journal article·2003-01

Impurity and surface condition effects on pore formation at Al2O3/FeAl interfaces

Peggy Y. Hou, Chris Van Lienden

Materials at High Temperatures· Volume 20· Issue 3
Publisher page

Abstract

Interfacial pores are commonly observed at the scale/alloy interface in NiAl and FeAl alloys after high temperature oxidation. The pores are often an order of magnitude larger than the oxide grains, and many are formed during the initial stage of oxidation. In order to better understand the development of these pores, the effects of pre-oxidation surface condition and surface impurities on pore formation at the oxide/alloy interface in Fe–40at%Al are investigated. Surface conditions included polishing to 4000 grit with SiC and polishing to 1 µm with diamond suspension. Surface impurities included a number of nitrate salts dissolved in water. Pore number distribution in each case was determined and related to the treatment effects. Testing was also performed on an Hf-containing Fe–40Al to evaluate the effect of adding a reactive element. It was found that surface roughness and the presence of impurities, even residues from water drops, increased the number of interfacial pores. Hf addition made the alloy more resistant to pore formation, but large pores developed under heavy salt deposits.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. 10.1179/msc.1981.15.1.710.1179/msc.1981.15.1.7 ↗
2. 10.1016/0010-938X(93)90271-H10.1016/0010-938X(93)90271-H ↗
3. Xu C-H. · High Temp. Mater. Proc. · 2000 · 19 · 37110.1515/HTMP.2000.19.6.371 ↗
4. Hou P. Y. · p. 15
5. 10.1016/0956-716X(95)00341-R10.1016/0956-716X(95)00341-R ↗
6. Hou, P. Y. Impurity effect on pore formation at A1203/alloy inter-faces, to be published inProc. John Stringer Sym. on High Temperature Corrosion. ASM Materials Solution Conference, Indianapolis, IN, Nov. 5-8,2001
7. 10.1002/sia.74018080210.1002/sia.740180802 ↗
8. 10.4028/www.scientific.net/MSF.369-372.2310.4028/www.scientific.net/MSF.369-372.23 ↗
9. 10.1007/BF0167050510.1007/BF01670505 ↗
10. 10.1016/0039-6028(77)90353-310.1016/0039-6028(77)90353-3 ↗
11. Hou, P. Y., Niu, Y. and Van Lienden, C. Analysis of pore formation at oxide/alloy interfaces, part I. experimental results on FeAl,Oxid. Metals(in press)
12. 10.1016/S1359-6462(97)00451-X10.1016/S1359-6462(97)00451-X ↗
13. D. P. Woodruff,The Solid-Liquid Interface, pp. 21-38, Cambridge University Press (1973).
14. 10.1016/0039-6028(77)90011-510.1016/0039-6028(77)90011-5 ↗
15. 10.1179/03071698480327480010.1179/030716984803274800 ↗
16. 10.1021/j150528a01810.1021/j150528a018 ↗
17. 10.1023/A:101889972975810.1023/A:1018899729758 ↗
18. 10.1007/978-1-4615-5393-9_510.1007/978-1-4615-5393-9_5 ↗
19. 10.1149/1.277383110.1149/1.2773831 ↗
20. 10.1007/BF0066501810.1007/BF00665018 ↗
21. 10.1016/S1359-6454(97)00378-910.1016/S1359-6454(97)00378-9 ↗
22. 10.1007/BF0084669010.1007/BF00846690 ↗
23. Prescott R. · J. Oxidation mechanisms of P-NiAl+Zr determined by SIMS. Corro. Sci. · 1995 · 37 · 1341
24. Gesmundo F.
25. 10.1016/0021-9517(89)90304-710.1016/0021-9517(89)90304-7 ↗
26. 10.1016/S0039-6028(97)00597-910.1016/S0039-6028(97)00597-9 ↗