Effect of seawater on compressive strength of concrete cylinders reinforced by non-adhesive wound hybrid polymer composites

Hsien-Kuang Liu, Nyan-Hwa Tai, Wen-Hung Lee

Composites Science and Technology· Volume 62· Issue 16
Publisher page

Abstract

Seawater absorption in concrete structures can be a serious problem in humid and marine environments. It was demonstrated that non-adhesive (separated by aluminum foil) filament wound tubes could better reinforce concrete cylinders. Furthermore, composites have ever proved to be resistant to detrimental environment. Therefore, in this study four kinds of non-adhesive composite materials are used to reinforce concrete cylinders, and then composite/concrete systems are subjected to six environmental conditions. The composites include hand-wrapped woven cloth glass/epoxy, filament wound glass/epoxy, glass-kevlar-glass hybrid, and glass-carbon-glass hybrid. These allow comparing reinforcement effect from various processing methods, fibers, and interface. The six environmental conditions consist of soaking in live or dead seawater, soaking before or after winding, and air aging before or after winding. The first and second conditions can verify the accuracy of the experiment in laboratory (dead seawater) without bothering to test near coast (live seawater). The third to sixth conditions can provide a good designing criterion regarding what the best sequence is for reinforcing seawater or air attacked concrete structure by composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Structural Behavior of Reinforced Concrete · Innovative concrete reinforcement materials · Structural Response to Dynamic Loads

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Filament winding cylinders10.1177/002199839002401202 ↗
2. Filament winding cylinders10.1177/002199839002401203 ↗
3. Filament winding cylinders10.1177/002199839002401204 ↗
4. Compressive strength of composite/concrete cylinders after low energy impact10.1177/073168401772678968 ↗
5. Compression after impact (CAI) strength of concrete cylinders reinforced by non-adhesive filament wound composites10.1002/pc.10184 ↗
6. Compression strength of concrete cylinders reinforced by non-adhesive filament wound hybrid composites10.1016/S1359-835X(99)00075-5 ↗
7. Composite wraps for aging infrastructure10.1016/S0263-8223(97)00041-X ↗
8. Interactions between hygrothermal aging and fatigue damage in unidirectional glass/epoxy composites10.1016/S0266-3538(97)00149-8 ↗
9. Composite degradation due to fluid absorption10.1016/S1359-8368(00)00025-1 ↗
10. A study of the coupling between the phenomena of water absorption and damage in glass/epoxy composite pipes10.1016/S0266-3538(97)00076-6 ↗
11. Durability characteristics of concrete columns confined with advanced composite materials10.1016/S0263-8223(98)00125-1 ↗
12. Effects of freeze-thaw exposure on performance of concrete columns strengthened with advanced composites
13. Durability characteristics of concrete beams externally bonded with FRP composite sheets10.1016/S0958-9465(97)00028-0 ↗