Oxidation of SS304 and SS316 and the formation of diffusionally isolated regions leading to localised premature breakaway oxidation
Source abstract
Abstract
The results are presented on the oxidation behaviour of two chromia-forming steels, over the temperature range 800°C to 900°C, regions of premature localised breakaway oxidation were observed. SiO2 formation along emergent grain boundaries encapsulated smaller grains, acting as diffusion barriers to the replenishment of chromium from deeper in the alloy. Rapid depletion of chromium from these isolated grains continued with increasing time until the concentration was insufficient to maintain a protective Cr2O3 resulting in the localised chemical failure and formation of breakaway oxides. A finite difference model was used to demonstrate the effect of SiO2 formation. It was also found that the low concentration of silicon restricted the encapsulation process to only the smaller grains at the surface and protective oxidation was re-established underneath at the alloy surface. The predicted lifetime of components with wall thicknesses of 2 mm was calculated to be in excess of 30 years.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Metallurgy and Materials, University of Birmingham, Birmingham, UK
Recycling Technologies, Swindon, UK
References (35)
Show source-provided references
1. Whittle DP, Stringer J. VIII. Improvement in properties additives in oxidation resistance. Phil Trans R Soc Load. 1980;A 295:309–329.
2. 10.1088/0034-4885/50/7/00210.1088/0034-4885/50/7/002 ↗
3. 10.1007/BF0104672510.1007/BF01046725 ↗
4. 10.1080/09603409.1997.1168956510.1080/09603409.1997.11689565 ↗
5. 10.1007/s11085-008-9097-y10.1007/s11085-008-9097-y ↗
6. Bainbridge JE Horsley GW Cairns JA et al. UK patent: GB 2 097 821A. Carbon Deposition Inhibition; 1982.
7. 10.1007/BF0065622510.1007/BF00656225 ↗
8. 10.1007/BF0065658010.1007/BF00656580 ↗
9. 10.1098/rspa.1987.008610.1098/rspa.1987.0086 ↗
10. 10.1179/mst.1989.5.8.82810.1179/mst.1989.5.8.828 ↗
11. 10.1007/s11085-019-09891-410.1007/s11085-019-09891-4 ↗
12. 10.1016/j.msea.2007.05.03510.1016/j.msea.2007.05.035 ↗
13. 10.1149/1.277960510.1149/1.2779605 ↗
14. 10.1149/1.243015910.1149/1.2430159 ↗
15. 10.1023/A:101885591473710.1023/A:1018855914737 ↗
16. 10.1007/BF0061208810.1007/BF00612088 ↗
17. 10.1016/0040-6090(84)90012-910.1016/0040-6090(84)90012-9 ↗
18. 10.1023/A:101880892575610.1023/A:1018808925756 ↗
19. Quadakkers WJ, Bongark K. The prediction of breakaway oxidation for alumina forming ODS alloys using Oxidation Diagrams. Mat Corro. 1994;4(5):232–241.
20. 10.1007/BF0264707910.1007/BF02647079 ↗
21. 10.1016/S1359-6454(03)00381-110.1016/S1359-6454(03)00381-1 ↗
22. 10.1007/s11085-010-9225-310.1007/s11085-010-9225-3 ↗
23. 10.1088/0965-0393/14/4/01410.1088/0965-0393/14/4/014 ↗
24. 10.1007/s11085-006-9039-510.1007/s11085-006-9039-5 ↗
25. Moore P. Stainless steel grade selection. Atlas steels. 2020 https://www.atlassteels.com.au
26. smst_booklet_304_2008.pdf. Salzgitter Mannesmann 2008. 2020. https://salzgitter-mannesmann-uk.com
27. smst_booklet_304l_2008.pdf. Salzgitter Mannesmann 2008. 2020. https://salzgitter-mannesmann-uk.com
28. smst_booklet_304ln_2008.pdf. Salzgitter Mannesmann 2008. 2020. https://salzgitter-mannesmann-uk.com
29. 10.1002/jctb.500063050110.1002/jctb.5000630501 ↗
30. Richardson FD, Jeffes HEJ. The thermodynamics of substances of interest in iron and steel making from 0 °C to 2400 °C. J Iron Steel Inst. 1948;160:261–273.
31. Hansson AN, Hattel JH, Dahl KV, et al. Modelling Cr depletion under a growing Cr2O3 layer on austenitic stainless steel: the influence of grain boundary diffusion Modelling Simul. Mater Sci Eng. 2009;17:1–19.
32. 10.1023/A:101036902414210.1023/A:1010369024142 ↗
33. 10.2320/matertrans.45.294510.2320/matertrans.45.2945 ↗
34. 10.1007/s11669-021-00897-710.1007/s11669-021-00897-7 ↗
35. 10.1002/maco.20080413510.1002/maco.200804135 ↗