journal article·2009-09

Hot corrosion of two nickel-base superalloys under alkali sulfate deposition conditions

R.F.A. Pettersson, F. Karlsson, J. Flyg

Materials at High Temperatures· Volume 26· Issue 3
Publisher page

Abstract

The single crystal MD2 (Ni – 8Cr – 5Al –5Co– 2Mo– 8W–6Ta – 1Ti) and the polycrystalline Inconel 792 (Ni –13Cr – 3Al –9Co– 2Mo– 4W–4Ta– 4Ti) were exposed at 850 and 900°C in an severely sulfidising environment comprising synthetic air with 8% water vapour and 2000 ppm SO2, and a deposit of 20 mol% Na2SO4+80 mol% K2SO4 applied every 160 hours.Results were evaluated in terms of mass change, which indicated the existence of an incubation time before the onset of extensive attack, and post-test metallography to evaluate metal loss. Metallographic studies are presented showing the complex external oxide scale formation and internal oxidation and sulfidation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. 10.1007/BF0066548810.1007/BF00665488 ↗
2. Stringer J · 1987
3. Kofstad P · 1988
4. Cyclic oxidation testing—Development of a code of practice for the characterisation of high temperature materials performance (COTEST), European Commission report under contract G6RD-CT-2001-00639.
5. 10.3184/096034007X26358710.3184/096034007X263587 ↗
6. 10.1016/j.corsci.2004.04.01310.1016/j.corsci.2004.04.013 ↗
7. Nakamori, M., Kayano, I., Tsukuda, Y, Takahashi, K. and Torigoe, T. (1997) Hot Corrosion and its prevention in high temperature heavy oil firing gas turbines.Mater Sci. For. 251-254, 633 — 640.10.4028/www.scientific.net/MSF.251-254.633 ↗
8. Pettersson R.
9. Pettersson R.F.A. · 2006