12.016 ↗
17. Plasma spray–physical vapor deposition toward advanced thermal barrier coatings: a review10.1007/s12598-019-01351-x ↗
18. Columnar-structured thermal barrier coatings (TBCs) by thin film low-pressure plasma spraying (LPPS-TF)10.1007/s11666-010-9549-1 ↗
19. Improved thermal cycling durability of thermal barrier coatings manufactured by PS-PVD10.1007/s11666-013-9971-2 ↗
20. CMAS corrosion and thermal cycle of Al-modified PS-PVD environmental barrier coating10.1016/j.ceramint.2018.06.019 ↗
21. Water vapor corrosion behavior of Yb2SiO5 environmental barrier coatings prepared by plasma spray-physical vapor deposition10.3390/coatings10040392 ↗
22. Investigation of the resistance of open-column-structured PS-PVD TBCs to erosive and high-temperature corrosive attack10.1016/j.surfcoat.2017.05.003 ↗
23. Novel thermal barrier coatings repel and resist molten silicate deposits10.1016/j.scriptamat.2018.12.028 ↗
24. Damage tolerance and extensive plastic deformation of β-Yb2Si2O7 from room to high temperatures10.1111/jace.13702 ↗
25. Equiatomic quaternary (Y1/4Ho1/4Er1/4Yb1/4)2SiO5 silicate: a perspective multifunctional thermal and environmental barrier coating material10.1016/j.scriptamat.2019.04.018 ↗
26. High temperature corrosion of (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 environmental barrier coating material subjected to water vapor and molten calcium-magnesium-aluminosilicate (CMAS)10.1016/j.corsci.2020.108881 ↗
27. Process development and coating characteristics of plasma spray-PVD10.1016/j.surfcoat.2012.08.067 ↗
28. Structure, composition, and defect control during plasma spray deposition of ytterbium silicate coatings10.1007/s10853-015-9358-5 ↗
29. Felsche · 1973 · 99
30. Plasma spray–physical vapor deposition toward advanced thermal barrier coatings: a review10.1007/s12598-019-01351-x ↗
31. Corrosion of RE2Si2O7 (RE=Y, Yb, and Lu) environmental barrier coating materials by molten calcium-magnesium-alumino-silicate glass at high temperatures10.1016/j.jeurceramsoc.2019.05.036 ↗
32. Silicate deposit degradation of engineered coatings in gas turbines: progress toward models and materials solutions10.1146/annurev-matsci-010917-105000 ↗
33. Enthalpies of formation of lanthanide oxyapatite phases10.1557/JMR.2001.0381 ↗
34. The use of ionization potentials Part 1. Ionic radii of the elements10.1016/0016-7037(52)90004-5 ↗
35. Calcium-magnesium-alumina-silicate (CMAS) delamination mechanisms in EB-PVD thermal barrier coatings10.1016/j.surfcoat.2004.12.029 ↗
36. Corrosion behaviors and mechanisms of ytterbium silicate environmental barrier coatings by molten calcium-magnesium-alumino-silicate melts10.1016/j.corsci.2021.109718 ↗
37. Resistance of pure and mixed rare earth silicates against calcium‐magnesium‐aluminosilicate (CMAS): a comparative study10.1111/jace.17328 ↗
38. Mixed phase ytterbium silicate environmental-barrier coating materials for improved calcium–magnesium–alumino-silicate resistance10.1557/jmr.2020.151 ↗
39. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
40. Gadolinium oxide solubility in molten silicate: dissolution mechanism and stability of Ca2Gd8(SiO4)6O2 and Ca3Gd2(Si3O9)2 silicate phases10.1016/j.jeurceramsoc.2017.02.022 ↗
41. Thermochemical interactions between CMAS and Ca2Y8(SiO4)6O2 apatite environmental barrier coating material10.1016/j.jeurceramsoc.2019.08.040 ↗