Carburization susceptibility of chromia-forming alloys in high-temperature CO2
Source abstract
Abstract
It is generally believed that when a chromia scale forms in high-temperature CO 2 environments, carbon uptake of alloys is nearly eliminated, thereby preventing carburization and associated degradation of properties. Herein we quantitively assess this notion through careful examination of several chromia-forming Ni-based and Fe-based commercial alloys after long-term (10,000-h) exposures to CO 2 and air at 700 °C. Small but measurable carbon uptake ensued independent of alloy base metal (Ni/Fe), alloy crystal structure (FCC/BCC), and chromia growth rate. The rate for Ni-based alloys was strongly dependent on Si and Mn content, highlighting the need to understand possible long-term effects on mechanical properties.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Materials performance in CO2 and supercritical CO2
2. Brun · 2017
3. Review of supercritical CO2 technologies and systems for power generation
4. Fleming · 2013
5. Mechanisms of breakaway oxidation and application to a chromia-forming steel10.1023/A:1018855914737 ↗
6. Oxidation limited life times of chromia forming ferritic steels10.1002/maco.200303798 ↗
7. Predicting oxidation-limited lifetime of thin-walled components of NiCrW alloy 23010.1007/s11085-016-9653-9 ↗
8. High-temperature materials
9. Young · 2016
10. Effect of pressure and thermal cycling on long-term oxidation in CO2 and supercritical CO210.1007/s11085-020-10004-9 ↗
11. Alloy corrosion by Hot CO2 gases10.1007/s11837-018-2944-7 ↗
12. Volatility of common protective oxides in high-temperature water vapor: current understanding and unanswered questions
13. Calculation of reactive-evaporation rates of chromia10.1007/s11085-008-9091-4 ↗
14. High-temperature oxidation of transient-liquid phase bonded Ni-based alloys in 1 bar and 250 bar carbon dioxide10.1080/09603409.2020.1818046 ↗
15. High-temperature oxidation of commercial alloys in supercritical CO2 and related power cycle environments10.1007/s11837-018-2952-7 ↗
16. High temperature oxidation of Ni alloys in CO2 containing impurities10.1016/j.corsci.2019.05.019 ↗
17. Structural evolution of a Ni alloy surface during high-temperature oxidation10.1007/s11085-017-9821-6 ↗
18. Effects of silicon on high temperature corrosion of Fe–Cr and Fe–Cr–Ni alloys in carbon dioxide10.1007/s11085-013-9467-y ↗
19. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
20. Effect of pressure on the corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature carbon dioxide environments10.1016/j.corsci.2016.06.004 ↗
21. Effect of surface finish on high temperature oxidation of steels in CO2, supercritical CO2 and air10.1007/s11085-019-09938-6 ↗
22. High temperature oxidation of steels in CO2 containing impurities10.1016/j.corsci.2019.108316 ↗
23. Molecular-scale investigation of the oxidation behavior of chromia-forming alloys in high-temperature CO210.1038/s41529-021-00194-1 ↗
24. Carburisation of ferritic Fe–Cr alloys by low carbon activity gases10.1016/j.corsci.2011.05.013 ↗
25. Corrosion of 9Cr steel in CO2 at intermediate temperature ii: mechanism of carburization10.1007/s11085-011-9272-4 ↗
26. Type 304 stainless steel vs flowing CO2 at atmospheric pressure and 1100–1800F10.5006/0010-9312-21.3.84 ↗
27. Corrosion behaviour of Ni-Cr alloys in wet CO2 atmosphere at 700 and 800 °C10.1016/j.corsci.2018.10.029 ↗
28. Alloys SS316 and hastelloy-C276 in supercritical CO2 at high temperature10.1007/s11085-015-9589-5 ↗
29. Water vapor effects on corrosion of Fe–Cr and Fe–Cr–Ni alloys containing silicon in CO2 gas at 818 °C10.1007/s11085-015-9536-5 ↗
30. Effects of silicon and water vapour on corrosion of Fe–20Cr and Fe–20Cr–20Ni Alloys in CO2 at 650 °C10.1007/s11085-016-9681-5 ↗
31. Microstructures of chromia scales grown in CO210.1179/0960340914Z.00000000056 ↗
32. Effects of cerium and manganese on corrosion of Fe–Cr and Fe–Cr–Ni alloys in Ar–20CO2 and Ar–20CO2–20H2O gases at 650 °C10.1016/j.corsci.2015.08.012 ↗
33. Effects of Si, Mn, and water vapour on the microstructure of protective scales grown on Fe–20Cr in CO2 gas10.1080/09603409.2017.1389098 ↗
34. Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650 °C10.1016/j.corsci.2016.07.014 ↗
35. Oxidation behaviour and microstructural stability of alloy 625 during long-term exposure in steam10.1007/s10853-014-8344-7 ↗
36. DFT study of the solubility of hydrogen and carbon in Ni3Nb-D0a and Ni3Nb-D022 systems10.1016/j.jallcom.2014.04.174 ↗
37. Effects of corrosion in supercritical CO2 on the microstructural evolution in 800H Alloy10.1007/s11085-018-9852-7 ↗
38. The carburization behavior of alloy 800HT in high temperature supercritical-CO2
39. Effect of CO2 on the strength and ductility of type 304 stainless steel at elevated temperatures10.5006/0010-9312-19.5.157 ↗
40. Creep of MARBN-type 9Cr martensitic steel in gaseous CO2 environment10.1016/j.msea.2021.141996 ↗
41. Corrosion and creep behavior of a Ni-base alloy in supercritical-carbon dioxide environment at 650° C10.1016/j.corsci.2020.108843 ↗
42. Understanding the stress corrosion cracking growth mechanism of a cold worked alumina-forming austenitic steel in supercritical carbon dioxide10.1016/j.corsci.2022.110179 ↗