Abstract

Microstructure and hot corrosion resistance of four aluminide coatings with different Si contents ranging from 0 at % to 30 at% are studied. Si primarily exists as CrSi 2 and (Cr,Ti) 5Si 3 in the upper zone of Si-modified aluminide coatings; CrSi 2 transforms into Cr 3 Si phase during corrosion process. These silicides hinder the inward diffusion of the corrosive elements, resulting in enhanced corrosion resistance of Si-modified aluminide coatings at 700 °C. Mechanisms of severe corrosion in coatings with Si at 900 °C was disclosed; high content of Si leads to insufficient Al to renovate Al 2O 3 scale, as well as high temperature causes fast depletion of Al.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Novel processing in inert atmosphere and in air to manufacture high-activity slurry aluminide coatings modified by Pt and Pt/Ir10.1002/maco.201206773 ↗
2. Van Aller · US Pat. 1 · 1915 · 155
3. Mechanisms of formation of slurry aluminide coatings from Al and Cr microparticles10.1016/j.surfcoat.2018.11.077 ↗
4. Pack cementation coatings for superalloys: a review of history, theory, and practice10.1115/1.3240078 ↗
5. Preparation and hot corrosion behaviour of two Co modified NiAl coatings on a Ni-based superalloy10.1016/j.corsci.2013.07.008 ↗
6. Progress in coatings for gas turbine airfoils10.1016/S0257-8972(98)00667-7 ↗
7. Brill-Edwards · US Pat. 3 · 1974 · 801
8. The role of silicon in corrosion-resistant high temperature coatings10.1016/0040-6090(82)90578-8 ↗
9. Microstructure and hot corrosion behaviors of two Co modified aluminide coatings on a Ni-based superalloy at 700 degrees C10.1016/j.apsusc.2014.05.043 ↗
10. Chromium and reactive element modified aluminide diffusion coatings on superalloys: environmental testing10.1149/1.2056220 ↗
11. The protection of gas turbine blades: a platinum aluminide diffusion coating10.1108/eb035759 ↗
12. Cyclic oxidation behaviour of Co/Si co-doped beta-NiAl coating on nickel based superalloys10.1016/j.corsci.2018.01.032 ↗
13. The effect of silicon on thermal shock performance of aluminide-thermal barrier coatings10.1016/j.corsci.2013.05.025 ↗
14. Microstructure and hot corrosion behavior of Co-Si modified aluminide coating on nickel based superalloys10.1016/j.corsci.2015.08.011 ↗
15. Oxidation and microstructure evolution of Al-Si coated Ni3Al based single crystal superalloy with high Mo conten10.1016/j.apsusc.2014.11.076 ↗
16. Preparation and structure of Al plus Si codeposited coatings on. Ni-based Superalloys. Rare Metal Materials and Engineering
17. The role of silicon on microstructure and high temperature performance of aluminide coating on superalloy In-738LC10.2320/matertrans.43.2622 ↗
18. The approaches to thin film preparation and TEM observations on slurry Si-modified aluminide coatings. Materials and Corrosion10.1002/maco.200503907 ↗
19. Hot corrosion behaviour of Al-Si coating in mixed sulphate at 1150 degrees C10.1016/j.corsci.2018.11.026 ↗
20. Microstructural evolution of silicon-platinum modified aluminide coatings on superalloy GTD-11110.1016/j.surfcoat.2017.05.019 ↗
21. Comparison of microstructure and oxidation behavior between Pt-free and Pt-modified delta-Ni2Si coatings on Ni-based superalloys10.1016/j.corsci.2015.05.030 ↗
22. Phase fields of nickel silicides obtained by mechanical alloying in the nanocrystalline state10.1063/1.373553 ↗
23. Electrochemical study on hot corrosion of Si-modified aluminide coated In-738LC in Na2SO4–20 wt% NaCl melt at 750 degrees C10.1016/S0010-938X(02)00127-0 ↗
24. Low-activity aluminide coatings for superalloys using a slurry process free of halide activators and chromates10.1016/j.surfcoat.2013.01.033 ↗
25. Advances in coating design for high-performance gas turbines10.1557/mrs2003.194 ↗
26. The role of combustion synthesis in the formation of slurry aluminization10.1016/j.intermet.2013.08.002 ↗
27. Sulphidation behavior of a non harmful water-based Al and Al-Si slurry coating on CM247 superalloy10.1007/s11085-013-9412-0 ↗
28. Raghavan · J. Phase Equilibria Diffus. · 2005 · 26 · 26210.1007/s11669-005-0115-3 ↗
29. Zhao · A Compr. Investig. phase Evol. Al-Si Coat. Prolong. Aging 650 °C · 2021 · 189
30. Liang · 1993
31. Microstructure and oxidation behavior of Al+Si co-deposited coatings on nickel-based superalloys10.1016/j.surfcoat.2014.09.003 ↗
32. The effect of silicon on cyclic oxidation behavior of aluminide coatings on superalloy IN-738LC10.4028/www.scientific.net/MSF.461-464.335 ↗
33. Effect of water vapour on morphology of the Si/Ti-rich phase at the interface between oxide layer and aluminide coating10.1016/j.corsci.2019.108240 ↗
34. Chemical and mechanical stability of air annealed cathodic arc evaporated CrAlON coatings10.1016/j.surfcoat.2018.07.081 ↗
35. S.K. Hasan, M. Mobin, Hot Corrosion Behaviour of Protective Oxide Scales with Sodium Chloride in Chlorine Gas Environment. Corros. (2013). OnePetro, 2013.10.5006/C2013-02125 ↗
36. Experimental and thermodynamic investigations on the chlorine-induced corrosion of HVOF thermal sprayed NiAl coatings and 304 stainless steels at 700 °C10.1016/j.corsci.2018.02.047 ↗
37. Shifler · 2017 · 50770
38. The structure and high temperature corrosion performance of medium-thickness aluminide coatings on nickel-based superalloy GTD-11110.1016/j.corsci.2010.06.026 ↗
39. Evaluation of the hot corrosion protection of coatings for turbine hot section components10.1016/0257-8972(89)90084-4 ↗
40. Hot corrosion behavior of a Cr-modified aluminide coating on a Ni-based superalloy10.1007/s40195-014-0108-5 ↗
41. Identification of hot corrosion resistant MCrAlY based bond coatings for gas turbine engine applications10.1016/S0257-8972(00)01156-7 ↗