Reduction in defect content of oxide dispersion strengthened alloys
Source abstract
Abstract
Evidence from the literature has been considered for factors controlling the occlusion and retention of gas in powders, particularly those produced by mechanical alloying (MA). A series of experiments has been performed on oxide dispersion strengthened Fe3Al and PM 2000 powders to determine recovery, recrystallisation and vacuum degassing behaviour. As-MA ODS Fe3Al powders begin to recover and recrystallise at lower temperatures than PM 2000 (550°C c.f. 750°C, respectively) and recrystallise to a finer grain size (∼10μm maximum mean linear intercept c.f. ∼50μm in PM 2000). Both powders outgassed hydrogen, as well as smaller quantities of nitrogen and water vapour. However, PM 2000 released more hydrogen than Fe3Al. Both powders contained small pores which are likely to have entrained molecular hydrogen. Defects contained in consolidated secondary recrystallised Fe3Al included porosity, residual stringers of fine grains and intrusions. The latter were larger, more numerous and slightly elongated within the fine grained regions suggesting an association.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. Jones A.R. · 1998
2. 10.1179/mtlr.1966.11.1.15910.1179/mtlr.1966.11.1.159 ↗
3. 10.1016/0001-6160(83)90192-X10.1016/0001-6160(83)90192-X ↗
4. 10.1016/0925-8388(94)01465-510.1016/0925-8388(94)01465-5 ↗
5. Jaeger D.M. · University of Liverpool · 1994
6. Choo W.Y. · J. Mater. Sci. · 1981 · 16, 1285
7. Goodwin, P.S., and Ward-Close, C.M.Materials Science Forum, 179–181, 411 (1995).10.4028/www.scientific.net/MSF.179-181.411 ↗
8. Korb G · 1988