Corrosion behaviour of four high temperature engineering materials exposed to landfill gas engine flue gas
Source abstract
Abstract
Four engineering materials commonly used in high-temperature applications were exposed to landfill gas engine flue gas for 25 days at 411°C. The flue gas was composed mostly of nitrogen and oxygen, although some carbon monoxide and hydrocarbons were detected together with low concentrations of hydrogen chloride gas and sulphur oxides. Hydrogen fluoride was not analysed, but, due to the nature of the fuel, may have been present at low levels. The materials tested were a carbon steel, a low alloy steel, a 12%Cr stainless steel and an austenitic stainless steel. Thin, protective films were formed on the 12%Cr and austenitic stainless steels, however, the corrosion products formed on carbon and low-alloy steels consisted of several layers, the outermost of which were extremely friable and non-adherent, especially on cooling from the flue gas working temperature. The maximum corrosion rate obtained was 70 μm yr–1 for carbon steel, which may be acceptable for a number of flue gas applications. The exposed coupons were examined using conventional techniques such as X-ray diffraction (XRD), optical microscopy (OM) and scanning electron microscopy (SEM). The predominant scale formation mechanism controlling the corrosion appeared to be simple oxidation type reactions, however, the influence of HCl, as evidenced by the presence of akaganeite (β-FeO(OH)), was hypothesised. A model describing the corrosion mechanism is proposed in order to provide an improved life prediction capability for such flue gas environments.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Engineering and Material Science Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Krause H.H. · 1994
2. Meadowcroft D.B · Proc. Conf. Mats. for Advanced Power Eng · 1994
3. Meadowcroft D.B · 1994
4. McIlhone G · 1994
5. Millyan, A. Waste Resources Ltd., PO Box 53099, Auckland personal communication.
6. Blough J.L. · Mater. High Temp · 1997 · 181
7. Abbot N.H.C · 1992
8. Malcolm, R. Mercury Energy, Private Bag 92008, Auckland, personal communication.
9. XRD report No MSPCER 399 (1994).10.1111/j.1460-9592.1994.tb00418.x ↗
10. Brooks S. · 1985 · 515
11. 10.5006/0010-9312-36.7.36910.5006/0010-9312-36.7.369 ↗
12. 10.1002/maco.1988039110510.1002/maco.19880391105 ↗
13. Lai G.Y · 1990
14. Lichti K.A. · 1995
15. Lichti K.A. · 1995
16. Strafford K.N · Metall. Rev · 1969 · 138, 153
17. 10.1515/HTMP.1984.6.1-2.110.1515/HTMP.1984.6.1-2.1 ↗
18. 10.1007/BF0065989910.1007/BF00659899 ↗
19. Kofstad P · 1988
20. Darken L.S. · 1953
21. 10.1002/maco.1989040030810.1002/maco.19890400308 ↗
22. Grabke H.J · 1991
23. Pourbaix, M.Corros. Sci. , 35, 1167.10.1016/0010-938X(93)90337-G ↗
24. Pourbaix A. · 1989
25. McIlhone P.G.H. · 1995
26. 10.1016/0010-938X(95)00011-810.1016/0010-938X(95)00011-8 ↗
27. 10.1007/BF0264242710.1007/BF02642427 ↗
28. 10.1180/minmag.1962.033.259.0210.1180/minmag.1962.033.259.02 ↗
29. 10.1346/CCMN.1984.032030210.1346/CCMN.1984.0320302 ↗
30. 10.1346/CCMN.1981.029040410.1346/CCMN.1981.0290404 ↗
31. Taylor-Lawrence A. · Meteoritics · 1981 · 16 · 391
32. 10.1007/BF0191211710.1007/BF01912117 ↗
33. Grabke H.H · 1989
34. 10.1115/1.344558010.1115/1.3445580 ↗