journal article·2016-06-28

High temperature oxidation and γ′ depletion in the single-crystal superalloy PWA 1484

Robert L. Amaro, Stephen D. Antolovich, Richard W. Neu, Preet M. Singh

Materials at High Temperatures· Volume 33· Issue 4-5
Publisher page

Abstract

Single-crystal Ni-base superalloys are a favoured material for blades in the hot section of aero turbines. These materials exhibit excellent dimensional stability, deformation response and oxidation behaviour at higher temperatures, relative to other metals. Due to the high service temperatures and fluctuating loads experienced by turbine blades, a complete understanding of the material’s oxidation and γ′ depletion kinetics is sought to characterise this aspect of the material’s deformation response. This work provides the results and subsequent analysis of stress-free γ′ depletion tests performed on the single-crystal Ni-base superalloy PWA 1484. It was determined that the γ′ depletion kinetics of this material followed a sub-parabolic rate law. Furthermore, γ′ depletion kinetics were dependent upon surface roughness. Surface roughness can be an issue in practical application of oxidation principles and data. A relationship is developed, based on the literature and current work, which relates the stress-free γ′ depletion kinetics to exposure temperature, time and surface roughness.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · High-Temperature Coating Behaviors · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. 10.1149/1.240783710.1149/1.2407837 ↗
2. Reed R. C. · 2008
3. 10.1179/02670830322500197510.1179/026708303225001975 ↗
4. 10.5006/1.358304510.5006/1.3583045 ↗
5. 10.5006/1.357932010.5006/1.3579320 ↗
6. 10.4028/www.scientific.net/MSF.251-25410.4028/www.scientific.net/MSF.251-254 ↗
7. 10.1016/j.msea.2008.01.04310.1016/j.msea.2008.01.043 ↗
8. 10.1023/A:102360421424510.1023/A:1023604214245 ↗
9. 10.1023/A:102462971645210.1023/A:1024629716452 ↗
10. 10.1023/A:102010260409010.1023/A:1020102604090 ↗
11. 10.1023/A:102017032002010.1023/A:1020170320020 ↗
12. 10.1016/0921-5093(92)90358-810.1016/0921-5093(92)90358-8 ↗
13. R. T. DeHoff:Thermodynamics in materials science. 2nd ed. 2006, Boca Raton: CRC/Taylor & Francis. 605.10.1201/9781420005851 ↗
14. Wright P. K. · Oxidation-fatigue interactions in a single-crystal superalloy · 1987
15. Zhao L. G. · Computational modelling of crack initiation in a single crystal superalloy under fatigue-oxidation conditions · 2007
16. 10.1016/j.jmps.2005.09.00110.1016/j.jmps.2005.09.001 ↗
17. 10.1080/1478643031000160540710.1080/14786430310001605407 ↗
18. Kupkovits R. · Thermomechanical fatigue behavior of the directionally-solidified nickel-base superalloy CM247LC, in Mechanical engineering · 2009
19. 10.1115/1.290319110.1115/1.2903191 ↗
20. 10.1016/j.actamat.2007.01.03410.1016/j.actamat.2007.01.034 ↗
21. 10.7449/1988/Superalloys_1988_235_24410.7449/1988/Superalloys_1988_235_244 ↗
22. Amaro R. L. · Thermomechanical fatigue crack formation in a single crystal Ni-base superalloy · 2010 · 321
23. 10.1016/j.corsci.2008.06.03310.1016/j.corsci.2008.06.033 ↗
24. Pilling N. B. · J. Inst. Metals · 1923 · 29 · 529
25. 10.1002/zaac.1920111010710.1002/zaac.19201110107 ↗
26. Wagner C. · Atom movements · 1951
27. 10.1016/0956-7151(94)90481-210.1016/0956-7151(94)90481-2 ↗
28. Fleury E. · Endommagement du superalliage monocristallin AM1 en fatigue isotherme et anisotherme · 1991
29. 10.1111/j.1460-2695.2011.01660.x10.1111/j.1460-2695.2011.01660.x ↗
30. 10.1007/BF0055107510.1007/BF00551075 ↗
31. 10.1016/j.jallcom.2009.02.11510.1016/j.jallcom.2009.02.115 ↗