journal article·2017-07-04

Material behaviour and plant experience of P91/P92 components

Andreas Thomas, Peter Seliger, Thomas Hauke

Materials at High Temperatures· Volume 34· Issue 4
Publisher page

Abstract

In several lignite-fired power plants of the ‘Vattenfall Generation AG’ in Germany components of P91/P92 material are used in long-time operation. About this experience in operation of selected components will be reported. In this context own experimental results of a research project in the damage evolution will be presented. The project ‘Damage development III’ was edited together with the MPA Stuttgart and was supported by Vattenfall and AVIF. The aim of the project was to improve the knowledge about the process of creep damage by experimental tests and additional numerical calculations. An instruction was given for planning, implementation and analysis of recurrent investigations on components consisting of 9% Cr steels which are subjected to high operation loading. Finally, the damage phenomena are presented by two case studies, a damage in a pipe bend due to faulty heat treatment and the creep-crack assessment of a lack of side-wall fusion in a reheater weld by fracture mechanics.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Metallurgy and Material Forming · Mechanical Failure Analysis and Simulation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Siempelkamp Pruef- und Gutachter-Gesellschaft mbH, Dresden, Germany

Vattenfall Generation AG, Cottbus, Germany

References (23)

Show source-provided references
1. Blum R, Hald J, Bendick W, et al. Newly developed high-temperature ferritic-martensitic steels from USA, Japan and Europe. VGB Kraftwerkstechnik. 1994;74:553–563.
2. Brett SJ Bates JS Thomson RC. Aluminium nitride precipitation in low strength grade 91 power plant steels. EPRI – 4th International Conference on Advances in Materials Technology for Fossil Power Plants; South Carolina 2004.10.31399/asm.cp.am-epri-2004p1183 ↗
3. Peters J. Quality alert notice no. 2006-001. Global Supply Group – A Bechtel Company, 2006.
4. Schubert J Klenk A. Determination of weld stress factors for creep rupture strength of welded joints. ECCC creep conference; 2005 Sep 12–14; London.
5. Kimura K Tabuchi M Takahashi Y Yoshida K Yagi K. Long-term creep strength and strength reduction factor for welded joints of ASME grades 91 92 and 122 type steels. Safety and Reliability of Welded Components in Energy and Processing Industry: Proceedings of the IIW International Conference; 2008 Jul 10–11; Graz Austria.
6. Schubert J Schwass G. Zeitstandverhalten von modernen martensitischen Stahlguss-Schweißverbindungen im Temperaturbereich 550 bis 650 °C 35. Vortragsveranstaltung der Arbeitsgemeinschaften für warmfeste Stähle und Hochtemperaturwerkstoffe; 2012 Nov 30; Düsseldorf.
7. Vlasak T Hakl J Novak P Sochor J Cech J. Creep strength decrease of cast steel P91 weldments. 22nd International Conference on Metallurgy and Materials; 2013; Brno Czech Republic.10.4028/www.scientific.net/MSF.782.331 ↗
8. VGB-TW507 Ausgabe. Richtreihen zur Bewertung der Gefügeausbildungung und -schädigung zeitstandbeanspruchter Werkstoffe von Hochdruckrohrleitungen und Kesselbauteilen VGB-Kraftwerkstechnik GmbH Essen 1992.
9. VGB-TW507 2. Ausgabe. Richtreihen zur Bewertung der Gefügeausbildungung und Zeitstandschädigung warmfester Stähle für Hochdruckrohrleitungen und Kesselbauteile. Essen: VGB-Power Tech Service GmbH Essen 2005
10. Maile K, Pöllmann J, Seliger P, Reuter A. Abschlussbericht zum AVIF-Vorhaben A 229, Kriterien zur Schädigungsbeurteilung von Hochtemperaturbauteilen aus martensitischen 9-11% Cr-Stählen. Dresden: MPA Universität Stuttgart und Siempelkamp, 2008.
11. BRITE-EURAM Project BE1702, Contract BRPR-CT95-0128. (1996–1999) Validation, expansion and standardisation of Procedures for High Temperature Defect Assessment (HIDA) Final report 1702/PMB/58 – Uniaxial Creep Rupture (1CrMoV-forged) and CCG, CFG (1CrMoV-forged and P91 Steels) Tests of Lab Specimens and Post Test Metallography of CCG, CFG-Specimens, Siempelkamp Prüf- und Gutachter-Gesellschaft mbH Dresden; 1999
12. 10.1016/S0308-0161(01)00100-410.1016/S0308-0161(01)00100-4 ↗
13. Celard NJ Nikbin KM Webster GA. Validation expansion and standardisation of procedures for high temperature defect assessment (HIDA). Final report of Imperial College London; 2000 Apr.
14. European Project G5RD-CT-1999-00118 INTEGRITY. Integrity of repair welds in high temperature plants operation under steady and cyclic loading conditions; 2000–2005.
15. European Project GRD2-2000-30363 WELDON. Weld strength for high temperature components design and operation; 2001–2006
16. 10.1016/j.engfracmech.2006.08.01710.1016/j.engfracmech.2006.08.017 ↗
17. Seliger P Lepinski S. Zeitstand- und Kriechverhalten von dickwandigen Rohren aus X10CrMoVNb9-1 hergestellt aus Schmiedestücken. 26. Vortragsveranstaltung der Arbeitsgemeinschaften für warmfeste Stähle und Hochtemperaturwerkstoffe; 2003 Nov 28; Düsseldorf.
18. VdTÜV-Werkstoffblatt 511/3: Warmfester Stahl F91; X10CrMoVNb9-1; Werkstoff-Nr. 1.4903; Stabstahl Schmiedestück; VdTÜV e.V. Essen; 2013 März.
19. Andersson P Bergmann M Brickstad B Dahlberg L Nilsson F Sattari-Far I. A procedure for safety assessment of components with cracks – handbook. revised ed. Stockholm: SAQ Kontroll AB; 1998 Sep.
20. Ewald J, Kussmaul K, Keienburg KH. Hinweise auf Mechanismen und Einflussgrößen zur Beurteilung des Bauteilverhaltens im Kriechbereich anhand von Kleinproben. VDI-Bericht. 1979;354:39–57.
21. Maleki S Yanhui Zhang Y Nikbin K. Prediction of creep crack growth properties of P91 parent and welded steel using remaining failure strain criteria. International Conference of WELDS 2009: Design testing assessment and safety of high-temperature welded structures; 2009 Jun 24–26; Fort Myers FL USA.
22. 10.1179/096034011X1305703258555710.1179/096034011X13057032585557 ↗
23. Dogan B Petrovski B. High temperature behaviour of P91-steel weldments. Proceedings of the 9th International Conference; 2001 Apr; Swansea.