Crack behaviour of 10Cr-steels under creep and creep-fatigue conditions

F. Mueller, A. Scholz, C. Berger, A. Klenk, K. Maile, E. Roos

Materials at High Temperatures· Volume 25· Issue 3
Publisher page

Abstract

High-temperature components with notches, defects and flaws may be subjected to crack initiation and crack propagation under service conditions. To study these problems and to support an advanced remnant life evaluation, fracture mechanics procedures are required. Due to a more flexible service mode of power plants an increase of start up and shut down processes can be observed. Therefore knowledge of life assessment and integrity of such components is decisive.In order to enlighten these problems for steam power plant components, crack initiation time and crack growth rate of modern martensitic steels of type 10CrMoWVNbN were determined at 550 and 600°C in forged and cast conditions. For the experiments, side grooved compact tension, C(T), specimens were used as well as side grooved double edge notched tensile, DEN(T), specimens.Creep/creep-fatigue crack initiation and crack propagation can be described with the usual fracture mechanics parameters C* and KI and a modified two-criteria method was established in order to describe creep fatigue crack initiation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Kloos K. H. · 1992
2. Granacher J. · 1993
3. Berger C. · 1999
4. ECCC WG1.2. (2003)Recommendations for Creep Crack Initiation Assessments. Issue 1.
5. Berger C. · 2002
6. Granacher J. · Steel Res. · 1992 · 1 · 3910.1002/srin.199200468 ↗
7. 10.1007/978-3-642-82961-110.1007/978-3-642-82961-1 ↗
8. ASTM E 1457-00 (2000) Standard Test Method for Measurement of Creep Crack Growth Rates in Metals.
9. Irwin G. R · Trans. ASME, J AppL Mech. · 1957 · 24 · 36110.1115/1.4011547 ↗
10. Ewald, J. and Keienburg, K.H. (1986) A Two-Criteria-Dia-gram for creep crack initiation.Int. Conf on creep, Tokyo, 173 —78.
11. Fett T. · 1997
12. 10.1007/978-94-017-1771-710.1007/978-94-017-1771-7 ↗
13. 10.1016/S0308-0161(01)00085-010.1016/S0308-0161(01)00085-0 ↗
14. 10.1115/1.322585910.1115/1.3225859 ↗
15. 10.1016/S0308-0161(01)00106-510.1016/S0308-0161(01)00106-5 ↗
16. Larson ER. · Trans. ASME · 1952 · 74 · 765
17. Ewald J · 2003
18. Berger C. · 2002
19. 10.1016/S0308-0161(01)00109-010.1016/S0308-0161(01)00109-0 ↗