journal article·2017-01-02

Influence of sigma phase on corrosion behavior of 316L stainless steel in high temperature and high pressure water

Jie Ding, En-Hou Han, Zhiming Zhang, Siyan Wang, Jianqiu Wang

Materials at High Temperatures· Volume 34· Issue 1
Publisher page

Abstract

In order to elucidate the impact of σ phase on the oxidation film formation and stress corrosion cracking (SCC) resistance of 316L stainless steel, corrosion, SCC and three-point bending tests were conducted and the microstructures of the σ phase in 316L safe-end pipes were characterized via optical microscopy, environmental scanning electron microscopy and scanning Kelvin probe force microscopy. The results indicated that the σ phase was detrimental to the SCC resistance of 316L in high temperature and high pressure environments and the existence of inherently hard and brittle σ phase could change the cracking mode.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. 10.1016/0010-938X(91)90125-910.1016/0010-938X(91)90125-9 ↗
2. 10.1080/18811248.2006.971117310.1080/18811248.2006.9711173 ↗
3. 10.1016/S0010-938X(97)00140-610.1016/S0010-938X(97)00140-6 ↗
4. 10.1016/S0010-938X(02)00004-510.1016/S0010-938X(02)00004-5 ↗
5. 10.1080/18811248.2005.972638310.1080/18811248.2005.9726383 ↗
6. 10.1016/j.corsci.2010.09.00110.1016/j.corsci.2010.09.001 ↗
7. 10.1016/j.msea.2003.12.01710.1016/j.msea.2003.12.017 ↗
8. 10.1016/j.matchar.2007.05.01710.1016/j.matchar.2007.05.017 ↗
9. 10.1016/j.msea.2007.02.10710.1016/j.msea.2007.02.107 ↗
10. 10.1007/BF0264377910.1007/BF02643779 ↗
11. 10.1179/03063457879043406110.1179/030634578790434061 ↗
12. 10.1134/S0031918X0912009610.1134/S0031918X09120096 ↗
13. 10.1016/j.matchar.2005.11.00310.1016/j.matchar.2005.11.003 ↗
14. 10.1007/s11661-008-9511-810.1007/s11661-008-9511-8 ↗
15. 10.1016/S0010-938X(99)00009-810.1016/S0010-938X(99)00009-8 ↗
16. ASTM A923-01. Standard test methods for detecting intermetallic phase in wrought duplex austenitic/ferritic stianless steels. 2001;A01:1–7.
17. Tang XL · Microsc Microanal · 2005 · 11 · 78
18. 10.1007/s11661-006-9076-310.1007/s11661-006-9076-3 ↗
19. 10.1016/j.matchar.2006.03.01510.1016/j.matchar.2006.03.015 ↗
20. 10.1016/S0921-5093(97)00077-410.1016/S0921-5093(97)00077-4 ↗
21. 10.1016/j.matchar.2013.07.01910.1016/j.matchar.2013.07.019 ↗
22. 10.1016/j.scriptamat.2004.02.01410.1016/j.scriptamat.2004.02.014 ↗
23. 10.1016/S1359-6454(96)00125-510.1016/S1359-6454(96)00125-5 ↗
24. 10.1016/S1359-6454(01)00064-710.1016/S1359-6454(01)00064-7 ↗
25. 10.1016/j.corsci.2004.01.01910.1016/j.corsci.2004.01.019 ↗
26. 10.1149/1.291260110.1149/1.2912601 ↗
27. 10.1016/j.corsci.2009.05.01210.1016/j.corsci.2009.05.012 ↗
28. 10.1016/j.msea.2012.08.06910.1016/j.msea.2012.08.069 ↗
29. 10.1016/S0013-7944(02)00116-910.1016/S0013-7944(02)00116-9 ↗
30. 10.1007/s10534-011-9469-710.1007/s10534-011-9469-7 ↗
31. 10.1002/(ISSN)1097-455510.1002/(ISSN)1097-4555 ↗
32. 10.1016/j.jnucmat.2014.03.03810.1016/j.jnucmat.2014.03.038 ↗
33. 10.1016/j.jnucmat.2013.11.02710.1016/j.jnucmat.2013.11.027 ↗
34. 10.1016/j.corsci.2007.05.00110.1016/j.corsci.2007.05.001 ↗
35. 10.1016/0956-7151(91)90138-Q10.1016/0956-7151(91)90138-Q ↗
36. 10.1016/1359-6454(95)00301-010.1016/1359-6454(95)00301-0 ↗
37. 10.1016/j.corsci.2013.08.02810.1016/j.corsci.2013.08.028 ↗
38. 10.1016/j.electacta.2010.08.02810.1016/j.electacta.2010.08.028 ↗