Abstract
Abstract Previous atomistic simulations of hydrogen embrittlement in bcc iron have provided atomistic mechanisms for crack propagation and been used to develop predictive models. In order to bridge the nano-scale simulations to realistic field operations, in current study molecular dynamics (MD) simulations were first used to predict a hydrogen concentration that corresponds to ductile to brittle transition (DTB). The estimated hydrogen concentration was then used to assess the critical hydrogen concentration that induces DTB transition in experimental specimens. Apparently, the calculated critical hydrogen concentration is much larger than the actual concentration found in pipeline steel under routine operations. Recent experiments found that while the presence of minor cycles (i.e., R = Kmin/Kmax > 0.9) in underload spectra would only make small contribution to crack propagation in air, they could enhance crack growth significantly in the presence of hydrogen atoms. Therefore, it is reasonable to expect that minor cycles have a significant effect on accumulating hydrogen atoms in the plastic zone and inducing a DTB transition in the aqueous environment where diffusible hydrogen atoms can be generated. Based on this hypothesis, the theoretical critical hydrogen value obtained from atomistic simulation was then used to calculate the number of hydrogen atoms required to saturate the plastic zone. Furthermore, the number of minor cycles required to accumulate hydrogen atoms to cause a DTB transition could be assessed. The prediction based on this model and experimental results are in good agreement. The atomistic mechanism for DTB due to the accumulation of hydrogen during cyclic loading validated in current study implies the importance of the loading spectrum in hydrogen-assisted cracking.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
2. Hydrogen hardening effect in heavily deformed single crystal α-Fe10.1016/j.commatsci.2011.06.036 ↗
3. Semiempirical, quantum mechanical calculation of hydrogen embrittlement in metals10.1103/PhysRevLett.50.1285 ↗
4. A nanoscale study of dislocation nucleation at the crack tip in the nickel-hydrogen system10.1007/s11661-010-0451-8 ↗
5. Mechanisms of hydrogen-enhanced localized plasticity: an atomistic study using α-Fe as a model system10.1016/j.actamat.2014.01.008 ↗
6. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)10.1007/BF02642048 ↗
7. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
8. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
9. Interpreting hydrogen-induced fracture surfaces in terms of deformation processes: a new approach10.1016/j.scriptamat.2011.06.016 ↗
10. Testing continuum concepts for hydrogen embrittlement in metals using atomistics10.1088/0965-0393/18/4/045003 ↗
11. Simulation of hydrogen assisted stress corrosion cracking using the cohesive model10.1016/j.engfracmech.2007.10.002 ↗
12. A nanoscale mechanism of hydrogen embrittlement in metals10.1016/j.actamat.2010.11.019 ↗
13. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
14. Hydrogen diffusion and hydrogen influenced critical stress intensity in an API X70 pipeline steel welded joint – experiments and FE simulations10.1016/j.ijhydene.2012.05.005 ↗
15. Hydrogen diffusivities and concentrations in 520M carbon steel under cathodic protection in 0.5M NaCl and the effect of added sulphite, dithionite, thiosulphate, and sulphide10.1016/S1452-3981(23)17054-4 ↗
16. Hydrogen permeation in metals as a function of stress, temperature and dissolved hydrogen concentration10.1098/rspa.1966.0046 ↗
17. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
18. Atomic mechanism and prediction of hydrogen embrittlement in iron10.1038/nmat3479 ↗
19. Corrosion fatigue crack growth behavior of pipeline steel under underload-type variable amplitude loading schemes10.1016/j.actamat.2015.05.049 ↗
20. Hydrogen-enhanced local plasticity at dilute bulk H concentrations: the role of H – H interactions and the formation of local hydrides10.1016/j.actamat.2011.01.037 ↗
21. Computational modelling of hydrogen embrittlement in welded structures
22. Simulation of crack growth during hydrostatic testing of pipeline steel in near-neutral pH environment10.1016/j.corsci.2010.11.029 ↗
23. T.L. Anderson, Fracture Mechanics, Fundamentals and Applications, 3rd ed., 2005.10.1201/9781420058215 ↗
24. Underload-induced crack growth behaviour of minor cycles of pipeline steel in near-neutral pH environment10.1111/ffe.12274 ↗
25. Equation of state calculations by fast computing machines10.1063/1.1699114 ↗
26. Galilean-invariant Nosé-Hoover-type thermostats10.1103/PhysRevE.91.033312 ↗
27. Kinetic moments method for the canonical ensemble distribution10.1016/0375-9601(95)00973-6 ↗
28. Embedded-atom method: derivation and application to impurities, surfaces, and other defects in metals10.1103/PhysRevB.29.6443 ↗
29. Development of new interatomic potentials appropriate for crystalline and liquid iron10.1080/14786430310001613264 ↗
30. Interatomic potentials for hydrogen in α –iron based on density functional theory10.1103/PhysRevB.79.174101 ↗
31. Fast parallel algorithms for short-range molecular dynamics10.1006/jcph.1995.1039 ↗
32. Atomistic study of hydrogen distribution and diffusion around a {112}〈111〉 edge dislocation in alpha iron10.1016/j.actamat.2008.04.011 ↗
33. Atomistic simulations of hydrogen embrittlement10.1016/j.ijhydene.2009.09.052 ↗
34. Estimates from atomic models of tension-shear coupling in dislocation nucleation from a crack tip10.1016/0921-5093(93)90370-T ↗
35. The phenomena of rupture and flow in solids10.1098/rsta.1921.0006 ↗
36. First principles assessment of ideal fracture energies of materials with mobile impurities: implications for hydrogen embrittlement of metals10.1016/j.actamat.2004.06.037 ↗
37. Binding energy of hydrogen to mixed and screw dislocation
38. Hydrogen effect against hydrogen embrittlement10.1007/s11661-010-0275-6 ↗
39. Origins and implications of temperature-dependent activation energy barriers for dislocation nucleation in face-centered cubic metals10.1016/j.actamat.2009.05.024 ↗
40. Prediction of crack propagation under cyclic loading based on hydrogen diffusion10.1016/j.matlet.2015.03.045 ↗
41. ScienceDirect Dislocation density distribution around an indent in single-crystalline nickel: comparing nonlocal crystal plasticity finite-element predictions with experiments10.1016/j.actamat.2014.03.012 ↗
42. A mechanistic study of the temperature dependence of the stress corrosion crack growth rate in SUS316 stainless steels exposed to PWR primary water10.1016/j.actamat.2016.05.010 ↗
43. A microstructural based understanding of hydrogen-enhanced fatigue of stainless steels10.1016/j.ijfatigue.2012.08.009 ↗
44. Relationship between fatigue crack growth behaviour and local hydrogen concentration near crack tip in pipeline steel10.1016/j.ijfatigue.2012.05.017 ↗