Zirconium oxide and the crystallinity hallows

Roberto Nisticò

Publisher page

Abstract

Zirconium oxide is one of the most promising ceramic materials as it finds applications in several high-level technological fields, ranging from biomedicine to sensing. Zirconium oxide is characterized by showing very uncommon properties for being a ceramic substrate, such as a certain plastic behavior once subjected to mechanical stress, a naturally occurring phase transformation toughening, as well as a dramatic sensibility toward water-induced aging (if hydrothermally treated). In general, all these properties are strictly correlated with the tetragonal-to-monoclinic interphase transformation and, consequently, driven by the stabilization of the tetragonal phase. Hence, in this study, a summary of the main relevant principles guiding zirconium oxide interphase transformations is proposed, highlighting the important role of stabilizers and the correlation between microstructure and doping. A particular emphasis has been dedicated to the thermodynamics behind these phenomena.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. Iranmanesh, M., Hulliger, J.: Ceramic combinatorial syntheses exploring the chemical diversity of metal oxides. Prog. Solid State Chem. 44, 123–130 (2016). https://doi.org/10.1016/j.progsolidstchem.2016.11.00310.1016/j.progsolidstchem.2016.11.003 ↗
2. Chevalier, J., Gremillard, L.: 1.106 – Zirconia as a biomaterial. In: Ducheyne, P. (ed.) Comprehensive biomaterials, pp. 95–108. Elsevier, Oxford (2011). https://doi.org/10.1016/B978-0-08-055294-1.00017-910.1016/B978-0-08-055294-1.00017-9 ↗
3. Wang, G., Yang, Y., Han, D., Li, Y.: Oxygen defective metal oxides for energy conversion and storage. NanoToday. 13, 23–39 (2017). https://doi.org/10.1016/j.nantod.2017.02.00910.1016/j.nantod.2017.02.009 ↗
4. Sk, M.M., Yue, C.Y., Ghosh, K., Jena, R.K.: Review on advances in porous nanostructured nickel oxides and their composite electrodes for high-performance supercapacitors. J. Power Sources. 308, 121–140 (2016). https://doi.org/10.1016/j.jpowsour.2016.01.05610.1016/j.jpowsour.2016.01.056 ↗
5. Nisticò, R.: Magnetic materials and water treatments for a sustainable future. Res. Chem. Intermed. 43, 6911–6949 (2017). https://doi.org/10.1007/s11164-017-3029-x10.1007/s11164-017-3029-x ↗
6. Palma, D., Bianco Prevot, A., Brigante, M., Fabbri, D., Magnacca, G., Richard, C., Mailhot, G., Nisticò, R.: New insights on the photodegradation of caffeine in the presence of bio-based substances-magnetic iron oxide hybrid nanomaterials. Materials. 11, 1084 (2018). https://doi.org/10.3390/ma1107108410.3390/ma11071084 ↗
7. Dey, A.: Semiconductor metal oxide gas sensors: a review. Mater. Sci. Eng. B. 229, 206–217 (2018). https://doi.org/10.1016/j.mseb.2017.12.03610.1016/j.mseb.2017.12.036 ↗
8. Nisticò, R., Scalarone, D., Magnacca, G.: Sol-gel chemistry, templating and spin-coating deposition: a combined approach to control in a simple way the porosity of inorganic thin films/coatings. Microporous Mesoporous Mater. 248, 18–29 (2017). https://doi.org/10.1016/j.micromeso.2017.04.01710.1016/j.micromeso.2017.04.017 ↗
9. Ishak, N.F., Hashim, N.A., Othman, M.H.D., Monash, P., Zuki, F.M.: Recent progress in the hydrophilic modification of alumina membranes for protein separation and purification. Ceram. Int. 43, 915–925 (2017). https://doi.org/10.1016/j.ceramint.2016.10.04410.1016/j.ceramint.2016.10.044 ↗
10. Castano, C.E., O’Keefe, M.J., Fahrenholtz, W.G.: Cerium-based oxide coatings. Curr. Opin. Solid State Mater. Sci. 19, 69–76 (2015). https://doi.org/10.1016/j.cossms.2014.11.00510.1016/j.cossms.2014.11.005 ↗
11. Piconi, C., Porporati, A.A.: Bioinert ceramics: zirconia and alumina. In: Antoniac, I. (ed.) Handbook of Bioceramics and Biocomposites, pp. 59–89. Springer, Cham (2016). https://doi.org/10.1007/978-3-319-12460-5_410.1007/978-3-319-12460-5_4 ↗
12. Fletcher, L.: The occurrence of native zirconia (baddeleyite). Nature. 47, 283–284 (1893). https://doi.org/10.1038/047283b010.1038/047283b0 ↗
13. Lumpkin, G.R.: Physical and chemical characteristics of baddeleyite (monoclinic zirconia) in natural environments: an overview and case study. J. Nucl. Mater. 274, 206–217 (1999). https://doi.org/10.1016/S0022-3115(99)00066-510.1016/S0022-3115(99)00066-5 ↗
14. Piconi, C., Maccauro, G.: Zirconia as a ceramic biomaterial. Biomaterials. 20, 1–25 (1999). https://doi.org/10.1016/S0142-9612(98)00010-610.1016/S0142-9612(98)00010-6 ↗
15. Guo, X., Waser, R.: Electrical properties of the grain boundaries of oxygen ion conductors: acceptor-doped zirconia and ceria. Prog. Mater. Sci. 51, 151–210 (2006). https://doi.org/10.1016/j.pmatsci.2005.07.00110.1016/j.pmatsci.2005.07.001 ↗
16. Rahmati, M., Mozafari, M.: A critical review on the cellular and molecular interactions at the interface of zirconia-based biomaterials. Ceram. Int. 44, 16137–16149 (2018). https://doi.org/10.1016/j.ceramint.2018.06.19610.1016/j.ceramint.2018.06.196 ↗
17. Kelly, J.R., Denry, I.: Stabilized zirconia as a structural ceramic: an overview. Dent. Mater. 24, 289–298 (2008). https://doi.org/10.1016/j.dental.2007.05.00510.1016/j.dental.2007.05.005 ↗
18. Roza, G.: Understanding the elements of periodic table, Zirconium. Rosen Publishing Group Inc., New York (2009) ISBN: 978-1435850705
19. Chevalier, J.: What future for zirconia as a biomaterial? Biomaterials. 27, 535–543 (2006). https://doi.org/10.1016/j.biomaterials.2005.07.03410.1016/j.biomaterials.2005.07.034 ↗
20. Turon-Vinas, M., Anglada, M.: Strength and fracture toughness of zirconia dental ceramics. Dent. Mater. 34, 365–375 (2018). https://doi.org/10.1016/j.dental.2017.12.00710.1016/j.dental.2017.12.007 ↗
21. Garvie, R.C., Hannink, R.H., Pascoe, R.T.: Ceramic steel? Nature. 258, 703–704 (1975). https://doi.org/10.1038/258703a010.1038/258703a0 ↗
22. Brog, J.P., Chanez, C.L., Crochet, A., Fromm, K.M.: Polymorphism, what it is and how to identify it: a systematic review. RSC Adv. 3, 16905–16931 (2013). https://doi.org/10.1039/C3RA41559G10.1039/C3RA41559G ↗
23. Hannink, R.H.J., Kelly, P.M., Muddle, B.C.: Transformation toughening in zirconia-containing ceramics. J. Am. Ceram. Soc. 83, 461–487 (2000). https://doi.org/10.1111/j.1151-2916.2000.tb01221.x10.1111/j.1151-2916.2000.tb01221.x ↗
24. Chevalier, J., Gremillard, L., Virkar, A.V., Clarke, D.R.: The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends. J. Am. Ceram. Soc. 92, 1901–1920 (2009). https://doi.org/10.1111/j.1551-2916.2009.03278.x10.1111/j.1551-2916.2009.03278.x ↗
25. Li, P., Chen, I.W., Penner-Hahn, J.E.: Effect of dopants on zirconia stabilization—an X-ray absorption study: I, trivalent dopants. J. Am. Ceram. Soc. 77, 118–128 (1994). https://doi.org/10.1111/j.1151-2916.1994.tb06964.x10.1111/j.1151-2916.1994.tb06964.x ↗
26. Li, P., Chen, I.W., Penner-Hahn, J.E.: Effect of dopants on zirconia stabilization—an X-ray absorption study: II, tetravalent dopants. J. Am. Ceram. Soc. 77, 1281–1288 (1994). https://doi.org/10.1111/j.1151-2916.1994.tb05403.x10.1111/j.1151-2916.1994.tb05403.x ↗
27. Kohorst, P., Borchers, L., Strempel, J., Stiesch, M., Hessel, T., Bach, F.-W., Hubsch, C.: Low-temperature degradation of different zirconia ceramics for dental applications. Acta Biomater. 8, 1213–1220 (2012). https://doi.org/10.1016/j.actbio.2011.11.01610.1016/j.actbio.2011.11.016 ↗
28. Sulaiman, T.A., Abdulmajeed, A.A., Donovan, T.E., Vallittu, P.K., Narhi, T.O., Lassila, L.V.: The effect of staining and vacuum sintering on optical and mechanical properties of partially and fully stabilized monolithic zirconia. Dent. Mater. J. 34, 605–610 (2015). https://doi.org/10.4012/dmj.2015-05410.4012/dmj.2015-054 ↗
29. Gautam, C., Joyner, J., Gautam, A., Rao, J., Vajtai, R.: Zirconia based dental ceramics: structure, mechanical properties, biocompatibility and applications. Dalton Trans. 45, 19194–19215 (2016). https://doi.org/10.1039/C6DT03484E10.1039/C6DT03484E ↗
30. de Bernardi-Martin, S., Moshtaghioun, B.M., Gomez Garcia, D., Dominguez-Rodrigues, A.: Grain-boundary cation diffusion in ceria tetragonal zirconia determined by constant-strain-rate deformation tests. J. Eur. Ceram. Soc. 34, 4469–4472 (2014). https://doi.org/10.1016/j.jeurceramsoc.2014.06.02410.1016/j.jeurceramsoc.2014.06.024 ↗
31. Lughi, V., Sergo, V.: Low temperature degradation – aging – of zirconia: a critical review of the relevant aspects in dentistry. Dent. Mater. 26, 807–820 (2010). https://doi.org/10.1016/j.dental.2010.04.00610.1016/j.dental.2010.04.006 ↗
32. Dynacer.com. Data sheets Zirconia. http://www.dynacer.com/wp-content/themes/devvine/PDF/Material%20Properties%20datasheet.pdf (2018). Accessed 11 September 2018
33. Azom.com. Zirconia - physical and mechanical property comparison of the different types of zirconias. https://www.azom.com/article.aspx?ArticleID=940 (2018). Accessed 11 September 2018
34. Tsukuma, K., Shimada, M.: Strength, fracture toughness and Vickers hardness of CeO2-stabilized tetragonal ZrO2 polycrystals (Ce-TZP). J. Mater. Sci. 20, 1178–1184 (1985). https://doi.org/10.1007/BF0102631110.1007/BF01026311 ↗
35. Cousland, G.P., Cui, X.Y., Smith, A.E., Stampfl, A.P.J., Stampfl, C.M.: Mechanical properties of zirconia, doped and undoped yttria-stabilized cubic zirconia from first-principles. J. Phys. Chem. Solids. 122, 51–71 (2018). https://doi.org/10.1016/j.jpcs.2018.06.00310.1016/j.jpcs.2018.06.003 ↗
36. Eichler, J., Eisele, U., Rodel, J.: Mechanical properties of monoclinic zirconia. J. Am. Ceram. Soc. 87, 1401–1403 (2004). https://doi.org/10.1111/j.1151-2916.2004.tb07748.x10.1111/j.1151-2916.2004.tb07748.x ↗
37. Kuo, C.-W., Shen, Y.-H., Yen, F.-L., Cheng, H.-Z., Hung, I.-M., Wen, S.-B., Wang, M.-C., Stack, M.: Phase transformation behavior of 3 mol% yttria partially-stabilized ZrO2 (3Y–PSZ) precursor powder by an isothermal method. Ceram. Int. 40, 3243–3251 (2014). https://doi.org/10.1016/j.ceramint.2013.09.11210.1016/j.ceramint.2013.09.112 ↗
38. Li, P., Chen, I.W., Penner-Hahn, J.E.: Effect of dopants on zirconia stabilization—an X-ray absorption study: III, charge-compensating dopants. J. Am. Ceram. Soc. 77, 1289–1295 (1994). https://doi.org/10.1111/j.1151-2916.1994.tb05404.x10.1111/j.1151-2916.1994.tb05404.x ↗
39. Schnohr, C.S., Ridgway, M.C.: Chapter 1, introduction to X-ray absorption spectroscopy. In: Schnohr, C.S., Ridgway, M.C. (eds.) X-Ray absorption spectroscopy of semiconductors, Springer Series in Optical Sciences 190, pp. 1–26. Springer, Cham (2015). DOI https://doi.org/10.1007/978-3-662-44362-0_110.1007/978-3-662-44362-0_1 ↗
40. Escribano, V.S., Lopez, E.F., Panizza, M., Resini, C., Gallardo Amores, J.M., Busca, G.: Characterization of cubic ceria–zirconia powders by X-ray diffraction and vibrational and electronic spectroscopy. Solid State Sci. 5, 1369–1376 (2003). https://doi.org/10.1016/j.solidstatesciences.2003.07.00110.1016/j.solidstatesciences.2003.07.001 ↗
41. Varez, A., Garcia-Gonzalez, E., Sanz, J.: Cation miscibility in CeO2–ZrO2 oxides with fluorite structure. A combined TEM, SAED and XRD Rietveld analysis. J. Mater. Chem. 16, 4249–4256 (2006). https://doi.org/10.1039/B607778A10.1039/B607778A ↗
42. Chevalier, J., Gremillard, L.: Ceramics for medical applications: a picture for the next 20 years. J. Eur. Ceram. Soc. 29, 1245–1255 (2009). https://doi.org/10.1016/j.jeurceramsoc.2008.08.02510.1016/j.jeurceramsoc.2008.08.025 ↗
43. Becher, P.F., Swain, M.V.: Grain-size-dependent transformation behavior in polycrystalline tetragonal zirconia. J. Am. Ceram. Soc. 75, 493–502 (1992). https://doi.org/10.1111/j.1151-2916.1992.tb07832.x10.1111/j.1151-2916.1992.tb07832.x ↗
44. Simba, B.G., dos Santos, C., Strecker, K., de Almeida Junior, A.A., Adabo, C.L.: Recovery of tetragonal phase from previously transformed Y-TZP. Mater. Res. 19, 829–833 (2016). https://doi.org/10.1590/1980-5373-MR-2015-042610.1590/1980-5373-MR-2015-0426 ↗
45. Lange, F.F.: Transformation toughening. Part 1 size effects associated with the thermodynamics of constrained transformations. J. Mater. Sci. 17, 225–234 (1982). https://doi.org/10.1007/BF0080905710.1007/BF00809057 ↗
46. De Aza, A.H., Chevalier, J., Fantozzi, G., Schehl, M., Torrecillas, R.: Slow-crack-growth behavior of zirconia-toughened alumina ceramics processed by different methods. J. Am. Ceram. Soc. 86, 115–120 (2003). https://doi.org/10.1111/j.1151-2916.2003.tb03287.x10.1111/j.1151-2916.2003.tb03287.x ↗
47. Tsukuma, K., Takahata, T.: Mechanical properties and microstructure of TZP and TZP/Al2O3 composites. Mater. Res. Soc. Symp. Proc. 78, 123–135 (1986). https://doi.org/10.1557/PROC-78-12310.1557/PROC-78-123 ↗
48. Bannister, M.: Science and Technology of Zirconia V. CRC Press, Boca Raton (1993) ISBN: 9781566760737
49. Yu, C.S., Shetty, D.K.: Transformation zone shape, size, and crack-growth-resistance [R-curve] behavior of ceria-partially-stabilized zirconia polycrystals. J. Am. Ceram. Soc. 72, 921–928 (1989). https://doi.org/10.1111/j.1151-2916.1989.tb06245.x10.1111/j.1151-2916.1989.tb06245.x ↗
50. Swain, M.V., Rose, L.R.F.: Strength limitations of transformation-toughened zirconia alloys. J. Am. Ceram. Soc. 69, 511–518 (1986). https://doi.org/10.1111/j.1151-2916.1986.tb04785.x10.1111/j.1151-2916.1986.tb04785.x ↗
51. Studart, A.R., Filser, F., Kocher, P., Gauckler, L.J.: Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridges. Dent. Mater. 23, 106–114 (2007). https://doi.org/10.1016/j.dental.2005.12.00810.1016/j.dental.2005.12.008 ↗
52. Li, L.-S., Pabst, R.F.: Subcritical crack growth in partially stabilized zirconia (PSZ). J. Mater. Sci. 15, 2861–2866 (1980). https://doi.org/10.1007/BF0055055510.1007/BF00550555 ↗
53. Szutkowska, M., Boniecki, M.: Subcritical crack growth in zirconia-toughened alumina (ZTA) ceramics. J. Mater. Process. Technol. 175, 416–420 (2006). https://doi.org/10.1016/j.jmatprotec.2005.04.03010.1016/j.jmatprotec.2005.04.030 ↗
54. Schmitt, R., Fett, T., Munz, D.: Cyclic fatigue of zirconia. Fatigue Fract. Eng. Mater. Struct. 19, 1411–1420 (1996). https://doi.org/10.1111/j.1460-2695.1996.tb00177.x10.1111/j.1460-2695.1996.tb00177.x ↗
55. Zmak, I., Coric, D., Mandic, V., Cirkovic, L.: Hardness and indentation fracture toughening of slip cast alumina and alumina-zirconia ceramics. Materials. 13, 122 (2020). https://doi.org/10.3390/ma1301012210.3390/ma13010122 ↗
56. Marshall, D.B., Evans, A.G., Drory, M.: Transformation toughening in ceramics. In: Bradt, R.C., Evans, A.G., Hasselman, D.P.H., Lange, F.F. (eds.) Fracture Mechanics of Ceramics, vol. 6, pp. 289–307. Plenum Press, New York (1983) ISBN: 0306410222
57. Bocanegra-Bernal, M.H., Garcia-Reyes, A., Dominguez-Rios, C., Reyes-Rojas, A., Aguilar-Elguezabal, A., Echeberria, J.: Towards improving low-temperature degradation of zirconia/alumina ceramics via in situ formation of an Al2O3 functional surface layer through sintering in the presence of graphite powder. J. Alloys Compd. 818, 152840 (2020). https://doi.org/10.1016/j.jallcom.2019.15284010.1016/j.jallcom.2019.152840 ↗
58. AllThingsBiomaterials.org. The Prozyr Femoral Ball Re-call. http://allthingsbiomaterials.org/archives/170 (2020). Accessed 19 January 2020
59. Lawson, S.: Environmental degradation of zirconia ceramics. J. Eur. Ceram. Soc. 15, 485–502 (1995). https://doi.org/10.1016/0955-2219(95)00035-S10.1016/0955-2219(95)00035-S ↗
60. Sergo, V., Pompe, W., Clarke, D.R.: Deformation bands in ceria-stabilized tetragonal zirconia/alumina: I. Measurement of internal stresses. J. Am. Ceram. Soc. 78, 633–640 (1995). https://doi.org/10.1111/j.1151-2916.1995.tb08224.x10.1111/j.1151-2916.1995.tb08224.x ↗
61. Lange, F.F., Dunlpo, G.L., Davis, B.I.: Degradation during ageing of transformation toughened ZrO2-Y2O3 materials at 250 °C. J. Am. Ceram. Soc. 69, 237–240 (1986). https://doi.org/10.1111/j.1151-2916.1986.tb07415.x10.1111/j.1151-2916.1986.tb07415.x ↗
62. Yoshimura, M., Noma, T., Kawabata, K., Somiya, S.: Role of H2O on the degradation process of Y-TZP. J. Mater. Sci. Lett. 6, 465–467 (1987). https://doi.org/10.1007/BF0175680010.1007/BF01756800 ↗
63. Deville, S., Chevalier, J., Dauvergne, C., Fantozzi, G., Bartolomé, J.F., Moya, J.S., Torrecillas, R.: Microstructural investigation of the aging behavior of (3Y-TZP)-Al2O3 composites. J. Am. Ceram. Soc. 88, 1273–1280 (2005). https://doi.org/10.1111/j.1551-2916.2005.00221.x10.1111/j.1551-2916.2005.00221.x ↗
64. Lee, J.K., Kim, H.: Surface crack initiation in 2Y-TZP ceramics by low temperature aging. Ceram. Int. 20, 413–418 (1994). https://doi.org/10.1016/0272-8842(94)90028-010.1016/0272-8842(94)90028-0 ↗
65. Patil, N.A., Kandasubramanian, B.: Biological and mechanical enhancement of zirconium dioxide for medical applications. Ceram. Int. 46, 4041–4057 (2020). https://doi.org/10.1016/j.ceramint.2019.10.22010.1016/j.ceramint.2019.10.220 ↗
66. Kelly, P.M., Rose, L.R.F.: The martensitic transformation in ceramics – its role in transformation toughening. Prog. Mater. Sci. 47, 463–557 (2002). https://doi.org/10.1016/S0079-6425(00)00005-010.1016/S0079-6425(00)00005-0 ↗
67. Varghese, G., Moral, M., Castro-Garcia, M., Lopez-Lopez, J.J., Marin-Rueda, J.R., Yague-Alcaraz, V., Hernandez-Afonso, L., Ruiz-Morales, J.C., Canales-Vazquez, J.: Fabrication and characterization of ceramics via low-cost DLP 3D printing. Bol. Soc. Esp. Cerám. Vidrio. 57, 9–18 (2018). https://doi.org/10.1016/j.bsecv.2017.09.00410.1016/j.bsecv.2017.09.004 ↗
68. Zhu, W., Nakashima, S., Matsuura, M., Gu, H., Marin, E., Pezzotti, G.: Raman and X-ray photoelectron spectroscopic characterizations of thermal stability of 3mol% yttria stabilized zirconia ceramics. J. Eur. Ceram. Soc. 39, 4928–4935 (2019). https://doi.org/10.1016/j.jeurceramsoc.2019.06.05610.1016/j.jeurceramsoc.2019.06.056 ↗
69. Schunemann, F.H., Galarraga-Vinueza, M.E., Magini, R., Fredel, M., Silva, F., Souza, J.C.M., Zhang, Y., Herniques, B.: Zirconia surface modifications for implants dentistry. Mater. Sci. Eng. C. 98, 1294–1305 (2019). https://doi.org/10.1016/j.msec.2019.01.06210.1016/j.msec.2019.01.062 ↗
70. Berni, M., Lopomo, N., Marchiori, G., Gambardella, A., Boi, M., Bianchi, M., Visani, A., Pavan, P., Russo, A., Marcacci, M.: Tribological characterization of zirconia coatings deposited on Ti6Al4V components for orthopedic applications. Mater. Sci. Eng. C. 62, 643–655 (2016). https://doi.org/10.1016/j.msec.2016.02.01410.1016/j.msec.2016.02.014 ↗
71. Moos, R.: A brief overview on automotive exhaust gas sensors based on electroceramics. Int. J. Appl. Ceram. Technol. 2, 401–413 (2005). https://doi.org/10.1111/j.1744-7402.2005.02041.x10.1111/j.1744-7402.2005.02041.x ↗