Surface integrity and corrosion performance of biomedical magnesium-calcium alloy processed by hybrid dry cutting-finish burnishing

M. Salahshoor, C. Li, Z.Y. Liu, X.Y. Fang, Y.B. Guo

Publisher page

Abstract

Biodegradable magnesium-calcium (MgCa) alloy is a very attractive orthopedic biomaterial compared to permanent metallic alloys. However, the critical issue is that MgCa alloy corrodes too fast in the human organism. Compared to dry cutting, the synergistic dry cutting-finish burnishing can significantly improve corrosion performance of MgCa0.8 (wt%) alloy by producing a superior surface integrity including good surface finish, high compressive hook-shaped residual stress profile, extended strain hardening in subsurface, and little change of grain size. A FEA model was developed to understand the plastic deformation of MgCa materials during burnishing process. The measured polarization curves, surface micrographs, and element distributions of the corroded surfaces by burnishing show an increasing and uniform corrosion resistance to simulated body fluid.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Magnesium Alloys: Properties and Applications · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Bach, F., Denkena, B., Weinert, K., Alpers, P., Bosse, M., Hammer, N., 2007. Influence of cutting and non-cutting processes on the corrosion behavior and the mechanical properties of magnesium alloys. In: Proceedings of the 7th International Conference on Magnesium Alloys and their Applications. pp. 1076–1084.
2. Modeling large deformation and failure in manufacturing processes
3. Brooks · 2009
4. Biocompatible magnesium alloys as absorbable implant materials–adjusted surface and subsurface properties by machining processes10.1016/j.cirp.2007.05.029 ↗
5. Denkena, B., Becker, J., Podolsky, C., Kuhlmann, A., 2005. Safe machining of magnesium parts by cutting and burnishing operations. In: Proceedings of the 7th International Conference on Magnesium Alloys and their Applications. pp. 895–901.10.1002/3527603565.ch139 ↗
6. Process mechanics and surface integrity by high-speed dry milling of biodegradable magnesium–calcium implant alloys10.1016/j.cirp.2010.03.051 ↗
7. HKS, 2008. ABAQUS User’s Manual, ver. 6.8. Providence, RI.
8. Influence of different surface machining treatments of magnesium‐based resorbable implants on the degradation behavior in rabbits10.1002/adem.200800273 ↗
9. The role of implant surface characteristics in the healing of bone10.1177/10454411960070040301 ↗
10. Roller burnishing of hard turned surfaces10.1016/S0890-6955(97)00085-0 ↗
11. Case studies of fatigue life improvement using low plasticity burnishing in gas turbine engine applications
12. Ultrafine-grained surface layer on Mg–Al–Zn alloy produced by cryogenic burnishing for enhanced corrosion resistance10.1016/j.scriptamat.2011.06.013 ↗
13. Surface integrity of magnesium-calcium implants processed by synergistic dry cutting-finish burnishing
14. Process mechanics in ball burnishing biomedical magnesium–calcium alloy10.1007/s00170-012-4024-4 ↗
15. An analysis of the residual stresses generated in Inconel 718™ when turning10.1016/j.jmatprotec.2005.12.007 ↗
16. Formation of flank build-up in cutting magnesium alloys10.1016/S0007-8506(07)61938-6 ↗
17. The influence of tool coatings in machining of magnesium
18. Tönshoff, H., Friemuth, T., Winkler, J., Podolsky, C., 2006. Improving the characteristics of magnesium workpieces by burnishing operations. In: Proceedings of the 7th International Conference on Magnesium Alloys and their Applications. pp. 406–411.10.1002/3527607552.ch65 ↗