journal article·2022-04

Study on oxidation resistance and oxidative damage mechanism of SiBCN-Ta4HfC5 composite ceramics

Bingzhu Wang, Daxin Li, Zhihua Yang, Dechang Jia, Jingyi Guan, Delong Cai, Peigang He, Xiaoming Duan, Yu Zhou

Corrosion Science· Volume 197
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. D.X. Li, D.C. Jia, Z.H. Yang, Y. Zhou, Principles, design, structure and properties of ceramics for microwave absorption or transmission at high-temperatures. Int. Mater. Rev., 〈http://10.1080/09506608.2021.1941716〉.
2. A silicoboron carbonitride ceramic stable to 2000 °C10.1038/382796a0 ↗
3. Metastable Si-B-C-N ceramics and their matrix composites developed by inorganic route based on mechanical alloying: fabrication, microstructures, properties and their relevant basic scientific issues10.1016/j.pmatsci.2018.05.006 ↗
4. Preparation of polymer-derived Si–B–C–N monoliths by spark plasma sintering technique10.1016/j.jeurceramsoc.2014.11.021 ↗
5. Simple and low-cost synthetic route for SiBCN ceramic powder from a boron modified cyclotrisilazane10.1111/jace.15921 ↗
6. Crystallization and creep behavior of Si–B–C–N ceramics10.1016/j.actamat.2005.06.011 ↗
7. Characterization of free carbon in the as-thermolyzed Si-B-C-N ceramic from a polyorganoborosilazane precursor10.1007/s40145-013-0079-4 ↗
8. Polymer-derived SiBCN ceramic pressure sensor with excellent sensing performance10.1007/s40145-020-0377-6 ↗
9. Microstructure and mechanical properties of 3D Cf/SiBCN composites fabricated by polymer infiltration and pyrolysis10.1007/s40145-020-0414-5 ↗
10. Dense amorphous Si2BC1–4N monoliths resistant to high-temperature oxidation for hypersonic vehicle10.1016/j.corsci.2019.108231 ↗
11. Progress of a novel non-oxide Si-B-C-N ceramic and its matrix composites10.1007/s40145-012-0017-x ↗
12. Mechanical and dielectric properties of SiCf/BN/SiBCN composites via different synthesis technologies10.1016/j.jeurceramsoc.2019.05.033 ↗
13. Ceramic nanocomposites from tailormade preceramic polymers10.3390/nano5020468 ↗
14. Effects of high pressure on the low-temperature sintering of dense amorphous SiBCN monoliths10.1016/j.jeurceramsoc.2018.04.061 ↗
15. High-temperature oxidation resistance of dense amorphous boron-rich SiBCN monoliths10.1016/j.corsci.2019.06.001 ↗
16. Crystallization and microstructural evolution process from the mechanically alloyed amorphous Si-B-C-N powder to the hot-pressed nano SiC/BN(C) ceramic10.1007/s10853-012-6683-9 ↗
17. 2Si-B-3C-N ceramics prepared by mechanical alloying and hot-pressing consolidation
18. Enhanced mechanical properties, thermal shock resistance and ablation resistance of Si2BC3N ceramics with nano ZrB2 addition10.1016/j.jeurceramsoc.2018.12.005 ↗
19. Fabrication and microstructures of functional gradient SiBCN-Nb composite by hot pressing10.1016/j.matchar.2016.02.014 ↗
20. Effects of Zr and chopped C fiber on microstructure and mechanical properties of SiBCN ceramics10.1007/s11431-020-1657-7 ↗
21. Synthesis and characteristic of SiBCN/HfN ceramics with high temperature oxidation resistance10.1016/j.jallcom.2016.06.250 ↗
22. Enhanced ablation resistance of HfB2-HfC/SiBCN ceramics under an oxyacetylene torch environment10.1016/j.corsci.2021.109509 ↗
23. Effects of TaC addition on microstructure and mechanical properties of SiBCN composite ceramics10.1016/j.ceramint.2019.07.231 ↗
24. Creep deformation behavior during densification of ZrB2-SiBCN ceramics with ZrO2 additive10.1007/s40145-020-0393-6 ↗
25. Oxidation behavior of SiBCN-Zr composites at 1500 °C prepared by reactive spark plasma sintering10.1016/j.corsci.2018.01.003 ↗
26. Influence of sol-gel derived ZrB2 additions on microstructure and mechanical properties of SiBCN composites10.1016/j.ceramint.2016.12.083 ↗
27. Thermal ablation behavior of SiBCN-Zr composites prepared by reactive spark plasma sintering10.1016/j.ceramint.2017.03.068 ↗
28. Oxidation mechanism and kinetics of SiBCN/HfC ceramic composites at high temperatures10.1016/j.jmrt.2019.12.060 ↗
29. Investigations of the high-melting carbide systems connected with problem of the carbon melting
30. Melting point in systems ZrC-HfC, TaC-ZrC, TaC-HfC10.1007/BF00773385 ↗
31. Synthesis of highly dispersed super-refractory tantalum-zirconium carbide Ta4ZrC5 and tantalum-hafnium carbide Ta4HfC5 via sol-gel technology10.1134/S0036023611110258 ↗
32. Reduced-temperature processing and consolidation of ultra-refractory Ta4HfC510.1016/j.ijrmhm.2013.04.018 ↗
33. Polymer-derived Ta4HfC5 nanoscale ultrahigh-temperature ceramics: synthesis, microstructure and properties10.1016/j.jeurceramsoc.2018.10.012 ↗
34. High temperature ablation behavior of pressureless sintered Ta0.8Hf0.2C based ultra-high temperature ceramics10.1016/j.jeurceramsoc.2019.11.043 ↗
35. Pressureless densification, microstructure tailoring and properties of Ta0.8Hf0.2C-based composites10.1016/j.jeurceramsoc.2017.10.025 ↗
36. Solid-solution effects on the high-temperature oxidation behavior of polymer-derived (Hf,Ta)C/SiC and (Hf,Ti)C/SiC ceramic nanocomposites10.1002/adem.201800879 ↗
37. Microstructural evolution and mechanical properties of in situ nano Ta4HfC5 reinforced SiBCN composite ceramics10.1007/s40145-020-0410-9 ↗
38. Experimental investigation of passive/active oxidation behavior of SiC based ceramic thermal protection materials exposed to high enthalpy plasma10.1016/j.jeurceramsoc.2012.09.002 ↗