In situmaterials testing in a waste-to-energy power plant
Source abstract
Abstract
AbstractSamples of 16 different metals were assembled on air-cooled, retractable corrosion probes and exposed for over 4400 hours in a 300 ton/day waste-to-energy boiler. The probes were exposed in both the furnace and connection pass areas of the boiler and were controlled to two temperature bands in each of those areas. Alloy 625 had the lowest wastage rate in the furnace area of the boiler, and there was a linear dependency between corrosion and temperature. Also, in the upper convection pass, alloy 625 again had the lowest wastage rate of all the tested alloys, but the wastage rate curve vs temperature became more experimental in nature. In the convection pass area of the boiler, the wastage decreased linearly as a function of the sum of the chromium, nickel, and molybdenum in the alloys.Keywords: chlorine corrosioncorrosion probemolton saltcorrosion
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Aluminum Alloy Microstructure Properties · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Adkin P. · Mechanical Engineering · 1988 · 110 · 46
2. Krause, H. H.Metals Handbook, Vol. 13: Corrosion, 9th edn, p. 997. ASM International, Metals Park, Ohio (1987).
3. Daniel P. L. · Materials Performance · 1988 · 27 · 22
4. 10.1007/BF0283357110.1007/BF02833571 ↗
5. 10.1115/1.344569310.1115/1.3445693 ↗
6. Bryers, R. W. (ed.)Incinerating Municipal and Industrial Waste: Fireside Problems and Prospects for Improvement.Hemisphere Publishing Corporation, New York (1991).
7. Paul L. D. · 1993
8. Daniel P. L. · 1991
9. Blough J. L. · 11