Ratcheting and low cycle fatigue of nickel-based alloy GH3536 formed by selective laser melting at 800 °C

Lingfeng Pan, Peishan Ding, Kun Yan, Linwei Ma, Xiaotao Zheng

Materials at High Temperatures· Volume 39· Issue 4
Publisher page

Abstract

The cyclic uniaxial stress-controlled ratcheting behaviour of GH3536 formed by selective laser melting (SLM) was tested at 800 °C. The effects of different stress rates and building orientations of 0°, 45° and 90° were investigated. Results present that the ratcheting behaviour of SLM GH3536 at 800 °C exhibits significant stress rate dependence. Moreover, the accumulated ratcheting strain increasing with increasing the stress amplitude and stress rate. It is noted that the building orientation angle of the specimen has an important influence on the mechanical performance. The 45° specimen in the experimental conditions has the greatest low cycle fatigue life. The ratcheting evolution over the whole cyclic load history can be divided into three stages. The relationship between steady ratcheting strain range and low cycle fatigue life was established.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Hubei Provincial Key Laboratory of Chemical Equipment Intensification and Intrinsic Safety, School of Mechanical and Electrical Engineering, Wuhan Institute of Technology, Wuhan, P.R. China

School of Chemical Machinery and Safety, Dalian University of Technology, Dalian, Liaoning, P.R. China

Funding

National Natural Science Foundation of China · Open Research Fund Program of Hubei Provincial Key Laboratory of Chemical Equipment Intensification and Intrinsic Safety · 13th Postgraduate Education Innovation Fund of Wuhan Institute of Technology · Young Scientists Fund

References (26)

Show source-provided references
1. 10.1016/j.tafmec.2020.10260410.1016/j.tafmec.2020.102604 ↗
2. 10.1115/1.403423510.1115/1.4034235 ↗
3. M TS · Addit Manuf · 2015 · 8 · 36
4. 10.1016/j.addma.2015.07.00210.1016/j.addma.2015.07.002 ↗
5. 10.1016/j.ijfatigue.2016.03.01210.1016/j.ijfatigue.2016.03.012 ↗
6. 10.1016/j.ijfatigue.2016.03.01410.1016/j.ijfatigue.2016.03.014 ↗
7. 10.1016/j.msea.2015.10.06810.1016/j.msea.2015.10.068 ↗
8. 10.1016/j.msea.2015.07.05610.1016/j.msea.2015.07.056 ↗
9. 10.1080/09603409.2016.126151110.1080/09603409.2016.1261511 ↗
10. 10.1016/S1006-706X(07)60012-010.1016/S1006-706X(07)60012-0 ↗
11. 10.1016/S0029-5493(02)00062-610.1016/S0029-5493(02)00062-6 ↗
12. 10.1016/j.ijfatigue.2011.04.00910.1016/j.ijfatigue.2011.04.009 ↗
13. 10.1016/j.ijplas.2015.10.00110.1016/j.ijplas.2015.10.001 ↗
14. 10.1016/j.mechmat.2011.03.00210.1016/j.mechmat.2011.03.002 ↗
15. Zhao P · Acta Metall Sin · 2011 · 24 · 148
16. 10.1016/j.nucengdes.2012.02.01710.1016/j.nucengdes.2012.02.017 ↗
17. 10.1016/j.nucengdes.2006.09.00910.1016/j.nucengdes.2006.09.009 ↗
18. 10.1016/j.msea.2006.01.05210.1016/j.msea.2006.01.052 ↗
19. Liu H · Rare Metal MaterEng · 2014 · 43 · 2473
20. 10.1557/jmr.2019.710.1557/jmr.2019.7 ↗
21. 10.1016/j.ijplas.2005.05.00610.1016/j.ijplas.2005.05.006 ↗
22. 10.1016/j.msea.2013.03.00410.1016/j.msea.2013.03.004 ↗
23. 10.1016/j.mechmat.2015.05.01110.1016/j.mechmat.2015.05.011 ↗
24. 10.1016/j.nucengdes.2012.02.01710.1016/j.nucengdes.2012.02.017 ↗
25. 10.1007/s12540-020-00811-910.1007/s12540-020-00811-9 ↗
26. 10.1016/j.ijplas.2008.06.00410.1016/j.ijplas.2008.06.004 ↗