Boron additions and M3B2precipitation in an Fe-Ni-Cr-W-AI-Ti alloy
Source abstract
Abstract
In the cooling stage of solution treatment, fine plate-like M3B2 precipitated at grain boundaries, the quantity increasing with increasing boron content in the alloy. When boron content reached 310 ppm, the precipitation of M3B2 during cooling mainly concentrated on the surfaces of lump-like M3B2 at grain boundaries. In the process of standard heat treatment, the quantity of granular M3B2 increased with increasing boron content. Boron could suppress the segregation of plate-like MC at grain boundaries. Granular M3B2 precipitated homogeneously in a disperse form. It was discovered that it could precipitate on the surfaces of blocky-like M3B2 and plate-like MC when the boron content reached 310 ppm. Blocky-like and granular M3B2 in the alloy were composed of tungsten, titanium, chromium, iron, etc. with a general formula MxM'3-xB2; here, in addition to some granular M3B2 with x = 2, x was normally larger than 2.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (5)
Show source-provided references
1. Yie Jun ‘Nickel-base Superalloys in US’, Science Publishing Press, Beijing (1978)
2. Decker, R. F. and Sims, C. T. ‘Superalloys’ (Eds. C. T. Sims and W. C. Hagel), Wiley, New York (1972) pp. 33–77
3. 10.1179/imtr.1976.21.1.110.1179/imtr.1976.21.1.1 ↗
4. Yuqing Li · Acta Metall. Sinica · 1984 · 20 · A329
5. Li Yuqing and Liu Jinyan ‘Interstitial Phases in Superalloys’ Metallurgical Industrial Publishing Press, Beijing, (1990) pp. 203–213