journal article·1999-02

Effects of environment on the high-temperature strength of ZrSiO4-matrix/SiC-fiber composites

J.A Celemı́n, J.Y Pastor, J LLorca, U Anandakumar, R.N Singh

Composites Science and Technology· Volume 59· Issue 2
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Mechanical behaviour at 20°C and 1200°C of Nicalon. SiC fiber-reinforced Al2O3-matrix composites10.1111/j.1151-2916.1997.tb03159.x ↗
2. Advances in ceramic composites reinforced by continuous fibers10.1016/S1359-0286(96)80049-0 ↗
3. Theory of the mechanical properties of ceramic-matrix composites10.1111/j.1151-2916.1991.tb06852.x ↗
4. Fibers for structurally reliable metal and ceramic composites
5. Creep of chemically vapour deposited SiC fibres10.1007/BF01144723 ↗
6. High temperature mechanical behaviour of an uncoated SiC-SiC composite material10.1007/BF00543620 ↗
7. Oxidation embrittlement probe for ceramic-matrix composites10.1111/j.1151-2916.1995.tb08621.x ↗
8. Effect of interfacial shear strength on crackfiber interaction behavior in ceramic matrix composites10.1111/j.1151-2916.1996.tb07899.x ↗
9. SiC/SiC Composite ceramics
10. Lehman RL, El-Rahaiby SK, Wachtman JB, editors. Handbook on continuous fiber-reinforced ceramic matrix composites. Westerville, Ohio:American Ceramic Society, 1995.
11. Microstructural influences on the creep behaviour of CVD silicon carbide monofilaments
12. Influence of fiber and interfacial properties on fracture behavior of fiber-reinforced ceramic composites10.1111/j.1151-2916.1991.tb06858.x ↗
13. Interface materials for damage-tolerant oxide composites10.4028/www.scientific.net/KEM.127-131.27 ↗
14. Nair SV, Jakus K, editors. High temperature mechanical behaviour of ceramic composites. Boston:Butterworth-Heinemann, 1995.
15. The microstructure of the SCS-6 SiC fiber10.1557/JMR.1991.2234 ↗
16. Stable crack growth in ceramics at ambient and elevated temperature10.1115/1.2904219 ↗
17. A new technique for fracture characterization of ceramics at room and at high temperature10.1520/JTE10412J ↗
18. Fiber reinforced glasses and glass-ceramics for high performance applications
19. Silicon carbide fibre reinforced glass-ceramic composite tensile behaviour at elevated temperature10.1007/BF02397074 ↗
20. Interfacial properties and high temperature mechanical behavour of fiber reinforced composites10.1016/0921-5093(93)90322-6 ↗
21. Mechanical behavior of SiC(f)/SiC composites and correlation to in situ fiber strength at room and elevated temperatures10.1111/j.1151-2916.1996.tb07915.x ↗
22. Influence of residual stresses, interface roughness, and fiber coatings on interfacial properties in ceramic composites10.1111/j.1151-2916.1996.tb07891.x ↗
23. Creep and rupture of advanced ceramic fiber reinforcements
24. Testing the tensile properties of ceramic-matrix composites10.1007/BF03223222 ↗