Abstract

P91 and P92 steels are widely used in power plants and petrochemical industry for long-term service components. Due to high resistance to creep, fatigue and corrosion, the use of grade 91 and grade 92 steels allows ultrasupercritical conditions (600 °C, 300 bar). To achieve this goal the alloy design was based on the following metallurgical concepts: stable tempered martensitic microstructure, precipitation strengthening through M23C6 (Cr, Fe, Mo or W carbides) and fine MX (V, Nb carbides), solution hardening through elements as Mo or Mo/W and high Cr content. This study is focused on the microstructure evolution of grade 91 and grade 92 steels under aging and creep conditions. Three sets of laboratory-aged specimens heated in oven at 550°C, 600°C and 650°C were examined. Furthermore, the influence of stress on the microstructure was evaluated. The microstructures were characterized by several means of investigations and the results were compared to literature.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Intermetallics and Advanced Alloy Properties · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Inail Innovative Technologies Department, Rome, Italy

RINA Consulting - CSM S.p.A, Rome, Italy

References (15)

Show source-provided references
1. 10.5539/jmsr.v10n2p110.5539/jmsr.v10n2p1 ↗
2. 10.1016/j.ijpvp.2010.03.01710.1016/j.ijpvp.2010.03.017 ↗
3. 10.1007/s12666-010-0045-610.1007/s12666-010-0045-6 ↗
4. Hasegawa Y, Ishii N, Kodama M, et al. Possible microstructural resistant factors in P91 steel to the magnetic domain wall motion of electro-magnetic inspection method. In Proceedings of the High Temperature Plant Materials, Inspection, Monitoring & Assessment—MIMA 2 Conference, London, UK, 11–13 October 2022.
5. 10.1179/026708309X1256726892668710.1179/026708309X12567268926687 ↗
6. Hald J, Tassa O, Matera S. Creep behavior and precipitate evolution of P92 after long-term creep. Proc. 4th International ECCC Conference Creep & Fractur Düsseldorf, Germany; 2017.
7. 10.1179/174892306X9973210.1179/174892306X99732 ↗
8. Shibli A; Utilizzo del microscopio a scansione di forza (SFM) per la valutazione delle cavità allo stadio iniziale negli acciai martensitici. Proceedings of the AIPnD 2022 Conference - National Conference on Non-Destructive Testing Monitoring Diagnostics, Verona, Italy, 19-21 October 2022.
9. Tonti A, Augugliaro G, Lega D, et al. Microstructure atlas and life assessment tools. Proc. 3rd International ECCC Conference Creep & Fracture. Rome Italy; 2014.
10. Cipolla L, Caminada S, Venditti D, et al. Microstructural evolution of ASTM P91 after 100,000 hours exposure at 550°C and 600°C. 9th Liège Conference on Materials, for Advanced Power Engineering: September 27th — 29th, 2010, Liège • Belgium; 2010.
11. Di Gianfrancesco A, Tiberi Vipario S, Venditti D, et al. Microstructural evolution of ASTM P91 after 100,000 hours exposure at 550°C, 600°C and 650°C. 12th International Conference on Creep and Fracture of Engineering Materials and Structures JIMIS11. May. Kyoto Japan; 2012.
12. 10.1179/1743284714Y.000000063510.1179/1743284714Y.0000000635 ↗
13. 10.15406/ipcse.2018.03.0006810.15406/ipcse.2018.03.00068 ↗
14. Yaguchi M, Nakamura K. “Re-evaluation of long-term creep strength of welded joint of ASME Grade 91 type steel” Proceedings of the ASME 2016 Pressure Vessels and Piping Conference PVP2016 July 17-21, 2016, Vancouver, British Columbia, Canada.
15. Krein R. ”Creep rupture strength of P91 and P92 welded joints” ECCC workshop on creep strength and heat to heat variation of high chromium steels. Rome: RINA CSM; 2019 December.