journal article·2020-06-30Open access

Evaluation of Functionalized Coatings for the Prevention of Ice Accretion by Using Icing Wind Tunnel Tests

Pedro J. Rivero, Rafael J. Rodriguez, Silvia Larumbe, María Monteserín, Francisco Martín, Amador García, Carolina Acosta, María José Clemente, Paloma García, Julio Mora, Alina Agüero

Coatings· Volume 10· Issue 7

Abstract

Ice accretion presents serious safety issues, as airplanes are exposed to supercooled water droplets both on the ground and while flying through clouds in the troposphere. Prevention of icing is a main concern for both developers and users of aircraft. The successful solution of this problem implies the combination of active and passive methods and the use of advanced sensors for early detection of icing and monitoring of ice accretion and de-icing processes. This paper focuses on the development of passive solutions. These include advanced anti-icing coatings deposited by a variety of chemical methods including sol-gel, advanced paints based on polyester combined with fluorinated derivatives and applied by electrostatic spray deposition and conventional silicone-based paints modified by adding alumina nanoparticles. Water contact angle has been measured in all cases, demonstrating the hydrophobic character of the coatings. An ice accretion test has been carried out in a laboratory scale icing wind tunnel (IWT) located in a cold climate chamber. Three different studies have been undertaken: ice accretion measurement, durability of the anti-icing behavior after several icing/de-icing cycles and ice adhesion testing by means of the double lap shear test (DLST) methodology. All the studied coatings have shown significant anti-icing behavior which has been maintained, in some cases, beyond 25 cycles. Although these results are still far from any possible application for aeronautic components, they provide interesting insights for new developments and validate the laboratory scale tests.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Icing and De-icing Technologies · Surface Modification and Superhydrophobicity · Smart Materials for Construction

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

UPNA—Department of Engineering, Public University of Navarre, Campus Arrosadía s/n, 31006 Pamplona, Spain

INAMAT—Institute for Advanced Materials, Public University of Navarre, Campus Arrosadía s/n, 31006 Pamplona, Spain

AIN—Centre of Advanced Surface Engineering, 31191 Cordovilla, Spain

AIMPLAS—Instituto Tecnológico del Plástico, València Parc Tecnològic, Calle Gustave Eiffel 4, 46980 Paterna, Valencia, Spain

INTA—Instituto Nacional de Técnica Aeroespacial, Área de Materiales Metálicos, Ctra. Ajalvir Km 4, 28850 Torrejón de Ardoz, Spain

References (60)

Show source-provided references
1. Liquid-Infused Nanostructured Surfaces with Extreme Anti-Ice and Anti-Frost Performance10.1021/nn302310q ↗
2. Relationships between Water Wettability and Ice Adhesion10.1021/am1006035 ↗
3. Aircraft icing: An ongoing threat to aviation safety10.1016/j.ast.2017.12.028 ↗
4. Analysis and numerical simulation of an aircraft icing episode near Adolfo Suárez Madrid-Barajas International Airport10.1016/j.atmosres.2017.10.001 ↗
5. Characterizing the Supercooled Large Droplet Environment with Corresponding Turboprop Aircraft Response10.2514/2.2386 ↗
6. Aircraft Icing Caused by Large Supercooled Droplets10.1175/1520-0450(1989)028<0856:AICBLS>2.0.CO;2 ↗
7. De Gregorio, F. (2008). Aerodynamic Performance Degradation Induced by Ice Accretion. PIV Technique Assessment in Icing Wind Tunnel, Springer.
8. Whalen, E., Broeren, A., and Bragg, M. (2006, January 9–12). Considerations for Aerodynamic Testing of Scaled Runback Ice Accretions. Proceedings of the Collection of Technical Papers—44th AIAA Aerospace Sciences Meeting, Reno, Nevada.10.2514/6.2006-260 ↗
9. Study the effect of ice accretion on various aerodynamic flight characteristics using F-16 model
10. Design of Ice-free Nanostructured Surfaces Based on Repulsion of Impacting Water Droplets10.1021/nn102557p ↗
11. Ghalmi, Z., Menini, R., and Farzaneh, M. (2012). Effect of Different Aluminium Surface Treatments on Ice Adhesion Strength, Scientific.Net.10.4028/www.scientific.net/AMR.409.788 ↗
12. Feasibility study of a hybrid ice protection system10.2514/1.C033161 ↗
13. Pulse electro-thermal de-icer (PETD)10.1016/j.coldregions.2010.06.002 ↗
14. Al-Khalil, K. (2007, January 8–11). Thermo-mechanical expulsion deicing system—TMEDS. Proceedings of the Collection of Technical Papers—45th AIAA Aerospace Sciences Meeting, Reno, NV, USA.10.2514/6.2007-692 ↗
15. Schulz, M., and Sinapius, M. (2015). Evaluation of Different Ice Adhesion Tests for Mechanical Deicing Systems, SAE. SAE Technical Paper.10.4271/2015-01-2135 ↗
16. Comparative measures of the toxicity of component chemicals in aircraft deicing fluid10.1002/etc.5620190601 ↗
17. Environmental Impact of Chemical Deicers—A Review10.1007/s11270-005-8265-9 ↗
18. Environmental Impacts of Chemicals for Snow and Ice Control: State of the Knowledge10.1007/s11270-011-1064-6 ↗
19. Anti-icing performance of superhydrophobic surfaces10.1016/j.apsusc.2011.02.057 ↗
20. Understanding the effect of superhydrophobic coatings on energy reduction in anti-icing systems10.1016/j.coldregions.2011.02.006 ↗
21. Atmospheric Ice Adhesion on Water-Repellent Coatings: Wetting and Surface Topology Effects10.1021/acs.langmuir.5b02725 ↗
22. Anti-Icing Superhydrophobic Coatings10.1021/la902882b ↗
23. Wettability versus roughness of engineering surfaces10.1016/j.wear.2010.03.029 ↗
24. Condensation-induced wetting state and contact angle hysteresis on superhydrophobic lotus leaves10.1007/s00396-012-2751-6 ↗
25. Evaluation of ice release coatings at cryogenic temperature for the space shuttle10.1016/j.coldregions.2007.03.002 ↗
26. Are Superhydrophobic Surfaces Best for Icephobicity?10.1021/la104762g ↗
27. Why Superhydrophobic Surfaces Are Not Always Icephobic10.1021/nn302138r ↗
28. Superhydrophobic Surfaces: Are They Really Ice-Repellent?10.1021/la104277q ↗
29. Superhydrophobic surfaces10.1016/j.cocis.2006.06.002 ↗
30. Ice Adhesion to Locks and Dams: Past Work; Future Directions?10.1061/(ASCE)0887-381X(2002)16:2(83) ↗
31. Designing durable icephobic surfaces10.1126/sciadv.1501496 ↗
32. Highly resistant icephobic coatings on aluminum alloys10.1016/j.coldregions.2010.03.004 ↗
33. Ice adhesion on super-hydrophobic surfaces10.1016/j.apsusc.2009.05.033 ↗
34. Low–interfacial toughness materials for effective large-scale deicing10.1126/science.aav1266 ↗
35. A predictive framework for the design and fabrication of icephobic polymers10.1126/sciadv.1701617 ↗
36. Design of anti-icing surfaces: Smooth, textured or slippery?10.1038/natrevmats.2015.3 ↗
37. Predictive Model for Ice Formation on Superhydrophobic Surfaces10.1021/la200816f ↗
38. Wettability of hierarchically-textured ceramic coatings produced by suspension HVOF spraying10.1039/C5TA02130H ↗
39. Developing hydrophobic and superhydrophobic TiO2 coatings by plasma spraying10.1016/j.surfcoat.2016.01.029 ↗
40. Anti-icing performance and durability of suspension plasma sprayed TiO2 coatings10.1016/j.coldregions.2018.11.018 ↗
41. A super-hard superhydrophobic Fe-based amorphous alloy coating10.1016/j.surfcoat.2017.11.046 ↗
42. Mora, J., García, P., Muelas, R., and Agüero, A. (2020). Hard Quasicrystalline Coatings Deposited by HVOF Thermal Spray to Reduce Ice Accretion in Aero-Structures Components. Coatings, 10.10.3390/coatings10030290 ↗
43. Rivero, P.J., Garcia, J.A., Quintana, I., and Rodriguez, R. (2018). Design of nanostructured functional coatings by usingwet-chemistry methods. Coatings, 8.10.3390/coatings8020076 ↗
44. Effect of graphene oxide and fluorinated polymeric chains incorporated in a multilayered sol-gel nanocoating for the design of corrosion resistant and hydrophobic surfaces10.1016/j.apsusc.2017.05.043 ↗
45. Rivero, P.J., Yurrita, D., Berlanga, C., Fernandez-Palacio, J., and Rodríguez, R.J. (2018). Functionalized Electrospun Fibers for the Design of Novel Hydrophobic and Anticorrosive Surfaces. Coatings, 8.10.3390/coatings8090300 ↗
46. Laboratory Test for Ice Adhesion Strength Using Commercial Instrumentation10.1021/la4044254 ↗
47. Effect of wettability and surface roughness on ice-adhesion strength of hydrophilic, hydrophobic and superhydrophobic surfaces10.1016/j.apsusc.2014.06.101 ↗
48. Minimization of Ice Adhesion to Space Shuttle Component Surfaces10.1163/016942411X574619 ↗
49. A new method for measuring ice adhesion strength at an ice–substrate interface10.1002/hyp.6110 ↗
50. Fortin, G., Beisswenger, A., and Perron, J. (2010, January 2–5). Centrifuge adhesion tests to evaluate icephobic coatings. Proceedings of the AIAA Atmospheric and Space Environments Conference 2010, Toronto, ON, Canada.10.2514/6.2010-7837 ↗
51. Preparation of Water-Repellent Glass by Sol–Gel Process Using Perfluoroalkylsilane and Tetraethoxysilane10.1006/jcis.2000.7313 ↗
52. Structure and surface properties of fluorinated organic–inorganic hybrid films10.1007/s10971-011-2620-7 ↗
53. Development of water-repellent organic–inorganic hybrid sol–gel coatings on aluminum using short chain perfluoro polymer emulsion10.1016/j.apsusc.2013.07.066 ↗
54. Rivero, P.J., Maeztu, J.D., Berlanga, C., Miguel, A., Fernandez-Palacio, J., and Rodríguez, R.J. (2018). Hydrophobic and Corrosion Behavior of Sol-Gel Hybrid Coatings Based on the Combination of TiO2 NPs and Fluorinated Chains for Aluminum Alloys Protection. Metals, 8.10.3390/met8121076 ↗
55. Karmouch, R., Coudé, S., Abel, G., and Ross, G.G. (2009, January 22–23). Icephobic PTFE coatings for wind turbines operating in cold climate conditions. Proceedings of the 2009 IEEE Electrical Power and Energy Conference, EPEC, Montreal, QC, Canada.10.1109/EPEC.2009.5420897 ↗
56. Advanced Icephobic Coatings10.1163/016942410X533372 ↗
57. Physical Mechanisms Responsible for Ice Adhesion10.1021/jp9632145 ↗
58. Study of the Surface of Ice, Ice/Solid and Ice/Liquid Interfaces with Scanning Force Microscopy10.1021/jp963217h ↗
59. Superhydrophobic surfaces cannot reduce ice adhesion10.1063/1.4752436 ↗
60. Fortin, G., Adomou, M., and Perron, J. (2011). Experimental Study of Hybrid Anti-Icing Systems Combining Thermoelectric and Hydrophobic Coatings, SAE.10.4271/2011-38-0003 ↗