journal article·1996-01

Influence of the metal/ceramic interface on the microstructure and mechanical properties of HIPed iron-based composites

E. Pagounis, M. Talvitie, V.K. Lindroos

Composites Science and Technology· Volume 56· Issue 11
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. HIPed wear resistant steel-matrix MMCs
2. Ferro-TiC metal matrix composites for high performance tooling and engineering applications
3. Microstructure and properties of ceramic reinforced super-duplex stainless steel
4. Characterisation of interfacial layer between nitrogen alloyed stainless steel and alumina in a metal matrix composite10.1016/0956-716X(94)90268-2 ↗
5. Wear resistant alloy bonded carbides produced by PM
6. Neue korrosions- und verschleissfeste, bearbeitbare hartstoffe: Ferro-Titanit fuer die chemische technik10.1002/maco.19790301208 ↗
7. Mechanical behaviour of sintered ferritic stainless steel-Al2O3 particulate composites containing ternary additions10.1016/0025-5416(85)90178-8 ↗
8. Steel bonded hardmetals
9. Sintered steels with high content of hard phases: A new class of wear resistant materials
10. Solidification processing and tribological behaviour of particulate TiC-ferrous matrix composites10.1016/0921-5093(90)90232-R ↗
11. Carbothermic reduction of ilmenite and rutile as means of production of iron based Ti(O,C) metal matrix composites10.1179/mst.1991.7.9.842 ↗
12. Dispersion and reaction of TiC in liquid iron alloys10.1179/mst.1992.8.5.399 ↗
13. Toughness in metal matrix composites10.1179/mst.1989.5.1.1 ↗
14. X-ray method of measuring retained austenite in heat treated white cast irons10.1007/BF02833237 ↗
15. Bonding, structure and properties of metal/ceramic interfaces: 1. Chemical bonding, chemical reaction, and interface structure10.1179/imr.1993.38.5.233 ↗
16. Effects of alloying on structural stability and cohesion between phases in oxide/metal composites10.1179/030634572790445803 ↗
17. Hondros · 1978 · 1
18. Changes in the chemical and phase composition of a Cr3C2 particle in contact with an iron matrix during sintering
19. Effect of thermal expansion coefficients on the martensitic transformation in a steel matrix composite10.1016/0956-716X(95)00529-5 ↗
20. Criterion for the action of applied stress in the martensitic transformation10.1016/0001-6160(53)90083-2 ↗
21. Deformation-induced martensitic transformation and transformation-induced plasticity in steels10.1179/030634582790427316 ↗
22. Aging characteristics of B4C-reinforced 6061-aluminium10.1016/0036-9748(84)90083-8 ↗
23. Influence of dislocation density and distribution on the aging behaviour of 6061 Al-SiCw composites10.1016/0956-7151(90)90071-N ↗
24. Accelerated aging in cast Al alloy-SiC particulate composites10.1016/0036-9748(89)90136-1 ↗
25. Microstructural development in an aluminium alloy-SiC whisker composite10.1016/0001-6160(88)90236-2 ↗
26. Nishiyama · 1978 · 269
27. Plastic relaxation of thermoelastic stress in maluminium/ceramic composites10.1007/BF02671938 ↗
28. Abrasive wear of two-phase metallic materials with a coarse microstructure
29. Pagounis, E., Talvitie, M. & Lindroos, V. K., Influence of matrix structure on the abrasion wear resistance and toughness of a HIPed white iron matrix composite. Metall. Mater. Trans. A (in press).
30. Crack deflection process—I. Theory10.1016/0001-6160(83)90046-9 ↗
31. Effect of particle size on fracture toughness of SiC/Al composite material10.1016/0001-6160(89)90039-4 ↗