Role of native metal oxide layer on emitted metal L line in low-voltage electron-probe microanalysis

Erkki Heikinheimo, Xavier Llovet

Materials at High Temperatures· Volume 26· Issue 1
Publisher page

Abstract

The thickness of the native oxide layer formed on bulk samples of metals Cu, Fe, Ni and Ti exposed to the ambient atmosphere for different exposure times, ranging from minutes up to 2500 hours, has been determined by electron-probe microanalysis (EPMA). Thicknesses were obtained by measuring the intensity of the OKα line emitted from the studied samples at varying electron incident energies, and analysing it with the help of an EPMA thin-film program. Using the thickness values obtained, the intensity loss of the metal L-line, due to the presence of the native oxide layer, has been calculated. This ranges from 5–8% at 2 keV to 1–2% at 10 keV for Cu, Fe and Ni, while for Ti it goes from 10 to 30% at 2 keV to 1–2% at 10 keV, depending on the exposure time. A correction to compensate for the metal L-line intensity loss due to the native oxide layer is discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electron and X-Ray Spectroscopy Techniques · X-ray Spectroscopy and Fluorescence Analysis · Advanced Materials Characterization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.