journal article·2020-02

Effect of CO2 gas pressure on composition, growth rate, and structure of duplex oxide formed on 9Cr steel at 550 °C

Mohammad Hassan Shirani Bidabadi, Yu Zheng, Abdul Rehman, Liang Yang, Chi Zhang, Hao Chen, Zhi-Gang Yang

Corrosion Science· Volume 163
Publisher page

Abstract

Abstract The oxidation behaviour of F91 in 0.1, 5, and 10 MPa CO2 was studied at 550 °C for 500 h. Previous results on the effect of CO2 pressure were summarised and compared with the results in this study. The oxidation kinetics decreased from 0.1 to 5 MPa and thereafter showed a lower dependence on the pressure (5–10 MPa). The carbon concentration at the oxide–alloy interface increased with time, but with different rates depending on the CO2 pressure. The amorphous carbon layers, and M23C6 carbides were identified in the inner oxide layer in the case of 5 MPa CO2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (77)

Show source-provided references
1. Brun · 2017
2. A review of thermodynamic cycles and working fluids for the conversion of low-grade heat10.1016/j.rser.2010.07.006 ↗
3. The supercritical carbon dioxide power cycle: comparison to other advanced power cycles10.13182/NT06-A3734 ↗
4. Supercritical CO2 Brayton cycles for solar-thermal energy10.1016/j.apenergy.2013.06.020 ↗
5. Materials performance in supercritical Co2 in comparison with atmospheric pressure Co2 and supercritical steam
6. Effect of pressure on the corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature carbon dioxide environments10.1016/j.corsci.2016.06.004 ↗
7. Pint · 2017
8. Initial assessment of Ni-Base alloy performance in 0.1 MPa and supercritical CO210.1007/s11837-015-1661-8 ↗
9. Characterization of chromia scales formed in supercritical carbon dioxide10.1080/09603409.2017.1389371 ↗
10. Corrosion testing of high temperature materials in supercritical carbon dioxide
11. Kishi · 2008
12. Klueh · 2001
13. Corrosion of austenitic and ferritic-martensitic steels exposed to supercritical carbon dioxide10.1016/j.corsci.2011.06.002 ↗
14. The oxidation behaviour of the 9% Cr steel P92in CO2- and H2O-rich gases relevant to oxyfuel environments10.3139/146.110271 ↗
15. Evolution mechanisms of T91 steel in subcritical conditions and role of an internal oxidation zone10.1007/s11085-018-9837-6 ↗
16. Gibbs · 2010
17. Oxidation/corrosion in materials for supercritical CO2 power cycles
18. Corrosion behavior of heat-resistant materials in high-temperature carbon dioxide environment10.1007/s11837-018-2975-0 ↗
19. A study of breakaway oxidation of 9Cr–1Mo steel in a Hot CO2 atmosphere using Raman spectroscopy10.1080/09603409.2017.1389424 ↗
20. Comparative oxidation behaviour of Fe-9Cr steel in CO2 and H2O at 550°C: detailed analysis of the inner oxide layer10.1016/j.corsci.2015.07.032 ↗
21. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe–Cr and Fe–Cr–X alloys10.1007/s11085-010-9215-5 ↗
22. The initiation of breakaway oxidation of Fe-9Cr-1Mo in a high pressure CO2 atmosphere10.1007/BF00659346 ↗
23. The effect of O2 and H2O on oxidation in CO2 at 700°-800°C
24. Effect of pressure on supercritical CO2 compatibility of structural alloys at 750 °C10.1002/maco.201508783 ↗
25. the effect of temperature on the sCO2 compatibility of conventional structural alloys
26. Corrosion of 9Cr steel in CO2 at intermediate temperature I: mechanism of void-induced duplex oxide formation10.1007/s11085-011-9271-5 ↗
27. Sridharan · 2013
28. A microstructural study of the oxidation of Fe-Ni-Cr alloys II. "non-protective" oxide growth
29. Non-steady state carburisation of martensitic 9–12%Cr steels in CO2 rich gases at 550°C10.1016/j.corsci.2014.07.024 ↗
30. Young · 2016
31. Pre-oxidation effect on oxidation behavior of F91 in carbon dioxide at 550 °C10.1007/s11085-018-9850-9 ↗
32. The mechanism of corrosion of Fe-9%Cr alloys in carbon dioxide10.1007/BF00603476 ↗
33. The growth and structure of oxide films formed on Fe in O2 and CO2 at 550°C10.1007/BF00612135 ↗
34. Kinetics of duplex oxide growth on 9Cr steels exposed in CO2: application of dimensional metrology10.1007/s11085-017-9766-9 ↗
35. Transport processes during the growth of oxide films at elevated temperature10.1103/RevModPhys.57.437 ↗
36. Detection of CO 2 in cavities in NiO scales10.1149/1.2403553 ↗
37. The role of metal lattice vacancies in the hightemperature oxidation of nickel10.1016/S0010-938X(72)80013-1 ↗
38. Some observations on void formation in Fe3O4 layers on Fe10.1016/0010-938X(81)90034-2 ↗
39. A model for mild steel oxidation in CO210.1007/BF00610578 ↗
40. Effect of normalization temperature on the creep strength of modified 9Cr-1Mo steel10.1007/s11661-006-0096-9 ↗
41. Optimization of cutting force by exponential model in milling heat-resistant steel F91
42. Corrosion behavior of FBR structural materials in high temperature supercritical carbon dioxide10.1299/jpes.4.252 ↗
43. Compatibility of FBR structural materials with supercritical carbon dioxide
44. Oxidation and carburizing of FBR structural materials in carbon dioxide
45. Breakaway oxidation of 9Cr-1Mo steel in the pressurized carbon dioxide10.2320/jinstmet1952.39.7_718 ↗
46. Effects of silicon on high temperature corrosion of Fe–Cr and Fe–Cr–Ni alloys in carbon dioxide10.1007/s11085-013-9467-y ↗
47. Supercritical CO2 compatibility of structural alloys at 400°–750°C
48. Oxidation of metallic materials in simulated CO2/H2O-rich service environments relevant to an oxyfuel plant10.4028/www.scientific.net/MSF.696.194 ↗
49. Corrosion behavior of different metallic materials in supercritical carbon dioxide at 550°C and 250 bars10.5006/1.3628683 ↗
50. A study of the mechanism of corrosion of some ferritic steels in high-pressure carbon dioxide with the aid of oxygen-18 as a tracer - III. Fe-9% Cr-1% Mo-0.26% Si
51. Corrosion performance of heat-resisting steels and alloys in supercritical carbon dioxide at 650 °C and 15 MPa10.1016/j.energy.2019.03.014 ↗
52. High-temperature oxidation behavior of 9Cr ferritic-steel in carbon dioxide10.2355/isijinternational.54.1379 ↗
53. Corrosion of 9-12Cr ferritic–martensitic steels in high-temperature CO210.1016/j.corsci.2016.01.009 ↗
54. Influence of CO2 purity on the oxidation of a 12Cr ferritic – martensitic steel at 550°C and importance of the initial stage10.3184/096034012X13323581167078 ↗
55. High-temperature oxidation of commercial alloys in supercritical CO2 and related power cycle environments10.1007/s11837-018-2952-7 ↗
56. Selective oxidation of chromium by O2 impurities in CO2 during initial stages of oxidation10.1007/s11085-013-9392-0 ↗
57. Carburisation of ferritic Fe–Cr alloys by low carbon activity gases10.1016/j.corsci.2011.05.013 ↗
58. Oxidation behavior and lifetime prediction of three commercial alloys used in power plants at 550 °C in CO2 environment10.1007/s42243-019-00232-y ↗
59. On the breakaway oxidation of Fe9Cr1Mo steel in high pressure CO210.1016/j.actamat.2017.02.034 ↗
60. Corrosion of 9Cr steel in CO2 at intermediate temperature II: mechanism of carburization10.1007/s11085-011-9272-4 ↗
61. Kubaschewski · 1993
62. High-temperature oxidation behavior of CrMoV, F91 and Mar-M247 superalloys exposed to laboratory air at 550 °C10.1007/s11085-018-9839-4 ↗
63. Raman microspectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
64. A Raman study of the systems Fe3−xCrxO4 and Fe2−xCrxO310.1016/0022-4596(89)90245-4 ↗
65. Microstructural investigation using advanced TEM techniques of inner oxide layers formed on T92 steel in oxyfuel environment10.1016/j.corsci.2018.12.008 ↗
66. Microstructural investigation of protective and non-protective oxides on 11% chromium steel10.1007/s11085-006-9035-9 ↗
67. Morphologies of oxide growth and exfoliation in superheater and reheater tubing of steam boiler10.3184/096034011X12982937656387 ↗
68. BIRKS · 2006
69. Comparative study on high temperature oxidation of T92 steel in dry and wet oxyfuel environments10.1007/s11085-015-9565-0 ↗
70. Impact of oxyfuel atmospheres H2O/CO2/O2 and H2O/CO2 on the oxidation of ferritic–martensitic and austenitic steels10.1016/j.corsci.2011.03.015 ↗
71. Corrosion of 9Cr steel in CO2 at intermediate temperature III: modelling and simulation of void-induced duplex oxide growth10.1007/s11085-011-9273-3 ↗
72. Enhanced oxidation of the 9%Cr steel P91 in water vapour containing environments10.1016/j.corsci.2006.02.002 ↗
73. Scale growth on steels at 1200°C: rationale of rate and morphology10.1179/msc.1984.18.3.127 ↗
74. The formation of multilayer scales on pure metals10.1007/BF00659339 ↗
75. The formation of two-phase layered scales on pure metals10.1007/BF00609944 ↗
76. Anomalous temperature dependence of oxidation kinetics during steam oxidation of ferritic steels in the temperature range 550–650 °C10.1016/j.corsci.2004.01.010 ↗
77. Kinetics of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗