journal article·2021-11

Twinning behavior and hydrogen embrittlement of a pre-strained twinning-induced plasticity (TWIP) steel

Cheng Zhang, Hang Yu, Huihui Zhi, Stoichko Antonov, Yanjing Su

Corrosion Science· Volume 192
Publisher page

Abstract

Abstract The twinning behavior and hydrogen embrittlement (HE) of a twinning-induced plasticity (TWIP) steel were investigated for different pre-strains at different strain rates. The lower pre-strain rate led to thinner twins and higher twin volume fraction. The influence of the twin characteristics on HE sensitivity was analyzed from statistical data on the evolution of surface crack characteristics during secondary straining period after cathodic hydrogen charging. Based on the ratio of crack initiation sites caused by the intersection of twins and grain boundaries, it was found that thinner twins in twin bundles of similar thickness promoted the generation of hydrogen-induced cracks (HICs).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
2. Outstanding tensile properties and their origins in twinning-induced plasticity (TWIP) steels with gradient substructures10.3390/ma13051184 ↗
3. On the relationship between the twin internal structure and the work-hardening rate of TWIP steels10.1016/j.scriptamat.2010.07.016 ↗
4. An alternative model for the strain hardening of FCC alloys that twin, validated for twinning-induced plasticity steel10.1016/j.scriptamat.2008.10.035 ↗
5. Internal stresses and the mechanism of work hardening in twinning-induced plasticity steels10.1016/j.scriptamat.2012.02.019 ↗
6. Stacking fault energy and deformation mechanisms in Fe-xMn-0.6C-yAl TWIP steel10.1016/j.msea.2016.08.106 ↗
7. Effect of stacking-fault energy on deformation twin thickness in Cu–Al alloys10.1016/j.scriptamat.2008.10.005 ↗
8. Negative to positive transition of strain rate sensitivity in Fe-22Mn-0.6C-x(Al) twinning-induced plasticity steels10.1016/j.msea.2017.02.014 ↗
9. Comparison of twinning evolution with work hardening ability in twinning-induced plasticity steel under different strain rates10.1016/j.msea.2014.11.031 ↗
10. Effect of hydrogen content on the embrittlement in a Fe–Mn–C twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
11. Hydrogen embrittlement in a Fe–Mn–C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
12. Hydrogen transport in solution-treated and pre-strained austenitic stainless steels and its role in hydrogen-enhanced fatigue crack growth10.1016/j.ijhydene.2008.11.018 ↗
13. Hydrogen-induced cracking at grain and twin boundaries in an Fe–Mn–C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
14. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
15. Effect of hydrogen on nanomechanical properties in Fe-22Mn-0.6C TWIP steel revealed by in-situ electrochemical nanoindentation10.1016/j.actamat.2018.12.055 ↗
16. Hydrogen degradation of a boron-bearing steel with 1050 and 1300MPa strength levels10.1016/j.scriptamat.2004.10.023 ↗
17. Delayed static failure of twinning-induced plasticity steels10.1016/j.scriptamat.2012.02.038 ↗
18. Effect of hydrogen on the embrittlement susceptibility of Fe–22Mn-0.6C TWIP steel revealed by in-situ tensile tests10.1016/j.msea.2020.140638 ↗
19. Effect of strain rate on hydrogen embrittlement susceptibility of twinning-induced plasticity steel pre-charged with high-pressure hydrogen gas10.1016/j.ijhydene.2016.06.259 ↗
20. Investigations of dislocation-type evolution and strain hardening during mechanical twinning in Fe-22Mn-0.6C twinning-induced plasticity steel10.1016/j.actamat.2020.05.062 ↗
21. Origins of back stress strengthening in Fe-22Mn-0.6C (-3Al) TWIP steels10.1016/j.msea.2020.139834 ↗
22. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
23. Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe–Mn–C TWIP steels10.1016/j.corsci.2014.01.022 ↗
24. Effect of aluminium on hydrogen-induced fracture behaviour in austenitic Fe–Mn–C steel
25. Effects of grain size and dislocation density on the susceptibility to high-pressure hydrogen environment embrittlement of high-strength low-alloy steels10.1016/j.ijhydene.2011.10.099 ↗
26. Effect of grain size on hydrogen embrittlement in stable austenitic high-Mn TWIP and high-N stainless steels10.1016/j.ijhydene.2019.07.227 ↗
27. Hydrogen-enhanced densified twinning (HEDT) in a twinning-induced plasticity (TWIP) steel10.1016/j.scriptamat.2020.08.047 ↗
28. A nanotwinned austenite stainless steel with high hydrogen embrittlement resistance10.1016/j.jallcom.2019.02.312 ↗
29. Effects of strain, strain rate and temperature on deformation twinning in a Cu–Zn alloy10.1016/j.scriptamat.2008.06.060 ↗
30. Influence of addition elements on the stacking-fault energy and mechanical properties of an austenitic Fe–Mn–C steel10.1016/j.msea.2006.12.170 ↗
31. Effect of strain-induced martensite on hydrogen embrittlement of austenitic stainless steels investigated by combined tension and hydrogen release methods10.1016/j.ijhydene.2013.01.198 ↗
32. Characterization of hydrogen-induced crack initiation in metastable austenitic stainless steels during deformation10.1063/1.3477321 ↗
33. On the negative strain rate sensitivity of Hadfield steel10.1016/j.scriptamat.2008.07.027 ↗
34. Effect of grain boundary engineering on hydrogen embrittlement in Fe-Mn-C TWIP steel at various strain rates10.1016/j.corsci.2018.07.028 ↗
35. Microstructural evolution and deformation behavior of twinning-induced plasticity (TWIP) steel during wire drawing10.1016/j.msea.2015.07.034 ↗
36. On the stress state dependence of the twinning rate and work hardening in twinning-induced plasticity steels10.1016/j.scriptamat.2012.01.063 ↗
37. On the relationship between work hardening and twinning rate in TWIP steels10.1016/j.msea.2012.01.123 ↗
38. Temperature dependence of the flow stress of Fe–18Mn–0.6C–xAl twinning-induced plasticity steel10.1016/j.actamat.2013.07.042 ↗
39. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
40. III. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum10.1080/14786435608238074 ↗
41. Effect of high-pressure torsion on hydrogen trapping in Fe–0.01mass% C and type 310S austenitic stainless steel10.1016/j.actamat.2009.09.043 ↗
42. Effect of grain and twin boundaries on the hardening mechanisms of twinning-induced plasticity steels10.1016/j.scriptamat.2007.10.050 ↗
43. Single-mechanism rate theory for dynamic strain aging in fcc metals10.1016/j.actamat.2008.04.030 ↗
44. Study of hydrogen-induced delayed fracture in high-Mn TWIP/TRIP steels during in situ electrochemical hydrogen-charging: role of microstructure and strain rate in crack initiation and propagation10.1016/j.corsci.2019.108191 ↗
45. The effect of pre-strain on hydrogen embrittlement in 310S stainless steel10.1016/j.jallcom.2014.02.038 ↗
46. Effect of pre-strain on hydrogen embrittlement of metastable austenitic stainless steel under different hydrogen conditions10.1016/j.ijhydene.2019.08.046 ↗
47. Hydrogen embrittlement of catholically hydrogen-precharged 304L austenitic stainless steel: Effect of plastic pre-strain10.1016/j.ijhydene.2014.04.122 ↗
48. Improving hydrogen embrittlement resistance of Hadfield steel by thermo-mechanical flash-treatment10.1016/j.msea.2017.11.036 ↗
49. First-principles investigation of hydrogen trapping and diffusion at grain boundaries in nickel10.1016/j.actamat.2015.07.031 ↗
50. The dual role of coherent twin boundaries in hydrogen embrittlement10.1038/ncomms7164 ↗
51. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
52. A novel way to enhance the strength of twinning induced plasticity (TWIP) steels10.1016/j.scriptamat.2018.05.045 ↗
53. Plasticity in cryogenic brittle fracture of ferritic steels: dislocation versus twinning10.1016/j.msea.2018.12.038 ↗