journal article·2022-11

Droplet size dependent localized corrosion evolution of M50 bearing steel in salt water contaminated lubricant oil

Wanjun He, Qunfeng Zeng, Lei Cheng, Jianing Zhu, Zhao Wang, Jian Zhuang, Xunkai Wei

Corrosion Science· Volume 208
Publisher page

Abstract

Corrosion of M50 steel in salt water contaminated lubricant oil (SCO) were systematically studied in combination with settling dynamics of droplet and characterization of localized corrosion area (LCA). Results show that LCA on steel surface existed in two forms: eye-like LCA and isolated outer zone. Larger outer zone was more likely to create and enlarge inner zone inside it. Outer zone actually resulted from larger droplet, because larger droplet had higher approaching velocity in oil, allowing longer duration at stabilization stage. Underlying formation mechanisms of sunken inner zone and bulging outer zone were respectively given as galvanic and uniform corrosion.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. The effect of prior cold rolling on the carbide dissolution, precipitation and dry wear behaviors of M50 bearing steel10.1016/j.triboint.2018.12.031 ↗
2. Evolution of microstructure and mechanical properties during tempering of M50 steel with Bainite/Martensite duplex structure10.1016/j.jmrt.2020.04.075 ↗
3. Correlative atomic scale characterisation of secondary carbides in M50 bearing steel10.1080/14786435.2017.1410290 ↗
4. Improvement of the corrosion property of Cr4Mo4V bearing steel using plasma immersion ion implantation10.1016/S0168-583X(97)00047-5 ↗
5. Structure and corrosion properties of Cr coating deposited on aerospace bearing steel10.1016/j.apsusc.2017.06.099 ↗
6. Failure analysis of an inter-shaft bearing of an aero gas turbine engine10.1007/s11668-015-9933-8 ↗
7. Failure analysis of bearings of aero-engine10.1007/s11668-019-00746-3 ↗
8. Corrosion initiation and propagation on carburized martensitic stainless steel surfaces studied via advanced scanning probe microscopy10.3390/ma12060940 ↗
9. Corrosion assessment and characterization of aerospace-bearing steels in seawater and ester-based lubricants10.5006/0459 ↗
10. Surface-chemical aspects of the rusting of steel surfaces in oil containing an entrained aqueous phase10.1016/0010-938X(69)90023-7 ↗
11. Microstructure modifications and corrosion behaviors of Cr4Mo4V steel treated by high current pulsed electron beam10.1016/j.matchemphys.2010.12.016 ↗
12. Influence of irradiation number of high current pulsed electron beam on the structure and properties of M50 steel10.1016/j.nimb.2010.04.019 ↗
13. Microstructure and corrosion behavior of Cr coating on M50 steel fabricated by electrospark deposition10.1007/s11665-019-04148-2 ↗
14. FIB/SEM study of AA2024 corrosion under a seawater drop, part II10.1016/j.corsci.2011.10.012 ↗
15. The cathodic behaviour of Al-Mn precipitates during atmospheric and saline aqueous corrosion of a sand-cast AM50 alloy10.1016/j.corsci.2014.02.030 ↗
16. Bacterial distribution in SRB biofilm affects MIC pitting of carbon steel studied using FIB-SEM10.1016/j.corsci.2020.108512 ↗
17. Insight into atmospheric pitting corrosion of carbon steel via a dual-beam FIB/SEM system associated with high-resolution TEM10.1016/j.corsci.2019.03.017 ↗
18. Groysman · 2014
19. The growth of the passive film on iron in 0.05 M NaOH studied in situ by Raman micro-spectroscopy and electrochemical polarization. Part I: near-resonance enhancement of the Raman spectra of iron oxide and oxyhydroxide compounds10.1002/jrs.2837 ↗
20. In-situ Raman and X-ray photoelectron spectroscopic studies on the pitting corrosion of modified 9Cr-1Mo steel in neutral chloride solution10.1016/j.apsusc.2017.09.179 ↗
21. Effect of austenitizing temperature on microstructure of M50 steel
22. Carbides in M-50 high speed steel10.1007/BF02917552 ↗
23. Proposal for a methodology based on XRD and SEM-EDS to monitor effects of lime-treatment on clayey soils10.3390/app10072569 ↗
24. Corrosion performance of HVOF and APS thermally sprayed NiTi intermetallic coatings in 3.5% NaCl solution10.1016/j.corsci.2009.11.034 ↗
25. SEM, EDS, EPMA-WDS and EBSD characterization of carbides in HP type heat resistant alloys10.1016/j.matchar.2008.02.001 ↗
26. Surface roughness and the corrosion resistance of 21Cr ferritic stainless steel10.1016/j.corsci.2012.06.031 ↗
27. Influence of surface morphology on corrosion and electronic behavior10.1016/j.actamat.2005.09.017 ↗
28. Influence of surface roughness on the corrosion behaviour of magnesium alloy10.1016/j.matdes.2010.12.016 ↗
29. Effect of surface roughness on corrosion behavior of the superalloy IN718 in simulated marine environment10.1016/j.jallcom.2018.01.042 ↗
30. Nanoscale scanning electrochemical cell microscopy and correlative surface structural analysis to map anodic and cathodic reactions on polycrystalline Zn in acid media10.1149/1945-7111/ab739d ↗
31. Churning power losses of a gearbox with spiral bevel geared transmission10.1016/j.triboint.2018.08.041 ↗
32. Water film drainage between a very viscous oil drop and a mica surface10.1103/PhysRevLett.127.124503 ↗
33. The drainage of thin liquid films between solid surfaces10.1063/1.449693 ↗
34. Butt · 2018
35. A comparative study of localized corrosion and stress corrosion cracking of 13Cr martensitic stainless steel using acoustic emission and X-ray computed tomography10.3390/ma12162569 ↗
36. Effects of secondary-phase formation on the electrochemical performance of a wire arc additive manufactured 420 martensitic stainless steel under different heat treatment conditions10.1007/s11665-021-05936-5 ↗
37. Electrochemical and in-situ SERS study of passive film characteristics and corrosion performance of 9%Cr microcomposite steel in highly alkaline environments
38. Corrosion behaviour of a quenched and partitioned medium carbon steel in 3.5 wt% NaCl solution10.1016/j.corsci.2017.10.027 ↗
39. Effect of ultrasonic surface rolling on microstructure and rolling contact fatigue behavior of 17Cr2Ni2MoVNb steel10.1016/j.surfcoat.2019.03.061 ↗
40. Stress corrosion crack evaluation of super 13Cr tubing in high-temperature and high-pressure gas wells10.1016/j.engfailanal.2018.09.030 ↗
41. Effects of pre-corrosion, water and detergent contamination on rolling contact fatigue10.1051/meca/2020023 ↗
42. Phase-transition-induced one-dimensional amorphous α-Fe2O3/β-FeOOH homojunction for efficient photocatalytic water oxidation10.1117/1.JPE.9.026501 ↗
43. Quantitative analysis of three-dimensional morphology of martensite packets and blocks in iron-carbon-manganese steels10.1016/j.jallcom.2012.02.004 ↗
44. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
45. The morphology and crystallography of lath martensite in alloy steels10.1016/j.actamat.2006.07.009 ↗
46. Influence of refined hierarchical martensitic microstructures on yield strength and impact toughness of ultra-high strength stainless steel10.1016/j.jmst.2020.04.001 ↗
47. Microstructure evolution and mechanical properties of PESR 55Cr17Mo1VN plastic die steel during quenching and tempering treatment10.1007/s42243-021-00689-w ↗
48. Influence of the secondary phase on micro galvanic corrosion of low carbon bainitic steel in NaCl solution10.1016/j.matchar.2018.03.021 ↗
49. Hydrostatic pressure effects on corrosion behavior of X70 pipeline steel in a simulated deep-sea environment10.1016/j.jelechem.2018.05.010 ↗
50. Effect of austenitisation temperature on corrosion resistance properties of dual-phase high-carbon steel10.1007/s10853-019-03859-0 ↗
51. Synergistic effect of Al2O3 inclusion and pearlite on the localized corrosion evolution process of carbon steel in marine environment10.3390/ma11112277 ↗
52. Influence of alloy sulfur content and bulk electrolyte composition on crevice corrosion initiation of austenitic stainless steel10.5006/1.3284838 ↗
53. Influences of thermomechanical conditions on corrosion behavior of low-carbon steels in artificial seawater10.20964/2019.03.65 ↗
54. Corrosion failure analysis of low alloy steel and carbon steel rebar in tropical marine atmospheric environment: Outdoor exposure and indoor test10.1016/j.engfailanal.2021.105720 ↗
55. The pitting to uniform corrosion evolution process promoted by large inclusions in mooring chain steels10.1016/j.matchar.2021.111456 ↗
56. Influence of inclusions on early corrosion development of ultra-low carbon bainitic steel in nacl solution10.5006/1837 ↗
57. Effect of microstructure variation on the corrosion behavior of high-strength low-alloy steel in 3.5wt% NaCl solution10.1007/s12613-015-1113-z ↗
58. Studies of X-65 pipeline steel corrosion in solutions containing carbon dioxide by electrochemical technique
59. Investigating a mechanism for transgranular stress corrosion cracking on buried pipelines in near-neutral pH environments10.5006/1.3278311 ↗
60. Dissolution kinetics of the sulfide-oxide complex inclusion and resulting localized corrosion mechanism of X70 steel in deaerated acidic environment10.1016/j.corsci.2020.108815 ↗
61. Electrochemical corrosion characteristics of type 316L stainless steel in hot concentrated seawater10.1016/j.corsci.2013.12.004 ↗
62. Influence of chromium on the flow-accelerated corrosion behavior of low alloy steels in 3.5% NaCl solution10.1016/j.corsci.2017.04.024 ↗
63. Oil-immersed scanning micropipette contact method enabling long-term corrosion mapping10.1021/acs.analchem.0c02177 ↗