Effect of environment on the scale formed on oxide dispersion strengthened FeCrAl at 1050°C and 1100°C
Source abstract
Abstract
The surface scale formed on specimens of a commercial oxide dispersion strengthened (ODS) FeCrAl alloy (PM2000) exposed for 1 and 500 h at 1050°C in dry O2, Air+10%H2O and Ar+10%H2O consisted of a two-layer α-Al2O3 structure with a columnar grain inner layer and a finer grain outer layer. The alumina scales formed in Air+10%H2O and Ar+10%H2O were slightly more than half of the thickness of the scale formed in dry O2. The same two-layer structure was also observed after exposure for 500 h at 1100°C in dry O2 and 50%CO2+50%H2O. The alumina scales formed in both atmospheres were similar in thickness. Oxides rich in Y and Ti at the gas – scale interface grew in size and number with time in each case. Using analytical transmission electron microscopy, alumina grain boundary segregation of both Y and Ti was evident near the gas interface but only Y segregation was detected near the metal interface. This difference was attributed to Ti depletion in the adjacent metal and the rapid outward flux of the smaller Ti ion through the scale.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. 10.1016/S0924-0136(02)00237-610.1016/S0924-0136(02)00237-6 ↗
2. 10.1002/maco.1994045040410.1002/maco.19940450404 ↗
3. Nicholls J. R. · Mater High Temp · 2003 · 20 · 93
4. 10.1007/s11661-999-0128-310.1007/s11661-999-0128-3 ↗
5. 10.1007/s11661-003-0020-510.1007/s11661-003-0020-5 ↗
6. Bachorczyk, R. and Fordham, R. (2005) Long-term, cyclic oxidation behaviour of alumina- and chromia-forming alloys, diffusion and defect data— solid state data, Pt. A. Defect Diffus. Forum, 237-240, 1107–1114.10.4028/www.scientific.net/DDF.237-240.1107 ↗
7. Smialek, J. L. (2008) Enigmatic moisture effects on A1203 scale and TBC adhesion. Mater. Sci. Forum, 595-598, 191–198.10.4028/www.scientific.net/MSF.595-598.191 ↗
8. 10.1007/BF0213478610.1007/BF02134786 ↗
9. 10.1179/mht.2000.02010.1179/mht.2000.020 ↗
10. 10.1007/s11085-007-9055-010.1007/s11085-007-9055-0 ↗
11. 10.1016/j.corsci.2008.05.01910.1016/j.corsci.2008.05.019 ↗
12. 10.1007/s11085-010-9195-510.1007/s11085-010-9195-5 ↗
13. 10.1007/s11661-007-9342-z10.1007/s11661-007-9342-z ↗
14. 10.1002/maco.20050391710.1002/maco.200503917 ↗
15. 10.1007/s11085-009-9177-710.1007/s11085-009-9177-7 ↗
16. 10.1002/maco.20080411610.1002/maco.200804116 ↗
17. Pint B. A. · Mater. High Temp · 1995 · 13 · 310.1080/09603409.1995.11689496 ↗
18. Quadakkers W. J. · Suif. Sc · 1991 · 271
19. 10.1179/mht.2000.02210.1179/mht.2000.022 ↗
20. 10.1007/BF0061215810.1007/BF00612158 ↗
21. Nychka J. A. · acid. Met · 2005 · 63 · 325
22. 10.1007/s10853-008-2639-510.1007/s10853-008-2639-5 ↗
23. 10.1007/BF0104681810.1007/BF01046818 ↗
24. 10.1111/j.1151-2916.1998.tb02335.x10.1111/j.1151-2916.1998.tb02335.x ↗
25. 10.1149/1.183856310.1149/1.1838563 ↗