journal article·2001-02

Physico-chemistry of interfaces in inorganic-matrix composites

J. Bouix, M.P. Berthet, F. Bosselet, R. Favre, M. Peronnet, O. Rapaud, J.C. Viala, C. Vincent, H. Vincent

Composites Science and Technology· Volume 61· Issue 3
Publisher page

Abstract

The performances of metal matrix composites (MMCs) or ceramic matrix composites (CMCs) are usually limited by the characteristics of the fibre/matrix interface or more generally those of the interfacial zone. Concerning MMCs, the optimization of this zone involves control of the chemical reactivity between the reinforcement and the matrix, which constitute usually an out-of-equilibrium system. In the case of CMCs, it is possible to obtain a non-brittle material by associating two brittle components and to exhibit a good resistance to oxidation. The physical chemist is able to offer a significant contribution for solving these problems by acting on the reinforcement surface, the matrix composition or the manufacturing conditions of the composite.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical and Alloy Processes · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Chawla KK. In: Cahn RW, Haasen P, Kramer EJ, editors. Materials Science and Technology, vol. 13. Weinheim: VCH, 1993. p. 121–182.
2. Maruyama B, Barera EV, Rabenberg L. In: Everett RK and Arsenault RJ, editors. Metal matrix composites processing and interfaces. New York: Academic Press, 1991. p. 181–216.10.1016/B978-0-12-341832-6.50013-X ↗
3. Rebillat F, Guette A, Debieuvre C, Goujard S, Naslain R. Interphase multicouche BN pour composites SiC/SiC à ténacité et durée de vie améliorée. In: Lamon J, Baptiste D, editors. JNC11. Arcachon (France): AMAC, 1998. p. 575–584.
4. Interface tailoring in carbon fibres reinforced metal matrix composites10.1051/jp4:1997616 ↗
5. Procédé et dispositif de revêtement de fibres de carbone par un carbure et fibres de carbone ainsi revêtues
6. Bouix J, Viala JC, Vincent H, Vincent C, Ponthenier JL, Dazord J. Process for coating carbon fibre with a carbide. US patent 4 859 503, 1989.
7. Preparation of B4C–SiC composites by RCVD from BCl3–SiCl4–H2 phase10.1080/09603409.1995.11689497 ↗
8. Pastor S, Vincent C, Berthet MP, Oddou L, Vincent H, Bouix J. Aspects physicochimiques des procédés RCVD et LMTA de traitement de surface permettant l'infiltration spontanée des fibres de carbone par l'aluminium. In: Favre JP, Vautrin A, editors. JNC9. Saint-Etienne (France): AMAC, 1994. p. 1145–54.
9. Processing of polymeric precursors ceramic matrix composites10.1557/PROC-120-157 ↗
10. Héraut L, Naslain R, Quenisset JM. Procédé de fabrication d'un matériau composite à matrice céramique à ténacité améliorée. Brevet Fr 89 02918, 1989.
11. Droillard C. Elaboration et caractérisation de composites à matrice SiC et à interphase séquencée C/SiC. Thèse de doctorat Sciences des Matériaux, Université de Bordeaux, 1993.
12. Heurtevent F. Matériaux multicouches nanoséquencés (PyC/SiC)n. Application en tant qu'interphases dans les composites thermostructuraux. Thèse de doctorat Sciences des Matériaux, Université de Bordeaux, 1996.
13. Thermal degradation of fiber coatings in mullite–fiber-reinforced mullite composite10.1111/j.1151-2916.1997.tb03099.x ↗
14. Fracture behavior of multilayer silicon nitride/boron nitride ceramics10.1111/j.1151-2916.1996.tb08996.x ↗
15. Chen SH, Davis HO. Structural ceramic material having refractory interface layers. US Patent 4 837 230, 1989.
16. Rebillat F. Caractérisation des interfaces et des matériaux d'interphases dans les CMCs. Thèse de doctorat Sciences des Matériaux, Université de Bordeaux, 1996.
17. Stable and metastable phase equilibria in the chemical interaction between Al and SiC10.1007/BF01045395 ↗
18. Approche thermodynamique de l'interaction chimique entre Al et TiC10.1016/0025-5408(90)90181-Z ↗
19. The chemical reactivity of aluminium with boron carbide B4C10.1023/A:1018625402103 ↗
20. Effect of magnesium on the composition, microstructure and mechanical properties of carbon fibres10.1007/BF00549880 ↗
21. Synthesis and structure of T2–Al2MgC210.1016/S0992-4361(98)80017-9 ↗
22. Bouix J, Viala JC, Abiven H, Picouet L, Claveyrolas J. Composite material combining a magnesium alloy containing zirconium with a carbon reinforcement and its production process. US Patent Demand 08 120 249, 1996.