journal article·2017-12-05Open access

Insights on the Role of Copper Addition in the Corrosion and Mechanical Properties of Binary Zr-Cu Metallic Glass Coatings

Junlei Tang, Qiuhong Zhu, Yingying Wang, Mihai Apreutesei, Hu Wang, Philippe Steyer, Mohamad Chamas, Alain Billard

Coatings· Volume 7· Issue 12

Abstract

The effect of copper addition on the corrosion resistance and mechanical properties of binary Zr100–xCux (x = 30, 50, 80, 90 at.%) glassy coatings was investigated by means of electrochemical measurements, scanning electron microscopy (SEM), energy dispersive analysis spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS) and nano-indentation techniques. The corrosion resistance in 0.01 M deaerated H2SO4 solution and the mechanical properties of the Zr-Cu glassy coatings depend considerably upon the copper content in the glassy matrix. The top surfaces of the Zr-Cu coatings with lower Cu content were covered by a compact protective ZrO2 passive film. The competition between the oxidation of Zr atoms (ZrO2 film formation) and the oxidation–dissolution of Cu atoms assumed the most important role in the electrochemical behavior of the Zr-Cu glassy coatings. The generation of ZrO2 on the surface benefited the formation of passive film; and the corrosion resistance of the metallic glass coatings depended on the coverage degree of ZrO2 passive film. The evolution of free volume affected both the mechanical and corrosion behaviors of the Zr-Cu glassy coatings.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · High-Temperature Coating Behaviors · Electrodeposition and Electroless Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Chemistry and Chemical Engineering, Southwest Petroleum University, Chengdu 610500, China

State Key Laboratory of Oil and Gas Reservoir Geology and Exploitation, Southwest Petroleum University, Chengdu 610500, China

MATEIS Laboratory-UMR CNRS 5510, Université de Lyon, INSA-Lyon, 7 Avenue Jean Capelle, 69621 Villeurbanne CEDEX, France

School of Material Science and Engineering, Southwest Petroleum University, Chengdu 610500, China

Institut FEMTO-ST, CNRS, UTBM, University Bourgogne Franche-Comté, Site de Montbéliard, 90010 Belfort CEDEX, France

Funding

National Natural Science Foundation of China · Qihang Science Research founding of Southwest Petroleum University

References (39)

Show source-provided references
1. Metallic glass matrix composites10.1016/j.mser.2015.12.001 ↗
2. Bulk metallic glasses10.1016/j.mser.2004.03.001 ↗
3. Metallic glasses as structural materials10.1016/j.scriptamat.2005.09.051 ↗
4. Hashimoto, K. (1983). Chapter 24—Chemical properties. Amorphous Metallic Alloys, Elsevier.10.1016/B978-0-408-11030-3.50029-7 ↗
5. Corrosion behavior of amorphous and crystalline Cu50Ti50 and Cu50Zr50 alloys10.1016/0022-3093(78)90053-4 ↗
6. The influence of structure on the corrosion of glassy copper-zirconium alloys
7. Acid corrosion of amorphous and crystalline Cu-Zr alloys10.1016/0169-4332(88)90036-0 ↗
8. Comparing the pitting corrosion behavior of prominent Zr-based bulk metallic glasses10.1557/jmr.2014.371 ↗
9. Metallic glasses from “alchemy” to pure science: Present and future of design, processing and applications of glassy metals10.1016/j.matdes.2011.09.028 ↗
10. Correlation between mechanical behavior and glass forming ability of Zr-Cu metallic glasses10.1016/j.intermet.2011.03.009 ↗
11. Mechanical behavior of amorphous alloys10.1016/j.actamat.2007.01.052 ↗
12. Extrinsic mechanical size effects in thin ZrNi metallic glass films10.1016/j.actamat.2015.02.038 ↗
13. Recent progress in nanoimprint technology and its applications10.1088/0022-3727/37/11/R01 ↗
14. Nanoimprinting of Ti–Cu-based thin-film metallic glasses deposited by unbalanced magnetron sputtering10.1016/j.jallcom.2016.11.174 ↗
15. Thin film metallic glasses: Unique properties and potential applications10.1016/j.tsf.2012.03.092 ↗
16. Compositional-induced structural change in ZrxNi100−x thin film metallic glasses10.1016/j.jallcom.2013.12.054 ↗
17. Microstructural, thermal and mechanical behavior of co-sputtered binary Zr-Cu thin film metallic glasses10.1016/j.tsf.2013.05.177 ↗
18. Amorphous Zr-Cu thin-film alloys with metallic glass behavior10.1016/j.jallcom.2016.12.098 ↗
19. Estimation of compositions of Zr-Cu binary sputtered film and its characterization10.1155/2008/518354 ↗
20. Corrosion behavior and porous structure formation of sputtered Cu-Zr nanostructured films10.1016/j.jallcom.2007.10.101 ↗
21. Binary Zr-Ni/Co metallic glass films: Role of the structural state on their durability10.1016/j.actamat.2015.01.056 ↗
22. Study of ZrN layers deposited by reactive magnetron sputtering
23. Improved chemical stability of ITO transparent anodes with a SnO2 buffer layer for organic solar cells10.1016/j.solmat.2015.10.005 ↗
24. Zr-Cu thin film metallic glasses: An assessment of the thermal stability and phases’ transformation mechanisms10.1016/j.jallcom.2014.08.253 ↗
25. Inhibition of copper corrosion by bis-(1,1′-benzotriazoly)-α,ω-diamide compounds in aerated sulfuric acid solution10.1016/j.apsusc.2005.07.010 ↗
26. Effect of surface finishing of a Zr-based bulk metallic glass on its corrosion behavior10.1016/j.corsci.2010.01.027 ↗
27. Corrosion and surface study of sputtered Al-W coatings with a range of tungsten contents10.1016/j.corsci.2013.01.002 ↗
28. Effects of Cu on the passive film stability of Fe-20Cr-xCu (x = 0, 2, 4 wt.%) alloys in H2SO4 solution10.1016/j.electacta.2012.10.058 ↗
29. Atomic packing density and its influence on the properties of Cu-Zr amorphous alloys10.1016/j.scriptamat.2007.07.019 ↗
30. Microstructure and electrochemical behavior of Ti-coated Zr55Al10Ni5Cu30 bulk metallic glass10.1016/j.intermet.2009.04.009 ↗
31. Paunovic, M., and Schlesinger, M. (2006). Equilibrium Electrode Potential. Fundamentals of Electrochemical Deposition, Wiley-Interscience. [2nd ed.].10.1002/0470009403 ↗
32. Characterization of the surface film on Zr-based bulk metallic glass using X-ray photoelectron spectroscopy (XPS) and scanning electron microscopy (SEM)10.1016/j.jallcom.2011.03.051 ↗
33. Copper corrosion inhibition in O2-saturated H2SO4 solutions10.1016/j.corsci.2009.12.035 ↗
34. Correlation between plasticity and other materials properties of Cu-Zr bulk metallic glasses: An atomistic simulation study10.1016/j.actamat.2010.10.027 ↗
35. Free-volume-induced enhancement of plasticity in a monolithic bulk metallic glass at room temperature10.1016/j.scriptamat.2008.02.025 ↗
36. Enhanced plasticity in Zr-Cu-Ag-Al-Be bulk metallic glasses10.1016/j.jnoncrysol.2015.01.002 ↗
37. Crystallization and hardening of Zr-40 at.% Cu thin film metallic glass: Effects of isothermal annealing10.1016/j.matdes.2015.07.149 ↗
38. Effect of thermally induced relaxation on passivity and corrosion of an amorphous Al-Co-Ce alloy10.1016/j.corsci.2012.03.012 ↗
39. Passivation behaviour of structurally relaxed Zr48Cu36Ag8Al8 metallic glass10.1016/j.jallcom.2009.01.056 ↗