Recent Development of Corrosion Factors and Coating Applications in Biomass Firing Plants
Source abstract
Abstract
Due to global warming, biomass fuels are gradually being used to replace fossil fuels. However, high-temperature biomass corrosion is a crucial issue affecting its future application. In this article, different factors affecting boiler performance are summarized from various studies to guide the optimization of boiler parameters in practical applications, such as corrosive components and boiler temperatures. Meanwhile, different coating formation methods and materials are summarized to provide better protection strategies. The potential coating materials for future research are also discussed. The addition of other elements, such as Ti, Mo, and W, has the potential to accelerate the formation of oxide layers during high-temperature corrosion and directly slow down the corrosion rate. Future studies should focus on these elements containing materials.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Thermochemical Biomass Conversion Processes · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
College of Mechanical Engineering, Yangzhou University, Yangzhou 225127, China
Funding
Natural Science Foundation of Jiangsu Province · Innovative and Entrepreneurial Talents Program of Jiangsu Province (Innovative and Entrepreneurial Doctors) · Lvyang Jinfeng Plan for Excellent Doctor of Yangzhou City
References (82)
Show source-provided references
1. Biomass combustion in fluidized bed boilers: Potential problems and remedies10.1016/j.fuproc.2008.07.012 ↗
2. A review on biomass as a fuel for boilers10.1016/j.rser.2011.02.015 ↗
3. Potential applications of renewable energy sources, biomass combustion problems in boiler power systems and combustion related environmental issues10.1016/j.pecs.2005.02.002 ↗
4. Combustion characteristics of different biomass fuels10.1016/j.pecs.2003.10.004 ↗
5. Experiences with high temperature corrosion at straw-firing power plants in Denmark10.1002/maco.201005856 ↗
6. Leading global energy and environmental transformation: Unified ASEAN biomass-based bio-energy system incorporating the clean development mechanism10.1016/j.biombioe.2011.04.013 ↗
7. Discursive shifts in energy from biomass: A 30 year European overview10.1016/j.rser.2012.03.037 ↗
8. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
9. Experimental research on agglomeration in straw-fired fluidized beds10.1016/j.apenergy.2011.05.046 ↗
10. Combustion properties of biomass10.1016/S0378-3820(97)00059-3 ↗
11. An overview of the chemical composition of biomass10.1016/j.fuel.2009.10.022 ↗
12. Mathematical Modeling and Experimental Study of Biomass Combustion in a Thermal 108 MW Grate-Fired Boiler10.1021/ef700689r ↗
13. Deposition and high temperature corrosion in a 10 MW straw fired boiler10.1016/S0378-3820(97)00062-3 ↗
14. Field test corrosion experiments in Denmark with biomass fuels. Part 2: Co-firing of straw and coal10.1002/1521-4176(200203)53:3<185::AID-MACO185>3.0.CO;2-K ↗
15. Sharp, W.B.A. (2011). Superheater Corrosion in Biomass Boilers: Today’s Science and Technology.10.2172/1048711 ↗
16. Corrosion of alloys and their diffusion aluminide coatings by KCl:K2SO4 deposits at 650 °C in air10.1002/maco.200804118 ↗
17. Influence of fuel ashes on corrosion of surface coatings cladded by CMT method
18. Kawahara, Y. (2016). An Overview on Corrosion-Resistant Coating Technologies in Biomass/Waste-to-Energy Plants in Recent Decades. Coatings, 6.10.3390/coatings6030034 ↗
19. Utilizing biomass and waste for power production—A decade of contributing to the understanding, interpretation and analysis of deposits and corrosion products10.1016/j.fuel.2004.08.026 ↗
20. Advances in Corrosion-Resistant Thermal Spray Coatings for Renewable Energy Power Plants. Part I: Effect of Composition and Microstructure10.1007/s11666-019-00938-1 ↗
21. Corrosion behaviour of Ni and nickel aluminide coatings exposed in a biomass fired power plant for two years10.1016/j.surfcoat.2018.12.129 ↗
22. Wu, D.L., Dahl, K.V., Grumsen, F.B., Christiansen, T.L., Montgomery, M., and Hald, J. (2020). Breakdown mechanism of γ-Al2O3 on Ni2Al3 coatings exposed in a biomass fired power plant. Corros. Sci., 108583.10.1016/j.corsci.2020.108583 ↗
23. Advances in Corrosion-Resistant Thermal Spray Coatings for Renewable Energy Power Plants: Part II—Effect of Environment and Outlook10.1007/s11666-019-00939-0 ↗
24. Behaviour of NiAl APS-coatings in chlorine-containing atmospheres10.1002/maco.200804140 ↗
25. Effects of Different Fuel Specifications and Operation Conditions on the Performance of Coated and Uncoated Superheater Tubes in Two Different Biomass-Fired Boilers10.1021/acsaem.7b00253 ↗
26. High temperature oxidation of metallic chromium exposed to eight different metal chlorides10.1016/j.corsci.2011.06.007 ↗
27. Determination of the corrosivity of Pb-containing salt mixtures10.1016/j.corsci.2012.09.024 ↗
28. The role of chlorine in high temperature corrosion in waste-to-energy plants10.1080/09603409.1997.11689546 ↗
29. The influence of alloying elements on the chlorine-induced high temperature corrosion of Fe-Cr alloys in oxidizing atmospheres10.1002/(SICI)1521-4176(199910)50:10<561::AID-MACO561>3.0.CO;2-L ↗
30. Role of molten phase content of deposits for high-temperature corrosion in waste incineration environment10.1080/09603409.1997.11689553 ↗
31. Sulfur recirculation for increased electricity production in Waste-to-Energy plants10.1016/j.wasman.2013.09.002 ↗
32. Performance testing of iron based thermally sprayed HVOF coatings in a biomass-fired fluidised bed boiler10.1016/j.surfcoat.2014.04.025 ↗
33. A comparative study on the high temperature corrosion of TP347H stainless steel, C22 alloy and laser-cladding C22 coating in molten chloride salts10.1016/j.corsci.2014.03.012 ↗
34. A thermodynamic approach on vapor-condensation of corrosive salts from flue gas on boiler tubes in waste incinerators10.1016/j.corsci.2008.02.004 ↗
35. A comparative study on the air, the oxygen-enriched air and the oxy-fuel combustion of lignites in CFB10.1016/j.energy.2020.117021 ↗
36. A Comparative Study of Cyclic Oxidation and Sulfates-Induced Hot Corrosion Behavior of Arc-Sprayed Ni-Cr-Ti Coatings at Moderate Temperatures10.1007/s11666-015-0222-6 ↗
37. Chlorine-induced high temperature corrosion of Inconel 625 sprayed coatings deposited with different thermal spray techniques10.1016/j.surfcoat.2016.12.086 ↗
38. Corrosion performance of bi-layer Ni/Cr2C3 -NiCr HVAF thermal spray coating10.1016/j.apsusc.2016.02.002 ↗
39. Thermally sprayed coatings resistant to erosion and corrosion for power plant boilers—A review10.1016/j.surfcoat.2014.10.046 ↗
40. Nickel-based HVOF coatings promoting high temperature corrosion resistance of biomass-fired power plant boilers10.1016/j.fuproc.2014.04.006 ↗
41. Optimisation of HVOF thermal spray coatings for their implementation as MSWI superheater protectors10.1179/147842209X12601838533508 ↗
42. Optimised selection of new protective coatings for biofuel boiler applications10.1002/maco.201005898 ↗
43. Production of nanocrystalline Ni-20Cr coatings for high-temperature applications10.1007/s11666-014-0055-8 ↗
44. Thermal Spray Coatings for High-Temperature Corrosion Protection in Biomass Co-Fired Boilers
45. Optimizing NiCr and FeCr HVOF Coating Structures for High Temperature Corrosion Protection Applications10.1007/s11666-014-0192-0 ↗
46. Influence of KCl and HCl on high temperature corrosion of HVAF-sprayed NiCrAlY and NiCrMo coatings10.1016/j.matdes.2018.03.048 ↗
47. Fireside corrosion behavior of HVOF and plasma-sprayed coatings in advanced coal/biomass Co-fired power plants10.1007/s11666-013-9887-x ↗
48. Modelling fireside corrosion of thermal sprayed coatings in co-firing of coal/biomass10.1002/maco.201307063 ↗
49. Experimental and thermodynamic investigations on the chlorine-induced corrosion of HVOF thermal sprayed NiAl coatings and 304 stainless steels at 700 °C10.1016/j.corsci.2018.02.047 ↗
50. Increased lifetime for biomass and waste to energy power plant boilers with HVOF coatings: High temperature corrosion testing under chlorine-containing molten salt10.1007/s11666-013-9928-5 ↗
51. High temperature corrosion of thermally sprayed NiCr and FeCr coatings covered with a KCl-K2SO4 salt mixture10.1016/j.surfcoat.2014.11.012 ↗
52. HVOF and Laser-Cladded Fe–Cr–B Coating in Simulated Biomass Combustion: Microstructure and Fireside Corrosion10.1007/s11085-017-9774-9 ↗
53. Corrosion testing of Ni alloy HVOF coatings in high temperature environments for biomass applications10.1007/s11666-012-9820-8 ↗
54. High temperature chlorine-induced corrosion of Ni50Cr coating: HVOLF, HVOGF, cold spray and laser cladding10.1016/j.surfcoat.2018.01.025 ↗
55. Fireside corrosion degradation of HVOF thermal sprayed FeCrAl coating at 700–800 °C10.1016/j.surfcoat.2015.01.074 ↗
56. Oksa, M., Metsäjoki, J., and Kärki, J. (2016). Corrosion Testing of Thermal Spray Coatings in a Biomass Co-Firing Power Plant. Coatings, 6.10.3390/coatings6040065 ↗
57. Advanced coatings on furnace wall tubes10.1007/s11666-007-9030-y ↗
58. Chlorine-induced high temperature corrosion of HVAF-sprayed Ni-based alumina and chromia forming coatings10.1016/j.corsci.2017.12.033 ↗
59. Effect of water vapor on the oxidation behavior of HVAF-sprayed NiCr and NiCrAlY coatings10.1002/maco.201710005 ↗
60. Biomass corrosion behavior of steels and coatings in contact with KCl/K2SO4 at 550 °C under an oxy-fuel combustion atmosphere: A screening laboratory test10.1016/j.surfcoat.2018.05.082 ↗
61. High-Temperature Corrosion of HVAF-Sprayed Ni-Based Coatings for Boiler Applications10.1007/s11085-019-09906-0 ↗
62. KCl-Induced High-Temperature Corrosion Behavior of HVAF-Sprayed Ni-Based Coatings in Ambient Air10.1007/s11666-017-0684-9 ↗
63. Investigations on the behavior of laser cladding Ni-Cr-Mo alloy coating on TP347H stainless steel tube in HCl rich environment10.1016/j.surfcoat.2013.06.048 ↗
64. Effect of Al Enrichment by Pack Cementation of FeCr Coatings Deposited by HVOF
65. Microstructural investigations of Ni and Ni2Al3 coatings exposed in biomass power plants10.1080/09603409.2017.1389382 ↗
66. Application of aluminum diffusion coatings to mitigate the KCl-induced high-temperature corrosion10.1002/maco.201609047 ↗
67. Comparison between oxidation of Fe-Cr-Al sputter coatings in air and air-HCl environments at 550 °C10.1179/0960340914Z.00000000095 ↗
68. Quinlan, F.B., and Grobel, L.P. (1942). Treatment of Metals. (2,303,869), U.S. Patent.
69. Structure and morphology of aluminium-oxide films formed by thermal oxidation of aluminium10.1016/S0040-6090(02)00787-3 ↗
70. Electrochemical behaviour of passive films on molybdenum-containing austenitic stainless steels in aqueous solutions10.1016/j.electacta.2004.07.011 ↗
71. KCl-induced high temperature corrosion of selected commercial alloys: Part I: Chromia-formers10.1002/maco.201408213 ↗
72. KCl-induced high temperature corrosion of selected commercial alloys: Part II: Alumina and silica-formers10.1002/maco.201408215 ↗
73. High temperature corrosion of superheater steels by KCl and K2CO3 under dry and wet conditions10.1016/j.fuproc.2012.05.020 ↗
74. KCl-induced high temperature corrosion of the austenitic Fe-Cr-Ni alloys 304L and Sanicro 28 at 600 °C10.1016/j.corsci.2005.05.018 ↗
75. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
76. Corrosion mechanism of alloy 310 austenitic steel beneath NaCl deposit under varying SO2 concentrations in an oxy-fuel combustion atmosphere10.1021/ef4005626 ↗
77. Lab-scale investigation of deposit-induced chlorine corrosion of superheater materials under simulated biomass-firing conditions. Part 1: Exposure at 560 °C10.1021/ef9000924 ↗
78. KCl Induced Corrosion of a 304-type Austenitic Stainless Steel at 600 °C; The Role of Potassium10.1007/s11085-005-5704-3 ↗
79. The influence of KCl on the corrosion of an Austenitic stainless steel (304L) in oxidizing humid conditions at 600 °C: A microstructural study10.1007/s11085-009-9156-z ↗
80. Are NaCl and KCl equally corrosive on superheater materials of steam boilers?10.1016/j.fuel.2012.07.020 ↗
81. Alkali Induced Corrosion of 304-Type Austenitic Stainless Steel at 600 °C; Comparison between KCl, K2CO3 and K2SO410.4028/www.scientific.net/MSF.595-598.367 ↗
82. Effect of Mo and aging temperature on corrosion behavior of (CoCrFeNi)100-xMox high-entropy alloys10.1016/j.jallcom.2019.152139 ↗