Surfactant-Free Electroless Codeposition of Ni–P–MoS2/Al2O3 Composite Coatings

Ping Liu, Yongwei Zhu, Qi Shen, Meifu Jin, Gaoyan Zhong, Zhiwei Hou, Xiao Zhao, Shuncai Wang, Shoufeng Yang

Coatings· Volume 9· Issue 2

Abstract

This paper presents the influence of an inorganic Al2O3 layer over MoS2 particles on the tribological performance of electroless Ni–P–MoS2/Al2O3 composite coatings fabricated without using surfactants. The Al2O3-coated MoS2 particles were prepared by a heterogeneous nucleation process. The dry sliding tests of the composite coatings were tested against a WC ball. SEM was used to observe the surface morphology of particles, composite coatings, and worn surfaces. The results indicate that the coverage of an Al2O3 coating on MoS2 particles significantly affects the surface morphology, frictional coefficient and wear loss of the composite coatings. The incorporation of Al2O3-coated MoS2 particles with lower coverage (up to 7% of Al2O3) could obtain compact surface structure of composite coatings, which contribute to reduced wear loss. However, higher coverage would lead to loose surface structure of the composite coatings, and thus increase their wear loss.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Semiconductor materials and interfaces · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Jiangsu Key Laboratory of Precision and Micro-Manufacturing Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China

College of Engineering, Nanjing Agricultural University, Nanjing 210031, China

Key Laboratory of Modern Agricultural Equipment and Technology, Ministry of Education/High-tech Key Laboratory of Agricultural Equipment & Intelligentization of Jiangsu Province, Jiangsu University, Zhenjiang 212013, China

Jiangsu Key Laboratory of Advanced Manufacturing Technology, Huaiyin Institute of Technology, Nanjing 223003, China

Faculty of Engineering and Environment, University of Southampton, Southampton SO17 1BJ, UK

Production Engineering, Machine Design and Automation, Department of Mechanical Engineering, Katholieke Universiteit Leuven (KU Leuven), Leuven 3001, Belgium

Funding

National Natural Science Foundation of China · Key Laboratory of Modern Agricultural Equipment and Technology (Jiangsu University), Ministry of Education(MOE) / High-tech Key Laboratory of Agricultural Equipment \Intelligentization of Jiangsu Province · Jiangsu Key Laboratory of Precision and Micro-Manufacturing Technology · Jiangsu Key Laboratory of advanced manufacturing technology(Huaiyin Institute of Technology

References (49)

Show source-provided references
1. A novel electroless plating of Ni–P–Al–ZrO2 nanocomposite coatings and their properties10.1016/j.ceramint.2014.04.040 ↗
2. Characterization of Ni–P–SiO2–Al2O3 nano-composite coatings on aluminum substrate10.1016/j.matchemphys.2016.12.023 ↗
3. Preparation of Ni–P–GO composite coatings and its mechanical properties10.1016/j.surfcoat.2015.04.028 ↗
4. Influence of heat treatment on tribological properties of electroless Ni–P and Ni-P-Al2O3 coatings on Al-Si casting alloy10.1016/j.apsusc.2009.11.057 ↗
5. Effect of alumina nanoparticles as nanocomposites on morphology and corrosion resistance of electroless Ni–P coatings10.1179/174329409X438998 ↗
6. Effect of annealing temperature on microstructure, mechanical and tribological properties of nano-SiC reinforced Ni–P coatings10.1016/j.wear.2016.03.011 ↗
7. Corrosion and tribological behavior of electroless Ni–P/nano–SiC composite coating on aluminium 606110.1179/1743294415Y.0000000012 ↗
8. Improvement in tribological behavior of novel sol-enhanced electroless Ni–P–SiO2 nanocomposite coatings
9. Corrosion behaviour of electroless Ni–P–TiO2 nanocomposite coatings using Taguchi10.1179/1743294412Y.0000000093 ↗
10. A study on the wear resistance of electroless Ni-P/Diamond composite coatings10.1016/S0043-1648(00)00330-6 ↗
11. Tribological characteristics of electroless Ni–P–MoS2 composite coatings at elevated temperatures10.1016/j.apsusc.2012.10.055 ↗
12. Study of corrosion and friction reduction of electroless N–P coating with molybdenum disulfide nanoparticles10.1007/s11998-008-9131-7 ↗
13. Studies on electroless nickel–PTFE composite coatings10.1179/174329405X40902 ↗
14. The effect of incorporated self-lubricated BN(h) particles on the tribological properties of Ni–P–BN(h) composite coatings10.1016/j.apsusc.2015.09.207 ↗
15. Homogeneous functional Ni–P/ceramic nanocomposite coatings via stable dispersions in electroless nickel electrolytes10.1016/j.jcis.2011.09.032 ↗
16. Electroless Ni–P–PTFE-Al2O3 dispersion nanocomposite coating for corrosion and wear resistance10.1007/s11665-013-0710-0 ↗
17. Influence of SiO2 nanoparticles on hardness and corrosion resistance of electroless Ni–P coatings10.1016/j.surfcoat.2014.11.044 ↗
18. Optimization of Coating Process Parameters to Improve microhardness of Ni–P–TiO2 composite coatings10.1016/j.matpr.2015.07.303 ↗
19. Corrosion behavior of Ni–P–nano–Al2O3 composite coating in the presence of anionic and cationic surfactants10.1016/j.surfcoat.2016.12.089 ↗
20. Effect of surfactants on the coating properties and corrosion behaviour of Ni–P–nano–TiO2 coatings10.1016/j.surfcoat.2015.07.008 ↗
21. Preparation of electroless Ni–P composite coatings containing nano-scattered alumina in presence of polymeric surfactant10.1016/j.pnsc.2012.06.006 ↗
22. On the Influence of surfactant incorporation during electroless nickel plating10.1021/ie202625n ↗
23. Electroless nickel, alloy, composite and nano coatings—A critical review10.1016/j.jallcom.2013.03.107 ↗
24. Electroless alloy/composite coatings: A review10.1007/BF02706445 ↗
25. The performance of surfactant on the surface characteristics of electroless nickel coating on magnesium alloy10.1016/j.porgcoat.2011.10.022 ↗
26. Electroless deposition of Ni–P–nano–ZrO2 composite coatings in the presence of various types of surfactants10.1016/j.jcis.2012.03.049 ↗
27. Effect of surfactants on codeposition of PTFE particles with electroless Ni–P coating10.1016/S0254-0584(01)00513-2 ↗
28. Comparison of the coating properties and corrosion rates in electroless Ni–P–PTFE composites prepared by different types of surfactants10.1016/j.apsusc.2011.05.043 ↗
29. Effects of Surfactants in an Electroless Nickel–Plating Bath on the Properties of Ni–P Alloy Deposits10.1021/ie0105831 ↗
30. Influence of fluoro surfactants on the codeposition of ceramic nanoparticles and the morphology of electroless Ni–P coatings10.1016/j.surfcoat.2010.06.059 ↗
31. Effect of Sodium Dodecyl Sulphate on the Composition of Electroless Nickel-Yttria Stabilized Zirconia Coatings10.4236/aces.2011.13018 ↗
32. Surfactant-free electrodeposition of reduced graphene oxide/copper composite coatings with enhanced wear resistance10.1016/j.apsusc.2017.10.014 ↗
33. Preparation and characterization of Ni–P/nanodiamond coatings: Effects of surfactants10.1016/j.diamond.2012.10.003 ↗
34. Effect of surfactant on the fabrication and characterization of Ni–P–CNT composite coatings10.1016/j.jallcom.2010.10.057 ↗
35. Effect of surfactants on performance of electroless plating baths for nickel-ceramic composite membrane fabrication10.1179/1743294411Y.0000000035 ↗
36. Wear and scratch behaviour of electroless Ni-P-nano-TiO2: Effect of surfactants10.1016/j.wear.2015.11.015 ↗
37. Song, X., Jiang, N., Li, Y., Xu, D., and Qiu, G. (2008). Synthesis of CeO2-coated SiO2 nanoparticle and dispersion stability of its suspension. Mater. Chem. Phys., 128–135.10.1016/j.matchemphys.2008.01.042 ↗
38. Recent progress in surface coating of cathode materials for lithium ion secondary batteries10.1016/j.jallcom.2017.02.230 ↗
39. Comparative study of Al2O3-coated LiCoO2 electrode derived from different Al precursors uniformity, microstructure and electrochemical properties10.1016/j.electacta.2015.08.039 ↗
40. Hydrophilicity characterization of Al2O3-coated MoS2 particles by using thin layer wicking and sessile drop method10.1016/j.powtec.2015.05.011 ↗
41. Surface coating and application in plating of MoS2 powders with Al2O3
42. Preparation and properties of Ni–P–MoS2/Al2O3 composite coating
43. Friction and wear properties of Ni–P electroless composite coatings with core-shell nanodiamond
44. In situ X-ray diffraction of the transformation of gibbsite to a-alumina through calcination: Effect of particle size and heating rate10.1107/S0021889809021232 ↗
45. An investigation on corrosion resistance of asapplied and heat treated Ni–P/nanoSiC coatings10.1016/j.matdes.2009.04.020 ↗
46. The effect of heat treatment on the structure and abrasive wear resistance of autocatalytic NiP and NiP–SiC coatings10.1016/S0257-8972(01)01492-X ↗
47. Electroless Ni–P–(nano-MoS2) composite coatings and their corrosion properties10.1179/174329408X282532 ↗
48. The influence of SDS and CTAB surfactants on the surface morphology and surface topography of electroless Ni–P deposits10.1016/j.jmatprotec.2008.01.057 ↗
49. Deposition and properties of electroless nickel–phosphorus–molybdenum disulfide composites10.1016/S0026-0576(97)81449-3 ↗