journal article·2008-01

Origins of tensile stress-induced circumferential cracking of waterwall tubes in boilers

C.H. Hsueh, I.G. Wright

Materials at High Temperatures· Volume 25· Issue 4
Publisher page

Abstract

The leakage and rupture of boiler tubes in power plants is a serious problem that can lead to unscheduled and costly outages. The predominant failure location of current concern is circumferential cracking on the fireside of waterwall tubes in the furnace waterwall section of a boiler. Although there is basic agreement that cracking results from a combination of thermal fatigue and corrosion, a complete explanation of the basic phenomena needed to establish the root causes of this problem is lacking. The purpose of the present study was to analyse the sources of the tensile stress responsible for initiating circumferential cracking and to identify the key parameters controlling this tensile stress. The results of analytical modelling suggested that a combination of increasing tube wall temperature with increasing thickness of internal oxide layers, and temperature spiking due to deslagging events eventually may result in tensile stresses sufficient to crack the fireside oxide and initiate the development of circumferential cracks. This scenario also led to suggestions for reducing tensile stresses in waterwall tubes which, in turn, would be expected to delay/avoid circumferential cracking and improve the reliability of waterwall tubes.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear Engineering Thermal-Hydraulics · Advanced Power Generation Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.