MgO activated calcined marine clay and its carbonation
Source abstract
Abstract
Marine clay, a common waste product abundantly available in coastal regions, can serve as an alternative silica source after activation due to its pozzolanic reactivity. In this study, a binder comprising reactive MgO cement and thermally activated marine clay (AMC) was developed. It was found that the developed MgO-AMC binder with a mass ratio of MgO to AMC of 0.4 to 0.6 achieved a 28-day compressive strength of 20.4 MPa under ambient curing. Through accelerated carbonation curing, the highest 28-day compressive strength increased by 45%, and the highest carbon sequestration ratio reached 11.8%. The phase evolution and microstructural development of hydrated/carbonated binder were comprehensively investigated by TG-IR, XRD, NMR, and SEM-EDS. In addition, thermodynamic modelling was performed to further understand the phase assemblage of the hydrated binder, and indicated that M-A-S-H phase was thermodynamically more stable in the developed binder.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Calcium Carbonate Crystallization and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Civil and Environmental Engineering, Nanyang Technological University, Singapore
References (64)
Show source-provided references
1. 10.1038/s41561-022-00918-110.1038/s41561-022-00918-1 ↗
2. 10.3334/CDIAC/atg.01110.3334/CDIAC/atg.011 ↗
3. 10.1016/j.jece.2018.07.03310.1016/j.jece.2018.07.033 ↗
4. 10.1016/j.conbuildmat.2022.12961010.1016/j.conbuildmat.2022.129610 ↗
5. Unluer C. Carbon dioxide sequestration in magnesium-based binders, carbon dioxide sequestration in cementitious construction materials. Woodhead Publishing; 2018.
6. Al-Tabbaa A. Reactive magnesia cement, eco-efficient concrete. Woodhead Publishing; 2013.
7. 10.1016/j.jclepro.2016.07.07110.1016/j.jclepro.2016.07.071 ↗
8. 10.1016/j.conbuildmat.2017.03.03810.1016/j.conbuildmat.2017.03.038 ↗
9. 10.1016/j.cemconres.2019.10594110.1016/j.cemconres.2019.105941 ↗
10. 10.1016/j.desal.2017.12.02110.1016/j.desal.2017.12.021 ↗
11. 10.1038/s43247-021-00099-610.1038/s43247-021-00099-6 ↗
12. 10.1016/j.conbuildmat.2022.12772510.1016/j.conbuildmat.2022.127725 ↗
13. 10.1016/j.cemconcomp.2021.10406810.1016/j.cemconcomp.2021.104068 ↗
14. 10.1016/j.heliyon.2023.e1571810.1016/j.heliyon.2023.e15718 ↗
15. 10.1016/j.clay.2015.01.02810.1016/j.clay.2015.01.028 ↗
16. 10.1016/j.cemconres.2010.09.01310.1016/j.cemconres.2010.09.013 ↗
17. 10.1016/j.cemconres.2023.10741710.1016/j.cemconres.2023.107417 ↗
18. 10.1016/j.cemconres.2020.10605010.1016/j.cemconres.2020.106050 ↗
19. 10.1016/j.cemconres.2024.10746210.1016/j.cemconres.2024.107462 ↗
20. 10.1016/j.cemconres.2011.01.01610.1016/j.cemconres.2011.01.016 ↗
21. 10.1016/j.cemconres.2014.07.00110.1016/j.cemconres.2014.07.001 ↗
22. 10.1016/j.cemconcomp.2023.10498310.1016/j.cemconcomp.2023.104983 ↗
23. Shah V, Scott A. Assessment of hardened concrete properties of MgO-SiO2 binder systems. ACI Mater J. 2021;118(2).
24. 10.1016/j.conbuildmat.2021.12273610.1016/j.conbuildmat.2021.122736 ↗
25. 10.1111/jace.1797110.1111/jace.17971 ↗
26. 10.1617/s11527-022-01901-310.1617/s11527-022-01901-3 ↗
27. 10.1016/j.cemconres.2021.10642210.1016/j.cemconres.2021.106422 ↗
28. 10.1016/j.jclepro.2018.07.06810.1016/j.jclepro.2018.07.068 ↗
29. 10.1016/j.cemconcomp.2020.10382610.1016/j.cemconcomp.2020.103826 ↗
30. 10.1016/j.conbuildmat.2024.13583910.1016/j.conbuildmat.2024.135839 ↗
31. 10.1617/s11527-021-01807-610.1617/s11527-021-01807-6 ↗
32. 10.1016/j.clay.2007.03.00310.1016/j.clay.2007.03.003 ↗
33. 10.1016/j.cemconcomp.2023.10505710.1016/j.cemconcomp.2023.105057 ↗
34. ASTM C109/C109M-20. Standard test method for compressive strength of hydraulic cement mortars. Philadelphia (PA): American Society for Testing and Materials; 2020.
35. ASTM Standard C25. Standard test methods for chemical analysis of limestone, quicklime and hydrated lime. West Conshohocken (PA): ASTM international; 2019.
36. 10.1016/j.cemconcomp.2020.10381910.1016/j.cemconcomp.2020.103819 ↗
37. ASTM C1702. Standard test method for measurement of heat of hydration of hydraulic cementitious materials using isothermal conduction calorimetry. West Conshohocken (PA); 2017.
38. 10.1016/j.cemconres.2021.10639110.1016/j.cemconres.2021.106391 ↗
39. 10.1016/j.matlet.2017.01.07210.1016/j.matlet.2017.01.072 ↗
40. 10.1016/j.conbuildmat.2020.12174810.1016/j.conbuildmat.2020.121748 ↗
41. 10.1016/j.cemconres.2017.08.00310.1016/j.cemconres.2017.08.003 ↗
42. 10.1680/jadcr.21.0003410.1680/jadcr.21.00034 ↗
43. 10.1016/j.cemconres.2020.10615610.1016/j.cemconres.2020.106156 ↗
44. 10.1016/j.ceramint.2017.04.05810.1016/j.ceramint.2017.04.058 ↗
45. 10.3390/ma1106090910.3390/ma11060909 ↗
46. 10.1016/j.tca.2010.06.01210.1016/j.tca.2010.06.012 ↗
47. 10.1007/s10973-015-4756-010.1007/s10973-015-4756-0 ↗
48. 10.1016/j.conbuildmat.2019.11727510.1016/j.conbuildmat.2019.117275 ↗
49. 10.1016/j.conbuildmat.2021.12357310.1016/j.conbuildmat.2021.123573 ↗
50. 10.1155/2020/618906110.1155/2020/6189061 ↗
51. 10.1617/s11527-016-0810-z10.1617/s11527-016-0810-z ↗
52. 10.1016/j.cemconres.2015.08.00610.1016/j.cemconres.2015.08.006 ↗
53. 10.1016/j.clay.2014.07.01110.1016/j.clay.2014.07.011 ↗
54. 10.1016/j.cemconres.2015.10.00310.1016/j.cemconres.2015.10.003 ↗
55. 10.1016/j.cemconres.2019.10593110.1016/j.cemconres.2019.105931 ↗
56. 10.1039/c5dt00877h10.1039/c5dt00877h ↗
57. 10.1016/j.micromeso.2007.05.03810.1016/j.micromeso.2007.05.038 ↗
58. 10.1016/j.matdes.2020.10939110.1016/j.matdes.2020.109391 ↗
59. 10.1016/j.conbuildmat.2017.02.15810.1016/j.conbuildmat.2017.02.158 ↗
60. 10.1007/s10596-012-9310-610.1007/s10596-012-9310-6 ↗
61. Thoenen T Hummel W Berner U et al. The PSI/nagra chemical thermodynamic database. 2014;12(07).
62. 10.1016/j.cemconres.2018.04.01810.1016/j.cemconres.2018.04.018 ↗
63. 10.2136/sssaj1974.03615995003800030015x10.2136/sssaj1974.03615995003800030015x ↗
64. 10.1016/j.cemconres.2012.09.00210.1016/j.cemconres.2012.09.002 ↗