journal article·2020-02-20Open access

Synchronous Shot Peening Applied on HVOF for Improvement on Wear Resistance of Fe-based Amorphous Coating

Zhidan Zhou, Junchao Shang, Yongxiong Chen, Xiubing Liang, Baolong Shen, Zhibin Zhang

Coatings· Volume 10· Issue 2

Abstract

Shot peening was used synchronously to improve Fe-based amorphous coating performance by delivering ZrO2 ceramic particles into a low-temperature region of a flame during the high velocity oxygen flame (HVOF) spray process. The coating became denser, and its hardness became higher via the new process. Moreover, the compressive residual stress was induced by shot peening. The results from the dry friction test indicated that the coating’s wear resistance was enhanced obviously. The wear mechanism of coatings with and without shot peening is an abrasive wear combined with an oxidation wear at wear test conditions of a low load and a low frequency. The coating with the best wear resistance did not have the strongest microhardness but had the highest compressive residual stress. The compressive residual stress had a significant positive influence on the wear resistance at a low frequency, while its effect is weakened at a high frequency.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Diamond and Carbon-based Materials Research · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Massive Amorphous Metal Science, School of Chemistry and Chemical Engineering, China University of Mining and Technology, Xuzhou 221116, China

Academy of Military Science PLA China, National Innovation Institute of Defense Technology, Beijing 100071, China

Jiangsu Key Laboratory for Advanced Metallic Materials, School of Materials Science and Engineering, Southeast University, Nanjing 211189, China

Funding

Outstanding Innovation Scholarship for Doctoral Candidate of CUMT

References (52)

Show source-provided references
1. Investigations of hot corrosion resistance of hvof coated fe based superalloy a-286 in simulated gas turbine environment10.1016/j.engfailanal.2019.104224 ↗
2. Effect of hydrostatic pressure on the corrosion behavior of hvof-sprayed fe-based amorphous coating10.1016/j.jallcom.2018.05.100 ↗
3. Study of structure and corrosion resistance of fe-based amorphous coatings prepared by hvaf and hvof10.1016/j.corsci.2010.12.022 ↗
4. Relationships between spray parameters, microstructures and ultrasonic cavitation erosion behavior of hvof sprayed fe-based amorphous/nanocrystalline coatings10.1016/j.ultsonch.2017.04.011 ↗
5. Influence of ceramic particles and process parameters on residual stress of flame-sprayed fe-based coatings10.1016/j.surfcoat.2018.08.069 ↗
6. On the bonding strength in thermally sprayed fe-based amorphous coatings10.1016/j.surfcoat.2012.12.018 ↗
7. Effect of heat treatment on the structure, cavitation erosion and erosion–corrosion behavior of fe-based amorphous coatings10.1016/j.triboint.2015.04.039 ↗
8. Composite coating containing wc/12co cermet and fe-based metallic glass deposited by high-velocity oxygen fuel spraying10.1016/j.jallcom.2010.03.209 ↗
9. Characterization of gas tunnel type plasma sprayed tin reinforced fe-based metallic glass coatings10.1016/j.jallcom.2012.09.111 ↗
10. Laminar fe-based amorphous composite coatings with enhanced bonding strength and impact resistance10.1016/j.actamat.2014.03.047 ↗
11. Residual stresses in high-velocity oxy-fuel thermally sprayed coatings—Modelling the effect of particle velocity and temperature during the spraying process10.1016/j.actamat.2007.05.031 ↗
12. Residual stress development in cold sprayed al, cu and ti coatings10.1016/j.actamat.2013.06.033 ↗
13. Effects of processing conditions on the mechanical properties and deformation behaviors of plasma-sprayed thermal barrier coatings: Evaluation of residual stresses and mechanical properties of thermal barrier coatings on the basis of in situ curvature measurement under a wide range of spray parameters10.1016/j.actamat.2012.09.020 ↗
14. Experimental and numerical study of residual stress evolution in cold spray coating10.1016/j.apsusc.2013.09.074 ↗
15. Peening action and residual stresses in high-velocity oxygen fuel thermal spraying of 316l stainless steel10.1361/105996301770349457 ↗
16. The effect of residual stress on the electrochemical corrosion behavior of fe-based amorphous coatings in chloride-containing solutions10.1016/j.surfcoat.2016.05.034 ↗
17. Effect of grinding parameters on the wear resistance and residual stress of hvof-deposited wc–10co–4cr coating10.1016/j.surfcoat.2016.09.067 ↗
18. Modeling residual stress development in thermal spray coatings: Current status and way forward10.1007/s11666-017-0590-1 ↗
19. Effect of residual stress on the wear resistance of thermal spray coatings10.1007/s11666-015-0309-0 ↗
20. Effect of substrate roughness induced by grit blasting upon adhesion of wc-17% co thermal sprayed coatings10.1016/S0040-6090(00)01447-4 ↗
21. Influence of substrate roughness on the bonding mechanisms of high velocity oxy-fuel sprayed coatings10.1016/j.tsf.2005.03.024 ↗
22. Evaluation of wc-10ni thermal spray coating with shot peening on the fatigue strength of aisi 4340 steel10.1016/j.proeng.2010.03.070 ↗
23. Fatigue behavior of cold spray coatings: The effect of conventional and severe shot peening as pre-/post-treatment10.1016/j.surfcoat.2015.10.063 ↗
24. Surface severe plastic deformation of aisi 304 via conventional shot peening, severe shot peening and repeening10.1016/j.apsusc.2015.05.093 ↗
25. Simultaneous spray deposition and peening of metals (ssp)10.1179/030716984803274981 ↗
26. Elastoplastic analysis of process induced residual stresses in thermally sprayed coatings
27. Warm-particle peening assisted hvof spraying: A new process to improve the coating performances10.1016/j.surfcoat.2019.03.077 ↗
28. Influence of shot peening on high cycle fatigue properties of the high-strength wrought magnesium alloy az8010.1016/j.scriptamat.2004.11.003 ↗
29. Mechanical surface treatments on titanium, aluminum and magnesium alloys10.1016/S0921-5093(98)01168-X ↗
30. Effect of substrate roughness on splatting behavior of hvof sprayed polymer particles: Modeling and experiments10.1361/105996306X146839 ↗
31. Examination of substrate surface melting-induced splashing during splat formation in plasma spraying10.1361/105996306X146947 ↗
32. Super-resolution reconstruction based on incoherent optical aperture synthesis10.1364/OL.38.003471 ↗
33. Numerical analysis of flame and particle behavior in an hvof thermal spray process10.1016/j.matdes.2016.02.008 ↗
34. Shot peening mechanics: Experimental and theoretical analysis10.1016/0167-6636(94)00036-G ↗
35. Comparative studies on microstructure and mechanical properties of crn, cr–c–n and cr–mo–n coatings10.1016/j.jmatprotec.2006.11.090 ↗
36. High corrosion and wear resistance of al-based amorphous metallic coating synthesized by hvaf spraying10.1016/j.jallcom.2017.11.274 ↗
37. Residual stresses, interfacial adhesion and tribological properties of mon/cu composite coatings10.1016/j.wear.2012.01.007 ↗
38. Tribological performance of magnetic thin-film glass disks: Its relation to surface roughness and lubricant structure and its thickness10.1016/0043-1648(95)06648-9 ↗
39. Effects of al addition on microstructure and wear resistance of high-velocity-oxygen-fuel-sprayed feconicrmn high entropy alloy coating10.1166/sam.2019.3479 ↗
40. Assessments on friction and wear behaviors of p110 steel and chromizing coating sliding against two counterparts under dry and wet conditions10.1016/j.apsusc.2012.01.128 ↗
41. Effect of la2o3 addition on the microstructure, hardness and abrasive wear behavior of flame sprayed ni based coatings10.1016/j.wear.2008.12.029 ↗
42. Effect of heat treatment on residual stress and wear behaviors of the tini/ti 2 ni based laser cladding composite coatings10.1016/j.optlastec.2017.07.029 ↗
43. Wear deformation of ordered fe-al intermetallic alloys10.1016/0043-1648(93)90527-S ↗
44. Correlation of yield strength and tensile strength with hardness for steels10.1007/s11665-008-9225-5 ↗
45. Microstructure and mechanical properties of febsinb metallic glass coatings by twin wire arc spraying10.1007/s11666-013-9892-0 ↗
46. Effect of the microstructure and residual stress on tribological behavior of induction hardened gcr15 steel10.1016/j.triboint.2017.05.028 ↗
47. Effect of varying load on wear resistance of carbon steel under unlubricated conditions10.1016/S0043-1648(03)00222-9 ↗
48. Wear behavior of plasma-sprayed carbon nanotube-reinforced aluminum oxide coating in marine and high-temperature environments10.1007/s11666-011-9669-2 ↗
49. Sliding wear behavior of cr–mo–cu alloy cast irons with and without nano-additives10.1016/j.wear.2011.06.015 ↗
50. Residual stresses in tin, dlc and mos2 coated surfaces with regard to their tribological fracture behaviour10.1016/j.wear.2009.01.004 ↗
51. Tribological contact analysis of a rigid ball sliding on a hard coated surface, part iii: Fracture toughness calculation and influence of residual stresses10.1016/j.surfcoat.2005.03.042 ↗
52. Isolating the effect of residual stresses on coating wear by a mechanical stress relaxation technique10.1016/j.tsf.2017.06.016 ↗