Abstract

The aim of the study is a comparative analysis of micromechanical and microtribological properties of the cathodic arc-deposited Mo, Cr, and Ta coatings using nanoindentation and scratch test techniques as well as a microtribological dry sliding test with wear tracks post-examination and worn volume determination using interference profilometry. A new scratch test technique based on the statistical processing of registered sclerograms during a multi-pass scratch test well adopted for the scratch resistance assessment of rough surfaces is suggested. New approaches to microtribological testing based on the indentation tester equipped with an additional precision rotational stage are proposed, which could fill the gap between macro- and nano-scale. X-ray diffraction analysis reveals the structure of the studied coatings and phase compositions of the coating-substrate interface.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Tribology and Wear Analysis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Aircraft Design, State University “Kyiv Aviation Institute”, 1, Liubomyra Huzara Ave, 03058 Kyiv, Ukraine

M. K. Yanhel State Design Bureau “Pivdenne”, 3 Kryvoriz’ka Street, 49008 Dnipro, Ukraine

G.V. Kurdyumov Institute for Metal Physics of the NAS of Ukraine, 36 Academician Vernadsky Boulevard, 03142 Kyiv, Ukraine

E.O. Paton Electric Welding Institute of the NAS of Ukraine, 11 Kazymyr Malevych Street, 03150 Kyiv, Ukraine

References (64)

Show source-provided references
1. Klesnil, M., and Lukás, P. (1992). Fatigue of Metallic Materials, Elsevier. [2nd ed.].
2. Component level strategies for exploiting the lifespan of steel in products10.1016/j.resconrec.2013.11.014 ↗
3. Strategies for enhancing fire performance of steel bridges10.1016/j.engstruct.2016.10.040 ↗
4. Improvement in tribocorrosion behavior of 304 stainless steel by surface mechanical attrition treatment10.1016/j.surfcoat.2014.05.057 ↗
5. Nanostructured surface layer on metallic materials induced by surface mechanical attrition treatment10.1016/j.msea.2003.10.261 ↗
6. Surface alloying of H11 die steel by tungsten using EDM process10.1007/s00170-014-6743-1 ↗
7. Improved fatigue behavior of low-carbon steel 20GL by applying ultrasonic impact treatment combined with the electric discharge surface alloying10.1016/j.msea.2016.02.036 ↗
8. Tantalum films for protective coatings of steel10.1016/j.tsf.2004.04.041 ↗
9. Effects of ultrasonic impact treatment combined with the electric discharge surface alloying by molybdenum on the surface related properties of low-carbon steel G21Mn510.1016/j.surfcoat.2016.10.050 ↗
10. Wear performance of laser processed tantalum coatings10.1016/j.msec.2011.08.017 ↗
11. Kou, Q., Jin, W., Ge, C., Pang, J., Zhang, J., Haarberg, G.M., Xiao, S., and Wang, P. (2023). Preparation of molybdenum coatings by molten salt electrodeposition in Na3AlF6-NaF-Al2O3-MoO3 system. Coatings, 13.10.3390/coatings13071266 ↗
12. Broitman, E., Jahagirdar, A., Rahimi, E., Meeuwenoord, R., and Mol, J.M.C. (2024). Microstructural, nanomechanical, and tribological properties of thin dense chromium coatings. Coatings, 14.10.3390/coatings14121597 ↗
13. Evaluation of cell activation promoted by tantalum and tantalum oxide coatings deposited by reactive DC magnetron sputtering10.1016/j.surfcoat.2017.10.019 ↗
14. Elevation of the Wear Resistance of Low-Alloy Structural Steel by Plasma-Powder Surfacing with Alloys Based on Iron, Chromium, and Nickel10.1007/s11003-018-0195-y ↗
15. Effects of surface treatments on the fatigue strength of AISI 4340 aeronautical steel10.1016/S0142-1123(01)00015-9 ↗
16. Influence of surface integrity on fatigue strength of 40CrNi2Si2MoVA steel10.1016/j.matlet.2006.04.089 ↗
17. Hard chrome coatings deposited by vapour deposition10.1016/0040-6090(83)90501-1 ↗
18. Effects of tungsten carbide thermal spray coating by HP–HVOF and hard chromium electroplating on AISI 4340 high strength steel10.1016/S0257-8972(00)01148-8 ↗
19. Influence of galvanization on the corrosion fatigue performance of high-strength steel10.1016/j.surfcoat.2014.10.049 ↗
20. Fatigue strength of chromium coated elements and possibility of its improvement with slide diamond burnishing10.1016/j.surfcoat.2008.12.022 ↗
21. Mechanisms of chromium carcinogenicity and toxicity10.3109/10408449309105012 ↗
22. Micromechanical, corrosion and wet sliding wear behaviours of Co-28Cr-6Mo alloy: Wrought vs. LPBF10.1016/j.mtcomm.2023.105936 ↗
23. Microstructural characterization and mechanical properties of additively manufactured molybdenum and molybdenum alloys10.1016/j.ijrmhm.2022.105971 ↗
24. Porous tantalum structures for bone implants: Fabrication, mechanical and in vitro biological properties10.1016/j.actbio.2010.01.046 ↗
25. Microstructural evolution and sintering kinetics during spark plasma sintering of pure tantalum powder10.1016/j.jallcom.2018.12.049 ↗
26. Fully dense and crack free molybdenum manufactured by selective laser melting through alloying with carbon10.1016/j.ijrmhm.2019.105000 ↗
27. Quantify strengthening and weakening factors in molybdenum fabricated by laser powder bed fusion (LPBF) with a revisit of its oxygen sensitivity10.1016/j.msea.2025.147856 ↗
28. Experimental Study of the Iron-Tantalum Equilibrium Diagram10.1007/BF02664849 ↗
29. Structural phase transition in the Fe–Ta system studied by ion beam mixing10.1016/j.jallcom.2008.09.128 ↗
30. Metastable crystalline phases formed in the Fe–Ta system by solid-state reaction10.1016/S0925-8388(99)00138-3 ↗
31. The Fe-Mo (Iron-Molybdenum) System10.1007/BF02869315 ↗
32. Phase structure of electrodeposited Fe-Mo Alloys from aqueous solution
33. Laser surface alloying of AISI 304-stainless steel with molybdenum for improvement in pitting and erosion–corrosion resistance10.1016/S0921-5093(99)00053-2 ↗
34. Microstructure and tribological properties of Fe-Mo alloy-coated steel specimens prepared by low-pressure plasma spraying10.1016/j.intermet.2011.08.003 ↗
35. Determination of diffusivity on W and Mo in double glow discharge
36. Effect of molybdenum on the microstructure and wear resistance of Fe-based hardfacing coatings10.1016/j.msea.2007.12.020 ↗
37. Tribological properties of Fe7Mo6-based-alloy lubricated with poly-alpha-olefin containing PN additive10.1016/j.triboint.2009.06.012 ↗
38. Friction and wear properties of Fe7Mo6-based alloy in ethyl alcohol10.1016/j.triboint.2010.06.011 ↗
39. Review of the filtered vacuum arc process and materials deposition10.1016/S0040-6090(01)01169-5 ↗
40. Erosion of a chromium-plated tank gun barrel10.1016/0043-1648(89)90250-0 ↗
41. Mattox, D.M. (2010). Handbook of Physical Vapor Deposition (PVD) Processing, Elsevier. [2nd ed.].10.1016/B978-0-8155-2037-5.00008-3 ↗
42. High-temperature solid particle erosion of Cr–Ni–Fe–C arc cladded coatings10.1016/j.wear.2020.203439 ↗
43. Prediction of phase composition and mechanical properties Fe–Cr–C–B–Ti–Cu hardfacing alloys: Modeling and experimental Validations10.1016/j.heliyon.2024.e25199 ↗
44. Holmberg, K., and Matthews, A. (2009). Coating Tribology: Properties, Mechanisms, Techniques and Applications in Surface Engineering, Elsevier.
45. Formation mechanism, microstructural features and dry-sliding behaviour of “Bronze/WC carbide” composite synthesised by atmospheric pulsed-plasma deposition10.1016/j.vacuum.2020.110031 ↗
46. Review of recent progress in nanoscratch testing10.1179/1751584X13Y.0000000037 ↗
47. Using a standard pin-on-disc tribometer to analyse friction in a metal forming process10.1016/j.triboint.2017.04.052 ↗
48. The current state-of-the-art in scratch testing of coated systems10.1016/j.surfcoat.2019.125092 ↗
49. Taylor, A. (1964). X-Ray Metallography, John Wiley & Sons.
50. Cathodic arc deposition technology10.1016/0257-8972(86)90001-0 ↗
51. Characterization of ZrN coating low-temperature deposited on the preliminary Ar+ ions treated 2024 Al-alloy10.1016/j.surfcoat.2018.12.010 ↗
52. Glass Fracture during Micro-Scratching10.3390/surfaces3020016 ↗
53. Instrumented indentation study of materials edge chipping10.1016/j.ceramint.2021.07.133 ↗
54. Coatings strength evaluation of cutting inserts using advanced multi-pass scratch method10.1016/j.measurement.2022.110745 ↗
55. Size effect in the micro- and nanoindentation and its compensation with regard for the specific features of initial contact10.1007/s11223-009-9116-5 ↗
56. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
57. (2002). Metallic Materials—Instrumented Indentation Test for Hardness and Materials Parameters. Part 1: Test Method (Standard No. ISO/FDIS 14577-1: 2002).
58. High cycle fatigue behavior and strengthening mechanisms of laser powder bed fusion pure tantalum10.1016/j.ijfatigue.2024.108624 ↗
59. Breakdown of the Hall-Petch relationship in extremely fine nanograined body-centered cubic Mo alloys10.1016/j.actamat.2021.116950 ↗
60. Effect of constrained inter-granular regions on the inverse Hall-petch phenomena10.1016/j.msea.2023.145125 ↗
61. The Influence of Polishing on the Mechanical Properties of Zirconia—A Systematic Review10.3390/oral3010010 ↗
62. Mechanical Characteristics of High-Entropy Alloys and Their Constituent Metals in Friction Conditions at Low Sliding Velocities10.1007/s11106-019-00077-w ↗
63. Dienwiebel, M., and De Barros Bouchet, M.I. (2018). Analyzing Mild- and Ultra-Mild Sliding Wear of Metallic Materials by Transmission Electron Microscopy. Advanced Analytical Methods in Tribology, Springer.10.1007/978-3-319-99897-8 ↗
64. Mordyuk, B.N., Voloshko, S.M., Zakiev, V.I., Burmak, A.P., Skoryk, M.A., Mohylko, V.V., Khripta, N.I., Malinin, V.Y., and Lesyk, D.A. (2024). Wear and Friction Performance of Alumina-Reinforced Composite Coating on Ti-6Al-4V Alloy Produced by Combining Ultrasonic Impact Treatment and Air-Oxidation. J. Mater. Eng. Perform.10.1007/s11665-024-09979-2 ↗