High-Temperature Oxidation Behaviors of TA15 Titanium Alloy after Mechanical Grinding and Laser Cleaning

Zhi-Chao Li, Jie Xu, Dong-He Zhang, Zhen-Hai Xu, Shi-Rui Yang, De-Bin Shan, Bin Guo

Coatings· Volume 11· Issue 9

Abstract

This paper presents the results of a study on the high-temperature oxidation characteristics after mechanical and laser removal of TA15 titanium alloy oxide film. The morphology, components, and roughness of the surface were characterized by scanning electron microscope (SEM), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and laser confocal microscope (OM). The oxide film can be effectively removed with mechanical grinding and laser cleaning, and the oxide film after mechanical grinding is thicker and looser than that of after laser cleaning. The oxide film is principally composed of TiO2, Ti2O3 and TiO. Besides, there is a small amount of aluminum oxide on the surface. The surface after mechanical grinding was rougher than that of after laser cleaning. Thus, this work indicates that laser can not only clean the oxide film completely, but also strengthen the surface, which is a promising way to favor the widespread application of laser cleaning technology.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory of Micro-Systems and Micro-Structures Manufacturing of Ministry of Education, Harbin Institute of Technology, Harbin 150080, China

School of Materials Science and Engineering, Harbin Institute of Technology, Shenzhen 518055, China

Beijing Power Machinery Research Institute, Beijing 100074, China

Funding

the Guangdong Province Key Area R&D Program · the National Key R&D Program of China · the National Natural Science Foundation of China

References (30)

Show source-provided references
1. Titanium and titanium-based alloys for aerospace
2. Chemical interaction of the Ti94Al6 and Ti91Al9 alloys with ammonia between 150 and 500 °C10.1134/S002016851012006X ↗
3. Application of titanium and titanium alloys to fixed dental prostheses10.1016/j.jpor.2019.04.011 ↗
4. Jet electrochemical machining of TB6 titanium alloy10.1007/s00170-016-9500-9 ↗
5. Effect of titanium addition on the oxidation resistance of Fe–13Cr-5Al-0.3Ti alloy in air between 700 °C–1100 °C
6. Investigation of the oxidation behavior of orthorhombic Ti2AlNb Alloy10.1007/s11665-015-1449-6 ↗
7. Characterization of passive oxide film on a Ti–5%Ta–1.8%Nb alloy on exposure to severe oxidizing conditions10.1016/j.matchar.2010.08.009 ↗
8. Oxidation mechanism of biomedical titanium alloy surface and experiment10.1155/2020/1678615 ↗
9. Structural and me-chanical properties of titanium oxide thin films for biomedical application10.1016/j.tsf.2009.09.046 ↗
10. Characterization of air-formed surface oxide film on Ti–29Nb–13Ta–4.6Zr alloy surface using XPS and AES10.1016/j.corsci.2008.06.002 ↗
11. Oxidation stability of various Ti-alloys10.1007/s10973-017-6154-2 ↗
12. High-temperature oxidation of Ti–44Al–6Nb–2Cr–0.3Si–0.1C Alloy10.1166/sam.2016.2883 ↗
13. Oxidation behaviors of TA15 titanium alloy and TiBw reinforced TA15 matrix composites prepared by spark plasma sintering10.1016/j.jmst.2019.07.037 ↗
14. A study on laser cleaning and pulsed gas tungsten arc welding of Ti–3Al–2.5V alloy tubes10.1016/j.jmatprotec.2009.08.017 ↗
15. Ultraviolet laser cleaning and surface characterization of AH36 steel for rust removal10.2351/1.5127569 ↗
16. Nanosecond pulsed fiber laser cleaning of natural marine micro-biofoulings from the surface of aluminum alloy10.1016/j.jclepro.2019.118724 ↗
17. Inhibition effectiveness of laser-cleaned nanostructured aluminum alloys to sulfate-reducing bacteria based on superwetting and ultraslippery surfaces10.1021/acsabm.0c00714 ↗
18. A study of microstructure and mechanical properties of aluminum alloy using laser cleaning10.1016/j.jmapro.2019.04.015 ↗
19. Effect of scanning speed with UV laser cleaning on adhesive bonding tensile properties of CFRP10.1007/s10443-019-09768-4 ↗
20. Fabrication of superhydrophilic or superhydrophobic self-cleaning metal surfaces using picosecond laser pulses and chemical fluorination10.1080/10420150.2016.1211658 ↗
21. Characterizing corrosion properties of carbon steel affected by high-power laser cleaning10.1016/j.conbuildmat.2020.122085 ↗
22. Research on grain refinement and wear behavior of micro-remelted Ta15 alloy surface by laser cleaning10.1016/j.matchemphys.2020.124022 ↗
23. Surface roughness: A review of its measurement at micro-/nano-scale
24. Experimental investigation of added frictional resistance by paint rough surface using a rotating cylinder10.1007/s00773-020-00717-6 ↗
25. Characterization of oxide film formed on NiTi by laser oxidation10.1016/j.msea.2006.10.164 ↗
26. Surface analysis of chemical stripping titanium alloy oxide films10.1007/s11595-012-0473-8 ↗
27. Decontamination of U(VI) on graphene oxide/Al2O3 composites investigated by XRD, FT-IR and XPS techniques10.1016/j.envpol.2019.01.126 ↗
28. An X-ray photoelectron spectroscopy sputter profile study of the native air-formed oxide film on titanium10.1016/S0169-4332(98)00927-1 ↗
29. Ultrasonic impact treatment induced oxidation of Ti6Al4V alloy10.1016/j.actamat.2015.10.041 ↗
30. Ouyang, P., Mi, G., Li, P., He, L., Cao, J., and Huang, X. (2018). Non-isothermal oxidation behavior and mechanism of a high tem-perature near-α titanium alloy. Materials, 11.10.3390/ma11112141 ↗