Hot deformation behavior of in situ nano ZrB2 reinforced 2024Al matrix composite
Source abstract
Abstract
Abstract The hot deformation behavior of in situ 5 wt.% nano ZrB 2 /2024Al composite was studied at deformation temperatures of 350–450 °C and strain rates of 0.001–10 s −1 . The results show that the flow stress depends strongly on the deformation temperature and strain rate, and especially exhibits a strain hardening at high temperature and high strain rate, related to the introduction of nanoparticles (ZrB 2 : 15–40 nm). The kinetic equation was constituted and indicates that the key deformation mechanism is dynamic recrystallization (DRX), which is in accordance with the deformed microstructures. The processing maps (PMs) exhibit two deterministic domains of domain 1 (380–410 °C/0.018–0.032 s −1 ) and domain 2 (440–460 °C/0.075–0.56 s −1 ), where domain 2 has the higher power dissipation efficiency, higher strain rate, meaning more safety and higher efficiency for the hot processing. At the same time, the deformed specimen exhibits equiaxed and fine grains in domain 2, i.e., a typical DRX structure, thus is suggested as the optimum hot processing window for this nanocomposite.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Strong and ductile particulate reinforced ultrafine-grained metallic composites fabricated by flake powder metallurgy10.1016/j.scriptamat.2012.11.024 ↗
2. Hot deformation behavior of mechanically alloyed Al6063/0.75Al2O3/0.75Y2O3 nano-composite – a study using constitutive modeling and processing map10.1016/j.msea.2012.01.109 ↗
3. Hot workability and deformation mechanisms in Mg/nano-Al2O3 composite10.1016/j.compscitech.2009.01.032 ↗
4. On the hot working characteristics of 6061Al–SiC and 6061–Al2O3 particulate reinforced metal matrix composites10.1016/S0266-3538(02)00197-5 ↗
5. Forming behavior and workability of 6061/B4CP composite during hot deformation10.1016/j.compscitech.2011.02.009 ↗
6. Equal channel angular pressing of metal matrix composites: effect on particle distribution and fracture toughness10.1016/j.actamat.2005.07.010 ↗
7. Superplastic deformation mechanism of an ultrafine-grained aluminum alloy produced by friction stir processing10.1016/j.actamat.2010.05.003 ↗
8. Enhanced strength and ductility in ultrafine-grained aluminium produced by accumulative roll bonding10.1002/adem.200306582 ↗
9. Enhanced superplasticity in equal-channel angularly pressed Sn–5Sb alloy10.1016/j.scriptamat.2010.11.030 ↗
10. High-strength nanostructured Al/B4C composite processed by cross-roll accumulative roll bonding10.1016/j.msea.2011.12.101 ↗
11. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
12. In situ fabrication and microstructure of Al2O3 particles reinforced aluminum matrix composites10.1016/j.msea.2010.01.022 ↗
13. In situ (Al2O3+Al3Zr)(np)/Al nanocomposites synthesized by magneto-chemical melt reaction10.1016/j.compscitech.2007.10.036 ↗
14. Effects of in situ generated ZrB2 nano-particles on microstructure and tensile properties of 2024Al matrix composites10.1016/j.jallcom.2014.01.117 ↗
15. In situ fabrication and microstructure of micro-nano ZrB2p/Al composites
16. Hot deformation behavior of GH4169 superalloy associated with stick 8 phase dissolution during isothermal compression process10.1016/j.msea.2012.01.121 ↗
17. Hot deformation and processing map of 2519A aluminum alloy10.1016/j.msea.2010.10.080 ↗
18. Deformation behavior and microstructural evolution of as-cast 904 L austenitic stainless steel during hot compression10.1016/j.msea.2012.12.043 ↗
19. Constitutive equation and processing map for hot deformation of SiC particles reinforced metal matrix composites10.1007/s11665-010-9611-7 ↗
20. Microstructure evolutions of SiCp/AZ91 Mg matrix composites during hot compression10.1016/j.msea.2012.08.054 ↗
21. Superplastic tensile characteristics of in situ TiBw/Ti6Al4V composites with novel network microstructure10.1016/j.msea.2013.05.076 ↗
22. Constitutive relationships for hot deformation of austenite10.1016/j.actamat.2011.07.008 ↗
23. Strength and structure under hot-working conditions10.1179/095066069790138056 ↗
24. Behavior and modeling of high temperature deformation of an α+β titanium alloy10.1016/j.msea.2012.06.039 ↗
25. Effect of strain rate upon plastic flow of steel10.1063/1.1707363 ↗
26. Rate-controlling mechanisms of hot deformation in a medium carbon vanadium microalloy steel10.1016/j.msea.2012.08.095 ↗
27. General expression of the Zener–Hollomon parameter as a function of the chemical composition of low alloy and microalloyed steels10.1016/1359-6454(95)00151-0 ↗
28. Characterization of hot deformation behavior of as-cast TC21 titanium alloy using processing map10.1016/j.msea.2010.11.015 ↗
29. The effects of strain rate and temperature on the compressive deformation behaviour of Ti6Al4V alloy
30. Enhanced tensile plasticity in ultrafine-grained metallic composite fabricated by friction stir process10.1016/j.scriptamat.2008.06.040 ↗
31. Optimum parameters and rate-controlling mechanisms for hot working of extruded Mg–3Sn–1Ca alloy10.1016/j.msea.2008.10.041 ↗
32. On the development of instability criteria during hotworking with reference to IN 71810.1016/S0921-5093(98)00764-3 ↗
33. Processing maps and rate controlling mechanisms of hot deformation of electrolytic tough pitch copper in the temperature range 300–950°C10.1016/j.msea.2004.08.049 ↗