Abstract

Compact and uniform NiW composite coatings filled with ceramic particles such as CeO2 were electrodeposited on brass substrates using direct current (DC) and a well–designed pulse reverse current waveforms (PRC). PRC coatings exhibited the noblest corrosion potential and lowest current density compared to DC–electrodeposited coatings. Among all PRC coatings, PRC–NiW–CeO2 demonstrated the highest corrosion potential (−4.72 × 10−1 V) and the lowest current density (5.32 × 10−6 V). It also seems that the addition of CeO2 particles to the NiW matrix enhanced the wear resistance of the coatings, and the lowest wear volume of (133.10 × 103 µm3) and friction coefficient of 0.25 were obtained due to the formation of the uniform, void free and compact structures with a high content of CeO2 particles in the coating.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Semiconductor materials and interfaces · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Laboratory of New Materials for Energy and Electrochemistry, Polytechnique Montréal, 2500 Chemin de Polytechnique, Montreal, QC H3T 1J4, Canada

Funding

Laboratory of New Materials for Electrochemistry and Energy (LANOMAT), Montreal.

References (44)

Show source-provided references
1. Effect of Current Density on the Properties of Ni–CeO2 Composite Coatings prepared using Magnetic Field–Assisted Jet Electrodeposition10.20964/2021.06.13 ↗
2. A polymeric composite protective layer for stable Li metal anodes10.1186/s40580-020-00231-w ↗
3. In situ prepared nano–crystalline TiO2–poly(methyl methacrylate) hybrid enhanced composite polymer electrolyte for Li–ion batteries10.1039/c3ta00086a ↗
4. Preparation and electrocatalytic property of PbO2–CeO2 nanocomposite electrodes by pulse reverse electrodeposition methods10.1149/2.0091606jes ↗
5. Preparation of Ni–ZrO2–CeO2 Nanocomposite Coatings by Pulse Electrodeposition10.4028/www.scientific.net/AMM.395-396.174 ↗
6. Improved wear properties of Ni Ti nanocomposite coating with tailored spatial microstructures by extra adding CeO2 nanoparticles10.1016/j.surfcoat.2020.126119 ↗
7. Electrocatalytic Activity of Pd–CeO2 Nanobundle in an Alkaline Ethanol Oxidation10.1007/s10562-010-0378-0 ↗
8. A comparative study of pure nickel and the Ni–CeO2 nanocrystalline coatings: Microstructural evolution, oxidation behavior, and thermodynamic stability10.1007/s10853-014-8087-5 ↗
9. Tribological performance of Ni–CeO2 composite coatings by electrodeposition10.1016/j.surfcoat.2005.08.002 ↗
10. Formation of bilayer Ni–SiC composite coatings by electrodeposition10.1016/S0257-8972(98)00589-1 ↗
11. Electrodeposition and sliding wear resistance of nickel composite coatings containing micron and submicron SiC particles10.1016/S0257-8972(01)01336-6 ↗
12. XPS, UPS and ESR studies on the interfacial interaction in Ni–ZrO2 composite plating10.1023/A:1004741215543 ↗
13. Characterization of single and discretely–stepped electro–composite coatings of nickel–alumina10.1023/A:1004633923681 ↗
14. Electrodeposited Co–Ni–Al2O3 composite coatings10.1016/S0257-8972(03)00739-4 ↗
15. Effect of MoO2 and TiO2 on electrodeposition and properties of chromium coating10.1016/S0257-8972(00)01065-3 ↗
16. Composite layers in Ni–P system containing TiO2 and PTFE10.1016/S0040-6090(99)00175-3 ↗
17. The effect of second phase volume fraction on the erosion resistance of metal–matrix composites10.1016/S0043-1648(99)00363-4 ↗
18. The microstructure and wear resistance characteristics of electroformed nickel and partially stabilized zirconia composite coatings10.1023/A:1004780619429 ↗
19. The wear behaviour of electro–codeposited Ni–SiC composites10.1016/S0043-1648(02)00222-3 ↗
20. A novel plating apparatus for electrodeposition of Ni–SiC composite coatings using circulating–solution co–deposition technique10.1016/j.jallcom.2016.12.331 ↗
21. Tribological and anti–corrosion properties of Ni–W–CeO2 coatings against molten glass. Surface and Coatings Technology10.1016/j.surfcoat.2007.11.031 ↗
22. Effect of rare earth compounds as fillers on friction and wear behaviors of PTFE–based composites10.1002/(SICI)1097-4628(19990418)72:3<361::AID-APP6>3.0.CO;2-5 ↗
23. Wear and tribological characterization of nickel matrix electrodeposited composites: A review10.1016/j.wear.2021.204098 ↗
24. Codeposition of Cerium Oxide with Nickel and Cobalt: Correlation between Microstructure and Microhardness10.1179/026708404X1134 ↗
25. XRD characterisation of composite Ni–based coatings prepared by electrodeposition10.1016/j.nimb.2011.07.108 ↗
26. Properties of nickel–tungsten alloys electrodeposited from sulfamate electrolyte
27. Effect of tungsten on microstructures of annealed electrodeposited Ni–W alloy and its corrosion resistance10.1016/j.surfcoat.2018.01.070 ↗
28. Electroplating of Ni/W alloys: I. Ammoniacal citrate baths10.1149/1.1433750 ↗
29. Structural investigations on nanocrystalline Ni–W alloy films by transmission electron microscopy10.1016/j.tsf.2009.04.039 ↗
30. Synthesis and evaluation of hardness and sliding wear resistance of electrodeposited nanocrystalline Ni–W alloys10.1016/j.msea.2005.11.046 ↗
31. Improving the Corrosion Resistance of the Nickel–Tungsten Alloy by Optimization of the Electroplating Conditions10.1007/s12666-020-01894-z ↗
32. Pulsed electrodeposition and mechanical properties of Ni–W/SiC nano–composite coatings10.1016/j.matdes.2016.09.070 ↗
33. Effect of Saccharin on the Structure and Properties of Electrodeposition NiWP Alloy Coatings10.1007/s11665-016-2298-7 ↗
34. Cameron, J.C. (1983). Acetylenic Compositions and Nickel Plating Baths Containing Same. (No. 4,421,6111983), U.S. Patent.
35. Experimental investigation of grain boundaries misorientations and nano twinning induced strengthening on addition of silicon carbide in pulse electrodeposited nickel tungsten composite coating10.1016/j.matchar.2016.04.002 ↗
36. Shi, Y.Z., Yang, B., and Liaw, P.K. (2017). Corrosion–Resistant High–Entropy Alloys: A Review. Metals, 7.10.3390/met7020043 ↗
37. Feng, L., Ren, Y.-Y., Zhang, Y.-H., Wang, S., and Li, L. (2019). Direct Correlations among the Grain Size, Texture, and Indentation Behavior of Nanocrystalline Nickel Coatings. Metals, 9.10.3390/met9020188 ↗
38. In Situ Characterization of Pitting Corrosion of Stainless Steel by a Scanning Electrochemical Microscopy10.1007/s11665-011-9899-y ↗
39. Diffusion and segregation of substrate copper in electrodeposited Ni–Fe thin films10.1016/j.jallcom.2006.10.048 ↗
40. Influence of grain size on the corrosion behavior of a Ni–based superalloy nanocrystalline coating in NaCl acidic solution10.1016/j.electacta.2007.10.048 ↗
41. Palumbo, G., Dunikowski, D., Wirecka, R., Mazur, T., Lelek-Borkowska, U., Wawer, K., and Banaś, J. (2021). Effect of Grain Size on the Corrosion Behavior of Fe–3wt.%Si–1wt.%Al Electrical Steels in Pure Water Saturated with CO2. Materials, 14.10.3390/ma14175084 ↗
42. The influence of grain size on the corrosion resistance of nanocrystalline zirconium metal10.1016/j.msea.2006.10.029 ↗
43. Nyambura, S.M., Kang, M., Zhu, J., Liu, Y., Zhang, Y., and Ndiithi, N.J. (2019). Synthesis and Characterization of Ni–W/Cr2O3 Nanocomposite Coatings Using Electrochemical Deposition Technique. Coatings, 9.10.3390/coatings9120815 ↗
44. Corrosion behaviour of electrodeposited nanocrystalline Ni–W and Ni–Fe–W alloys10.1016/j.msea.2007.02.055 ↗