Investigations in Anti-Impact Performance of TiN Coatings Prepared by Filtered Cathodic Vacuum Arc Method under Different Substrate Temperatures

Da Huang, Weifeng He, Xin Cao, Yang Jiao

Coatings· Volume 10· Issue 9

Abstract

In this study, the anti-impact performance of the TiN coatings prepared under various substrate temperatures (35, 200, 400, and 600 °C) were evaluated using a cyclic impact tester under 104 cycles. Moreover, the microstructure and anti-impact performance-related mechanical properties (adhesion strength and nano-hardness) were investigated to reveal the underlying mechanism of how the substrate temperature affects the anti-impact performance of the coatings. The results showed that the substrate temperature has a great influence on the internal stress, nano-hardness, and adhesion strength as well as the anti-impact performance of TiN coatings, and the coatings prepared under 400 °C exhibit the best impact resistance. The small internal stress, strong adhesion strength as well as high hardness and H3/E2 value for the 400 °C prepared coatings are the main contributes.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Surface Treatment and Residual Stress

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Science and Technology on Plasma Dynamics Laboratory, Air Force Engineering University, Xi’an 710038, China

Cardiff School of Engineering, Cardiff University, Cardiff CF24 3AA, UK

Funding

National Major Science and Technology Projects of China

References (56)

Show source-provided references
1. Effect of cryogenic and aging treatments on low-energy impact behaviour of Ti–6Al–4V alloy10.1016/S1003-6326(17)60058-X ↗
2. Stress relaxation induced morphological evolution and texture weakening of α phase in Ti-6Al-4V alloy10.1016/j.matlet.2018.10.113 ↗
3. Erosive wear behavior of Ti/Ti(V,Zr)N multilayered PVD coatings for Ti-6Al-4V alloy10.1016/j.wear.2018.11.016 ↗
4. Evaluating the erosion resistance of Ti6Al4V coatings deposited by cold spray10.1016/j.wear.2020.203337 ↗
5. Nanolayered multilayer Ti/TiN coatings: Role of bi-layer thickness and annealing on solid particle erosion behaviour at elevated temperature10.1016/j.surfcoat.2018.10.007 ↗
6. Nanolayered CrAlTiN and multilayered CrAlTiN–AlTiN coatings for solid particle erosion protection10.1016/j.triboint.2014.11.002 ↗
7. Erosion wear of CrN, TiN, CrAlN, and TiAlN PVD nitride coatings10.1016/j.ijrmhm.2012.03.002 ↗
8. Performance and damage mechanism of TiN/ZrN nano-multilayer coatings based on different erosion angles10.1016/j.apsusc.2020.145457 ↗
9. Structural, mechanical, and sand erosion properties of TiN/Zr/ZrN multilayer coatings10.1016/j.vacuum.2015.09.026 ↗
10. Superior oxidation resistance, mechanical properties and residual stresses of an Al-rich nanolamellar Ti0.05Al0.95N coating prepared by CVD10.1016/j.surfcoat.2014.07.022 ↗
11. Ultra-thin multilayered erosion resistant Ti/TiN coatings with stress absorbing layers10.1016/j.apsusc.2019.02.012 ↗
12. The influence of ductile interlayer material on the particle erosion resistance of multilayered TiN based coatings10.1016/j.wear.2011.06.004 ↗
13. Ti–N multilayer systems for compressor airfoil sand erosion protection10.1016/j.surfcoat.2009.09.053 ↗
14. Erosion performance and characterization of nanolayer (Ti,Cr)N hard coatings for gas turbine engine compressor blade applications10.1016/j.surfcoat.2011.07.063 ↗
15. Structure and properties of TiN coatings10.1016/0040-6090(85)90333-5 ↗
16. Substrate-temperature dependent structure and composition variations in RF magnetron sputtered titanium nitride thin films10.1016/j.apsusc.2010.10.118 ↗
17. Corrosion resistance and mechanism of CeN, TiN and CeN/TiN bilayer composite film deposited by dual ion beam sputtering10.1016/j.surfcoat.2017.12.033 ↗
18. Microstructures and properties of titanium nitride films prepared by pulsed laser deposition at different substrate temperatures10.1016/j.apsusc.2015.09.061 ↗
19. Effect of substrate roughness on adhesion and tribological properties of nc-TiAlN/a-Si3N4 nanocomposite coatings deposited by cathodic arc PVD process10.1179/1743294415Y.0000000005 ↗
20. Improvement of structure and quality of nanoscale multilayered composite coatings, deposited by filtered cathodic vacuum arc deposition method10.1177/1847980416680805 ↗
21. Shulepov, I., Kashkarov, E., Stepanov, I., Syrtanov, M., Alina, S., Shanenkov, I., Obrosov, A., and Weiss, S. (2017). The formation of composite Ti-Al-N coatings using filtered vacuum arc deposition with separate cathodes. Metals, 7.10.3390/met7110497 ↗
22. Sand particle erosion resistance of the multilayer gradient TiN/Ti coatings on Ti6Al4V alloy10.1016/j.surfcoat.2018.08.066 ↗
23. Cao, X., Xu, W., and He, W. (2020). A method for evaluating the impact wear behavior of multilayer TiN/Ti coating. Coatings, 10.10.3390/coatings10020132 ↗
24. Damage evolution and mechanism of TiN/Ti multilayer coatings in sand erosion condition10.1016/j.surfcoat.2018.08.062 ↗
25. The anti-sand erosion performance of TiN films fabricated by filtered cathodic vacuum arc technique at different nitrogen flow rates10.1016/j.ceramint.2019.02.157 ↗
26. Mechanical modification and damage mechanism evolution of TiN films subjected to cyclic nano-impact by adjusting N/Ti ratios10.1016/j.jallcom.2019.151816 ↗
27. Micro-nano multilayer structure design and solid particle erosion resistance performance of CrAlNx/CrAlN coating10.1016/j.vacuum.2019.109064 ↗
28. Study on the abrasive wear behavior of laser shock peening Ti-6Al-4V titanium alloy under controlled cycling impact10.1016/j.wear.2019.01.112 ↗
29. Fracture toughness and structural evolution in the TiAlN system upon annealing10.1038/s41598-017-16751-1 ↗
30. Influence of substrate temperature on the materials properties of reactive DC magnetron sputtered Ti/TiN multilayered thin films10.1016/j.mseb.2010.08.004 ↗
31. Effect of substrate temperature and annealing on structure, stress and properties of reactively co-sputtered Ni-TiN nanocomposite thin films10.1016/j.tsf.2017.01.024 ↗
32. Zhang, Z., Chen, J., He, G., and Yang, G. (2019). Fatigue and mechanical behavior of Ti-6Al-4V alloy with CrN and TiN coating deposited by magnetic filtered cathodic vacuum arc process. Coatings, 9.10.3390/coatings9100689 ↗
33. Sand erosion resistance improvement and damage mechanism of TiAlN coating via the bias-graded voltage in FCVA deposition10.1016/j.surfcoat.2019.125009 ↗
34. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
35. Preparation and impact resistance performance of bionic sandwich structure inspired from beetle forewing10.1016/j.compositesb.2018.12.139 ↗
36. Low velocity impact wear behavior of MoS2/Pb nanocomposite coating under controlled kinetic energy10.1016/j.surfcoat.2017.07.029 ↗
37. Improving impact wear resistance of Ti-6Al-4V alloy treated by laser shock peening10.1016/S1003-6326(19)65051-X ↗
38. Impact wear behavior of WC/a-C nanomultilayers10.1088/2053-1591/ab4d29 ↗
39. Investigation into the impact wear behaviour of ceramic coatings10.1016/0257-8972(95)08314-6 ↗
40. Micro-impact testing of AlTiN and TiAlCrN coatings10.1016/j.wear.2018.11.010 ↗
41. Effect of interlayer design on the mechanical properties of AlTiCrN and multilayered AlTiCrN/TiSiN hard coatings10.1016/j.surfcoat.2020.125637 ↗
42. Load sensitivity in repetitive nano-impact testing of TiN and AlTiN coatings10.1016/j.surfcoat.2016.05.094 ↗
43. Film thickness effect on texture and residual stress sign transition in sputtered TiN thin films10.1016/j.ceramint.2017.06.050 ↗
44. Influence of deposition temperature on the structure and internal stress of TiN films deposited by filtered cathodic vacuum arc10.1116/1.1481043 ↗
45. Determination of residual stresses in cathodic arc coatings by means of the parallel beam glancing X-ray diffraction technique10.1016/j.tsf.2009.07.011 ↗
46. The effect of vacuum annealing on microstructure, adhesion strength and electrochemical behaviors of multilayered AlCrTiSiN coatings10.1016/j.apsusc.2018.10.171 ↗
47. The study of the adhesion of a TiN coating on steel and titanium alloy substrates using a multi-mode scratch tester10.1016/j.triboint.2005.04.011 ↗
48. Mechanical and tribological properties of CrN/TiN multilayer coatings deposited by pulsed dc magnetron sputtering10.1016/j.surfcoat.2015.06.064 ↗
49. Structure, adhesion and corrosion behavior of CrN/TiN superlattice coatings deposited by the combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering10.1016/j.surfcoat.2015.10.009 ↗
50. Effect of the substrate temperature in ZrN coatings grown by the pulsed arc technique studied by XRD10.1016/j.surfcoat.2006.02.030 ↗
51. Effect of substrate temperature on microstructure and optical properties of nanocrystalline alumina thin films10.1016/j.ceramint.2013.04.104 ↗
52. Hard and superhard nanocomposite coatings10.1016/S0257-8972(99)00586-1 ↗
53. Predictive tools for the design of erosion resistant coatings10.1016/j.surfcoat.2008.08.050 ↗
54. Thermal stability and oxidation resistance of sputtered TiAlCrN hard coatings10.1016/j.surfcoat.2017.05.053 ↗
55. Mechanical properties and impact resistance of multilayered TiAlN/ZrN coatings10.1016/j.surfcoat.2012.03.013 ↗
56. Effects of mechanical properties and layer structure on the cyclic dynamic loading of TiN-based coatings10.1016/j.surfcoat.2011.07.079 ↗