Abstract

Abstract The Newman and Raju formula for the stress intensity factor of a semi-elliptical surface crack loaded in uniaxial tension or in bending has been developed about 30 years ago using an FE-analysis for several geometric parameters and fitting an empirical equation to the data points. The Poisson's ratio analyzed was 0.3. In this paper a reassessment of the Newman and Raju formula is made, where all relevant geometric parameters of crack and specimen and the Poisson's ratio are considered. The deviations of the old formula from the new results are up to 21%, if the full range of Poisson's ratio is taken into account. Furthermore the influence of the crack-surface intersection angle is discussed. The results of this work are important for more precise fracture toughness measurements in brittle materials and give a practical guidance for appropriate specimen preparation for fracture toughness measurements, which is also considered here.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · Ultrasonics and Acoustic Wave Propagation · Numerical methods in engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Lawn · 1993
2. Munz · 2001
3. Fett · 1997
4. Murakami · 1987
5. An empirical stress-intensity factor equation for the surface crack10.1016/0013-7944(81)90116-8 ↗
6. Raju IS, Newman JC. Improved stress-intensity factors for semi-elliptical surface cracks in finite-thickness plates. NASA Report TM-X-72825; 1977
7. Newman JC, Raju IS. Analysis of srface cracks in finite plates under tension or bending loads. NASA. Report TP-1578; 1979.
8. Shackelford · 1994
9. Field · 1992
10. Czichos · 2008
11. Tension and bending of finite thickness plates with a semi-elliptical surface crack10.1007/BF01140626 ↗
12. McGowan · 1980
13. A review and assessment of the stress intensity factor for surface cracks
14. The elastic analysis of part-circular surface flaw problems by the alternation method
15. Stress intensity factors for a part-circular surface flaw
16. Fracture toughness by the surface crack in flexure (SCF) method: results of the VAMAS Round Robin10.1002/9780470314555.ch30 ↗
17. Quinn GD, Kübler J, Gettings RJ. Fracture toughness of advanced ceramics by the surface crack in flexure (SCF) method: a VAMAS Round Robin. VAMAS Report No. 17. Report 1994.
18. Fett · 2009
19. Anderson · 2005
20. Advantages of the J-integral approach for calculating stress intensity factors when using the commercial finite element software ABAQUS10.1016/j.engfracmech.2005.02.003 ↗
21. The influence of the Poisson's ratio and corner point singularities in three-dimensional plasticity-induced fatigue crack closure: a numerical study10.1016/j.ijfatigue.2008.01.009 ↗
22. Zúñiga DF, Kalthoff JF, Canteli AF, Grasa J, Doblaré M. Three dimensional effects along the crack front influencing the validity criteria for determining fracture toughnesses. 11th International Conference on Fracture, Turin (Italy): 2005.
23. Stress intensity factors for semi-elliptical surface cracks in a plate under tension based on the Isida's solution10.1007/BF00018395 ↗
24. ASTM C 1421-01b · 2001
25. ISO 18756 · 2003
26. Quantification of the influence of vertex singularities on fatigue crack behavior10.1016/j.commatsci.2008.08.009 ↗
27. The effect of a free surface on fatigue crack behaviour10.1016/j.ijfatigue.2010.01.009 ↗
28. Fracture mechanics of the three-dimensional crack front: vertex singularity versus out of plain constraint descriptions10.1016/j.proeng.2010.03.225 ↗