Internal oxide thickness measurement by ultrasonic method

Jana Vesela, Pavel Mareš, Roman Janura

Materials at High Temperatures· Volume 37· Issue 1
Publisher page

Abstract

Long-term exposition of re-heater and super-heater tubes in fossil-fired steam boilers at high temperature causes the growth of the iron oxide scale (magnetite) on the both internal and external tube surfaces. The presence of the internal oxide scale on the water side of the tube acts as a thermal insulator reduces heat transfer through the tube wall. Persistent overheating of the tube wall is a crucial issue, which leads to a metallurgical failure of the tube. The oxide scales react as a thermal insulator on the water side and reduce the heat transfer through the tube wall. Relatively thin oxide scale contributes to a reduction of boiler efficiency and causes persistent overheating of the tube wall. The growth of internal oxide scale is a time- and temperature-dependent process with a negative impact on the remaining creep-to-rupture life.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Minerals Flotation and Separation Techniques · Iron oxide chemistry and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Diagnostics and Qualification, Research Centre Rez Ltd, Husinec-Rez, Czech Republic

References (3)

Show source-provided references
1. French DN. Metallurgical failures in fossil fired boilers. New York: John Wiley & Sons; 1983. p. 143–145.
2. EPRI, 3002002053 · 2013
3. 10.1111/j.1365-246X.2009.04122.x10.1111/j.1365-246X.2009.04122.x ↗