‘Down’ and ‘up’ thermal shock experiments on cast and forged forms of 9/12Cr steels and their weldments at a maximum temperature of 565°C have demonstrated a marked reluctance to form traditional craze cracking and propagation into the body. However, in specimens of ex-service cast 1CrMoV material tested to the same number of cycles (1000), initiation and growth of (intergranular) cracks is much more likely in layers near the inner surface of the component than in layers deep within the section. This is due to the effect of prior thermal cycling of the inner material during start up and shut down events.Thermal shock and isothermal tests at a maximum temperature of 550°C on 1 weld features have indicated that crack propagation is generally along the fusion boundary (though for some cases, in the weld metal itself) and that cyclic growth rates lie close to an upper bound law valid for ferritic steels. The results from laboratory tests are compared with service experience as regards stresses generated, likely crack path and possibility of arrest.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Skelton R. P · High Temp. Technol. · 1990 · 8 · 7510.1080/02619180.1990.11753462 ↗
2. Skelton R. P. · High Temp. Technol. · 1984 · 2 · 2310.1080/02619180.1984.11753238 ↗
3. Skelton R. P. · High Temp. Technol. · 1987 · 5 · 310.1080/02619180.1987.11753335 ↗
4. 10.1007/978-3-7091-2516-8_210.1007/978-3-7091-2516-8_2 ↗
5. Brett S. J · 2003 · pp. 3
6. Fenton S. T. · 2003 · pp. 31
7. Rees C. J. · 1995 · pp. 135
8. 10.1179/mht.2002.02410.1179/mht.2002.024 ↗
9. Gysel W · Joint Internat. Conf on Creep · 1965 · 41 · pp. 3.33
10. Ainsworth, R. A. (ed.), R5: Assessment procedure for the high temperature response of structures, Issue 3, British Energy Generation Ltd., Barnwood, 2003.
11. 10.1098/rsta.1980.010410.1098/rsta.1980.0104 ↗
12. 10.1016/B0-08-043749-4/05122-310.1016/B0-08-043749-4/05122-3 ↗
13. Skelton R. P. · 1993 · pp. 299
14. 10.1179/mht.2004.01710.1179/mht.2004.017 ↗
15. Skelton R. P. · 1999 · pp. 683
16. 10.1016/S0013-7944(02)00089-910.1016/S0013-7944(02)00089-9 ↗
17. Rémy L. · 1992 · pp. 283
18. 10.1520/STP33958S10.1520/STP33958S ↗
19. R6: Assessment of the Integrity of Structures Containing Defects, Rev. 4, British Energy, Barnwood, UK, 2003.
20. Wells A. A · fracture mechanics and the brittle strengths of welded structures. Br Welding J. · 1965 · 12 · 2
21. Skelton R. P · Mechanical Behaviour of Materials · 1979 · 2 · pp. 13
22. 10.1016/S0013-7944(98)00110-610.1016/S0013-7944(98)00110-6 ↗
23. 10.1016/B0-08-043749-4/05021-710.1016/B0-08-043749-4/05021-7 ↗
24. Skelton R. P. · 1987 · pp. 359
25. Rees C. J · 1990 · pp. 161
26. Simpson, I. C. Superheater outlet header ligament cracking — stress analysis sensitivity study for potential replacement materials, Central Electricity Generating Board Report OED/STM/89/10007/N, 1989.
27. Proc. Internat. Seminar:Cyclic Operation of Power Plant, Shibli, I. A. et al. (eds.) London, 2001, EPRI Report No. 1004655, ISBN1-900814-45-5 (various papers).
28. Viswanathan R · 1989