journal article·1999-08

The transverse strain response of cross-plied fibre-reinforced ceramic-matrix composites

Eddy Vanswijgenhoven, Martine Wevers, Omer Van Der Biest

Composites Science and Technology· Volume 59· Issue 10
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Composite Material Mechanics · Rock Mechanics and Modeling

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. The physics and mechanics of fibre-reinforced brittle matrix composites10.1007/BF00355946 ↗
2. Tensile performance of carbon-fibre-reinforced glass10.1007/BF01174049 ↗
3. Mechanical behavior of unidirectional SiC/BMAS ceramic composites
4. Crack initiation in unidirectional brittle-matrix composites10.1111/j.1151-2916.1991.tb04346.x ↗
5. Matrix cracking and the mechanical behaviour of SiC-CAS composites10.1098/rspa.1992.0050 ↗
6. Characterization and modeling of microcracking and elastic moduli changes in Nicalon/CAS composites10.1016/0266-3538(93)90159-E ↗
7. Micromechanical analysis of damage mechanisms in ceramic matrix composites during mechanical and thermal cycling10.1016/0010-4361(93)90009-W ↗
8. Effect of fibre roughness on the overall stress–transverse strain response of ceramic composites10.1016/0956-716X(93)90079-8 ↗
9. Effect of off-axis loading on the tensile behavior of a ceramic-matrix composite10.1111/j.1151-2916.1996.tb08085.x ↗
10. The relationship between longitudinal stress and transverse strain during tensile testing of unidirectional fibre toughened ceramic matrix composites10.1016/S1359-6454(97)00006-2 ↗
11. Transverse strain response of Hi-Nicalon fibre reinforced silicon nitride matrix composites10.1016/S1359-6462(97)00382-5 ↗
12. Acoustic emission during tensile testing of SiC-fibre-reinforced BMAS glass–ceramic composites10.1016/S1359-835X(96)00147-9 ↗
13. Poisson’s ratio as a damage parameter in the static tensile loading of simple crossply laminates10.1016/0266-3538(90)90073-E ↗
14. Ply cracking and property degradations of symmetric balanced laminates under general in-plane loading10.1016/0266-3538(89)90059-6 ↗
15. Multiple matrix cracking in brittle matrix composites10.1016/0956-7151(93)90246-O ↗
16. The role of interfaces in fiber-reinforced brittle matrix composites10.1016/0266-3538(91)90010-M ↗
17. Tsai SW, Hahn HT. Introduction to composite materials. Lancaster: Technomic Publishing Company, 1980.
18. Analysis of composite materials—a survey10.1115/1.3167081 ↗
19. Thermal expansion coefficients of composite materials based on energy principles10.1177/002199836800200308 ↗
20. Behaviour of unidirectional and crossply ceramic matrix composites under quasi-static tensile loading10.1007/BF00540692 ↗
21. Damage mechanisms and the mechanical properties of a laminated 0/90 ceramic/matrix composite10.1111/j.1151-2916.1992.tb04428.x ↗
22. On multiple transverse cracking in glass fibre epoxy cross-ply composites10.1007/BF00541666 ↗
23. Matrix cracking in crossply ceramic matrix composites under quasi-static and cyclic loading10.1016/0956-7151(94)90281-X ↗
24. Definition and measurement of the shear-lag parameter, β, as an index of the stress transfer efficiency in polymer composites10.1023/A:1004357121802 ↗
25. Theory of mechanical properties of ceramic-matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
26. Matrix cracking in unidirectional ceramic matrix composites under quasi-static and cyclic loading10.1016/0956-7151(93)90178-U ↗
27. Models of fiber debonding and pullout in brittle composites with friction10.1016/0167-6636(90)90037-G ↗
28. Residual stresses in fiber-reinforced ceramics due to thermal expansion mismatch10.1111/j.1151-2916.1993.tb03988.x ↗
29. The role of coating compliance and fiber/matrix interfacial tomography on debonding in ceramic composites10.1016/0956-716X(95)90828-8 ↗
30. Relationships between hysteresis measurements and the constituent properties of ceramic matrix composites: II. experimental studies on unidirectional materials10.1111/j.1151-2916.1995.tb08047.x ↗
31. Surface roughness characterization of Nicalon and Hi-Nicalon ceramic fibers by atomic force microscopy10.1016/1044-5803(95)00103-6 ↗
32. Comparative study of the surface roughness of different Tyranno and Nicalon silicon carbide fibres10.1016/S1359-835X(98)00036-0 ↗
33. The one-dimensional car parking problem and its application to the distribution of spacings between matrix cracks in unidirectional fiber-reinforced brittle materials10.1111/j.1151-2916.1992.tb05456.x ↗