journal article·2019-07

Study on corrosion kinetics of 310H in different simulated MSW combustion environment. The influence of SO2 and H2O on NaCl assisted corrosion

Terrence Wenga, Guanyi Chen, Wenchao Ma, Beibei Yan

Corrosion Science· Volume 154
Publisher page

Abstract

Abstract In this study, the corrosion kinetics of alloy 310H with and without each of NaCl, H2O-vapor, and SO2 under an oxidizing environment at 500 °C was investigated and the corrosion characteristics in each exposure were compared. The contribution of NaCl, H2O, and SO2 to the corrosion rate was calculated and the corrosion mechanisms in each condition were characterized by means of ex-situ and in-situ thermogravimetric mass-gain measurements, SEM/EDS, XRD, XPS, and theoretical calculations. The contribution was in the order of NaCl>H2O > SO2. Corrosion was linear in the absence of SO2 while in the absence of NaCl, corrosion displayed a multi-stage behavior.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · nanoparticles nucleation surface interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. PESTEL analysis of the development of the waste-to-energy incineration industry in China10.1016/j.rser.2017.05.066 ↗
2. Release to the gas phase of metals, S and Cl during combustion of dedicated waste fractions10.1016/j.fuproc.2010.03.013 ↗
3. Investigation into high-temperature corrosion in a large-scale municipal waste-to-energy plant10.1016/j.corsci.2010.07.032 ↗
4. Full-scale experimental investigation of deposition and corrosion of pre-protector and 3rd superheater in a waste incineration plant10.1038/s41598-017-17438-3 ↗
5. Investigation of chloride deposit formation in a 24MWe waste to energy plant10.1016/j.fuel.2014.09.112 ↗
6. Effects of feed composition on boiler corrosion in waste-to-energy plants
7. Chlorine characterization and thermal behavior in MSW and RDF10.1016/j.jhazmat.2010.01.108 ↗
8. Frandsen · 2010
9. Frandsen · 2010
10. Corrosion behavior of pure Cr with a solid NaCl deposit in O2 plus water vapor10.1023/A:1004690518225 ↗
11. Influence of Cr content on the corrosion of Fe–Cr alloys: the synergistic effect of NaCl and water vapor10.1023/A:1023083309041 ↗
12. Studies on the corrosion behavior of Fe-20Cr alloy in NaCl solution spray at 600 °C10.1016/j.corsci.2018.01.033 ↗
13. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
14. Corrosion inhibition of 304 stainless steel by nano-sized Ti/silicone coatings in an environment containing NaCl and water vapor at 400–600 °C10.1023/B:OXID.0000038782.77162.5b ↗
15. Corrosion behavior of a sputtered K38G nanocrystalline coating with a solid NaCl deposit in wet oxygen at 600 to 700 °C10.1023/A:1016072726338 ↗
16. Synergistic effect of nacl and water vapor on the corrosion of 1Cr-11Ni-2W-2Mo-V Steel at 500-700 °C10.1023/A:1018854202982 ↗
17. NaCl induced corrosion of Ti-6Al-4V alloy at high temperature10.1016/j.corsci.2016.04.016 ↗
18. Alkali induced high temperature corrosion of stainless steel: the influence of NaCl, KCl and CaCl210.1007/s11085-012-9293-7 ↗
19. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
20. NaCl-induced hot corrosion of stainless steels10.1016/0025-5416(87)90404-6 ↗
21. Effects of alloying elements on NaCl-induced hot corrosion of stainless steels10.1016/0921-5093(89)90757-0 ↗
22. The hot corrosion of 310 stainless steel with pre-coated NaCl/Na2SO4 mixtures at 750 °C10.1016/j.matchemphys.2004.10.002 ↗
23. Microstructural investigation of the HCl-induced corrosion of the austenitic alloy 310S (52Fe26Cr19Ni) at 500 °C10.1007/s11085-013-9468-x ↗
24. NaCl-induced accelerated oxidation of chromium10.1007/BF00659184 ↗
25. Effect of water vapor on high-temperature corrosion under conditions mimicking biomass firing10.1021/acs.energyfuels.5b01045 ↗
26. The Effect of SO2and NaCl on High Temperature Hot Corrosion10.1149/1.2131463 ↗
27. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700 °C10.1016/S0010-938X(99)00142-0 ↗
28. fireside corrosion of stainless and low alloyed steels in a waste-fired CFB boiler; The effect of adding sulfur to the fuel10.4028/www.scientific.net/MSF.595-598.289 ↗
29. Sulfation of potassium chloride at combustion conditions10.1021/ef990057a ↗
30. KCl-induced high temperature corrosion of the austenitic stainless steel 304L – the influence of SO210.4028/www.scientific.net/MSF.696.224 ↗
31. Influence of SO2 on the oxidation of 304L Steel in O2 + 40%H2O at 600 °C10.1007/s11085-008-9096-z ↗
32. Influence of water vapor and flow rate on the high-temperature oxidation of 304L; effect of chromium oxide hydroxide evaporation10.1023/A:1004642310974 ↗
33. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600 °C10.1016/j.corsci.2005.08.012 ↗
34. Oxidation of Fe–10Cr in O2 and in O2+H2O environment at 600 °C: a microstructural investigation10.1016/j.corsci.2013.06.016 ↗
35. Comparison of potassium chloride and potassium carbonate with respect to their tendency to cause high temperature corrosion of stainless 304L steel10.1016/j.fuproc.2011.12.016 ↗
36. KCl-Induced corrosion of the FeCrAl Alloy Kanthal®AF at 600 °C and the effect of H2O10.1007/s11085-014-9506-3 ↗
37. KCl-Induced Corrosion of a 304-type austenitic stainless steel in O2 and in O2 + H2O environment: the influence of temperature10.1007/s11085-009-9153-2 ↗
38. An ESEM in situ investigation of the influence of H2O on iron oxidation at 500 °C10.1016/j.corsci.2009.05.016 ↗
39. Corrosion behavior of Cr, Fe and Ni based superalloy in molten NaCl10.1016/S1875-5372(14)60044-8 ↗
40. Kinetics of the sulfation of NaCl at combustion conditions10.1021/ie9603225 ↗
41. Corrosion behaviour of various model alloys with NaCl–KCl coating10.1016/j.matchemphys.2005.03.015 ↗
42. A comparative study on the high temperature corrosion of TP347H stainless steel, C22 alloy and laser-cladding C22 coating in molten chloride salts10.1016/j.corsci.2014.03.012 ↗
43. Reaction kinetics of formatton of HCI in municipal refuse incinerators10.1021/i200020a023 ↗
44. Ma · 2010
45. Chromic acid evaporation upon exposure of Cr2O3(s) to H2O(g) and O2(g) – mechanism from first principles10.1016/j.cplett.2003.11.079 ↗