Review of the Mitigation Scale Performance of Anti-Fouling Coatings Surface Characteristics on Industrial Heat Exchange Surfaces
Source abstract
Abstract
Industrial heat exchangers are widely used in industries such as petrochemicals, energy and power, and food processing, making them one of the most important pieces of heat and mass transfer equipment in industry. During operation, a layer of fouling often adheres to the heat transfer surfaces, which reduces the heat transfer coefficient of the equipment and increases the thermal resistance of the surfaces. Additionally, fouling can corrode the material of the heat transfer surfaces, compromise their integrity, and even lead to perforations and leaks, severely impacting equipment operation and safety while increasing energy consumption and costs for enterprises. The application of anti-fouling coatings on surfaces is a key technology to address fouling on heat transfer surfaces. This paper focuses on introducing major types of anti-fouling coatings, including polymer-based coatings, “metal material + X”-type coatings, “inorganic material + X”-type coatings, carbon-based material coatings, and other varieties. It analyzes and discusses the current research status and hotspots for these coatings, elaborates on their future development directions, and proposes ideas for developing new coating systems. On the other hand, this paper summarizes the current research on the main factors—surface roughness, surface free energy, surface wettability, and coating corrosion resistance—that affect the anti-fouling performance of coatings. It outlines the research hotspots and challenges in understanding the influence of these three factors and suggests that future research should consider the synergistic effects of multiple factors, providing valuable insights for further studies in the field of anti-fouling coatings.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Calcium Carbonate Crystallization and Inhibition · Erosion and Abrasive Machining · Marine Biology and Environmental Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Mechanical and Electrical Engineering, Guangdong University of Petrochemical Technology, Maoming 525011, China
School of Energy and Power Engineering, Guangdong University of Petrochemical Technology, Maoming 525011, China
Funding
Teaching Quality and Teaching Reform Engineering Construction Project for Undergraduate Universities in Guangdong Province
References (88)
Show source-provided references
1. Technology Development of Large-scale Heat Exchanger in China10.3901/JME.2013.10.134 ↗
2. Fouling of Heat Exchangers–New Approaches to Solve an Old Problem10.1080/01457630590889906 ↗
3. Heat Exchanger Fouling, Environmental Impacts10.1080/01457630902744119 ↗
4. Organic fouling behavior of commercially available hydrocarbon–based anion–exchange membranes by various organic–fouling substances10.1016/j.desal.2012.04.010 ↗
5. Fouling in microstructured devices: A review10.1039/C4CC07849G ↗
6. Thinking about Heat Transfer Fouling, A 5 × 5 Matrix10.1080/01457638108939594 ↗
7. Modification of molecular interactions at the interface crystal/heat transfer surface to minimize heat exchanger fouling10.1016/S1290-0729(00)00229-5 ↗
8. Anti–silica fouling coatings in geothermal environments10.1016/S0167-577X(02)00851-0 ↗
9. Evaluation of heat exchanger surface coatings10.1016/j.applthermaleng.2009.12.013 ↗
10. Application of nano–modified surfaces for fouling mitigation10.1002/er.1599 ↗
11. Use of a sol–gel hybrid coating composed by a fluoropolymer and silica for the mitigation of mineral fouling in heat exchangers10.1016/j.applthermaleng.2016.06.014 ↗
12. Perfluoropolyethers coatings design for fouling reduction on heat transfer stainless–steel surfaces10.1080/01457632.2015.1044417 ↗
13. Anti–scale and anti–corrosion properties of PDA/PTFE superhydrophobic coating on metal surface
14. Effects of modified celatom and PDMS on antiscaling and corrosion resistance of epoxy coatings
15. Investigation of graded Ni–Cu–P–PTFE composite coatings with antiscaling properties10.1016/j.apsusc.2004.01.044 ↗
16. Preparation of Zn–Ni/PTFE composite coatings and their corrosion resistance and scale inhibition performance in simulated wastewater
17. Effect of surface free energy on the adhesion of biofouling and crystalline fouling10.1016/j.ces.2005.04.006 ↗
18. Tailored surface free energy of membrane diffusers to minimize microbial adhesion10.1016/j.apsusc.2004.02.052 ↗
19. Experimental fouling investigation with electroless Ni–P coatings10.1016/j.ijthermalsci.2009.05.009 ↗
20. Minimization of CaSO4 deposition through surface modification10.1080/01457632.2010.495628 ↗
21. Effect of the microstructure on the anti–fouling property of the electroless Ni–P coating10.1016/j.matlet.2008.07.002 ↗
22. Effect of phosphorus content on anti–fouling and anti–corrosion properties of electroless Ni–P deposition
23. Effect of copper addition on the properties of electroless Ni–Cu–P coating on heat transfer surface10.1007/s00170-014-6437-8 ↗
24. Experimental study on the anti–fouling effects of Ni–Cu–P–PTFE deposit surface of heat exchangers10.1016/j.applthermaleng.2014.04.003 ↗
25. Study on the effect of Ni–P–PTFE composite coating on the deposition characteristics of particulate fouling
26. The experimental investigation of cooling water microbial fouling characteristics on modified heat exchanger surface
27. Iron bacteria fouling and corrosion properties effect on modified surface of electroless Ni–P coating
28. Analysis of composite modified surface inhibiting particle fouling accumulation characteristics
29. Characteristics of microbial fouling on Ni–P–(nano)TiO2 composite coating of plate heat exchanger
30. Enhancing flow boiling and antifouling with nanometer titanium dioxide coating surfaces10.1002/aic.11150 ↗
31. Antifouling and enhancing pool boiling by TiO2 coating surface in nanometer scale thickness10.1002/aic.11345 ↗
32. Pool boiling fouling and corrosion properties on liquid–phase–deposition TiO2 coatings with copper substrate10.1002/aic.12405 ↗
33. CaCO3 fouling on microscale–nanoscale hydrophobic titania–fluoroalkylsilane films in pool boiling10.1002/aic.14015 ↗
34. Observations and mechanism of CaSO4 fouling on hydrophobic surfaces10.1021/ie402308m ↗
35. Fouling resistance on chemically etched hydrophobic surfaces in nucleate pool boiling10.1002/ceat.201400194 ↗
36. Antifouling and anticorrosion behaviors of modified heat transfer surfaces with coatings in simulated hot–dry–rock geothermal water10.1016/j.applthermaleng.2017.12.071 ↗
37. Fouling and Corrosion Properties of SiO2 Coatings on Copper in Geothermal Water10.1021/ie202091b ↗
38. Enhanced Heat Transfer and Fouling Propensity of DLC Coated Smooth and Finned Tubes during External Nucleate Boiling10.1115/1.4033210 ↗
39. Heat transfer surfaces coated with fluorinated diamond–like carbon films to minimize scale formation10.1016/j.surfcoat.2004.02.030 ↗
40. Preparation of anti–fouling heat transfer surface by magnetron sputtering a–C film on electrical discharge machining Cu surface10.1016/j.surfcoat.2019.03.075 ↗
41. Xu, Z., Sun, M., Liu, Z., Wang, B., and Di, H. (2020). Properties of the iron bacteria biofouling on Ni–P–rGO coating. Appl. Sci., 10.10.3390/app10051567 ↗
42. Mitigation of CaCO3 Fouling on heat exchanger surface using green functionalized carbon nanotubes (Gfcnt) coating10.1016/j.tsep.2023.101878 ↗
43. Performance evaluation of green synthesized graphene nanoplatelets–multiwall carbon nanotubes hybrid nanofluids for the retardation of mineral fouling and its environmental benefits10.1016/j.carbon.2025.120243 ↗
44. He, Z., Wang, D., Fan, Z., Chen, Y., Li, S., and Mo, C. (2020). Fabrication of Fe–Al coatings with micro/nanostructures for antifouling applications. Coatings, 10.10.3390/coatings10090902 ↗
45. Investigation of zirconium (Zr) coated heat exchanger surface for the enhancement of heat transfer and retardation of mineral fouling10.1016/j.jtice.2023.105246 ↗
46. Heat transfer and fouling deposition investigation on the titanium coated heat exchanger surface10.1016/j.powtec.2020.07.010 ↗
47. Ultrahigh resistance of hexagonal boron nitride to mineral scale formation10.1038/s41467-022-32193-4 ↗
48. Surface lurking and interfacial ion release strategy for fabricating a superhydrophobic coating with scaling inhibition10.1016/j.petsci.2022.07.005 ↗
49. EDTA interfacial chelation Ca2+ incorporates superhydrophobic coating for scaling inhibition of CaCO3 in petroleum industry
50. Modified stainless steel surfaces targeted to reduce fouling–surface characterization10.1016/j.jfoodeng.2003.09.013 ↗
51. Effect of Surface Roughness on the morphology of calcite crystallizing on mild steel10.1006/jcis.1994.1044 ↗
52. Experimental observation of surface morphology effect on crystallization fouling in plate heat exchangers10.1016/j.icheatmasstransfer.2010.10.006 ↗
53. Influence of surface properties and characteristics on fouling in plate heat exchangers10.1080/01457630590897024 ↗
54. Influence of heat transfer surface characteristics on fouling induction period
55. Investigation of adhesion of CaCO3 crystalline fouling on stainless steel surfaces with different roughness10.1016/j.icheatmasstransfer.2011.04.003 ↗
56. Adhesion of single crystals on modified surfaces in crystallization fouling10.1016/j.jcrysgro.2012.09.032 ↗
57. Composition analysis and kinetic modeling of crystallization fouling in cooling seawater
58. Hydrophobic bacteria–repellant graphene coatings from recycled pencil stubs10.1007/s13369-017-2901-8 ↗
59. Corrosion and fouling behaviors on modified stainless steel surfaces in simulated oilfield geothermal water10.1134/S2070205118030322 ↗
60. Corrosion and fouling behaviours of copper–based superhydrophobic coating10.1080/02670844.2018.1433774 ↗
61. Strategy for fabricating degradable low–surface–energy cross–linked networks with excellent anti–fouling properties10.1021/acsami.4c19192 ↗
62. A criterion for the characterization of modified surfaces during crystallization fouling based on electron donor component of surface energy10.1016/j.cherd.2015.05.033 ↗
63. Innovative non–metal heat transfer surfaces to mitigate crystallization fouling10.1016/j.ijthermalsci.2019.01.003 ↗
64. Field evaluation of coated plates of a compact heat exchanger to mitigate crystallization deposit formation in an MD desalination plant10.1016/j.desal.2013.05.020 ↗
65. Tailored surface energy of stainless steel plate coupons to reduce the adhesion of aluminium silicate deposit10.1016/j.fuel.2016.04.105 ↗
66. Composite fouling characteristics on Ni–P–PTFE nanocomposite surface in corrugated plate heat exchanger10.1080/01457632.2020.1834202 ↗
67. The CQ ratio of surface energy components influences adhesion and removal of fouling bacteria10.1080/08927014.2011.563842 ↗
68. Impact of tube surface properties on crystallization fouling in falling film evaporators for seawater desalination
69. Engineering nanoscale roughness on hydrophobic surface–preliminary assessment of fouling behaviour10.1016/j.stam.2005.03.003 ↗
70. Adhesive behavior of a calcium carbonate particle to solid walls having different hydrophilic characteristics10.1016/j.ijheatmasstransfer.2015.08.068 ↗
71. Fabrication of superhydrophobic micro–nano structure Al2O3–13% TiO2/PTFE coating with anti–fouling and self–cleaning properties10.1016/j.surfin.2020.100559 ↗
72. Characterization of water–based anti–corrosion and anti–fouling coating in the heat exchanger tube of gas water heater
73. Jiang, H., Sun, N., Ju, Y., Li, J., and Chen, Z. (2023). Study on the effect of surfaceproperties of non–metallic materials on the growth mechanism of crystallization fouling. Processes, 11.10.3390/pr11082232 ↗
74. Enhanced pool boiling of ethanol on wettability–patterned surfaces10.1016/j.applthermaleng.2018.12.049 ↗
75. Enhancement of pool boiling heat transfer by laser texture–deposition on copper surface10.1016/j.apsusc.2024.160015 ↗
76. Modeling of CaSO4 crystallization fouling of finned tubes during nucleate pool boiling10.1016/j.cherd.2016.11.030 ↗
77. Experimental study on the anti–fouling effects of EDM machined hierarchical micro/nano structure for heat transfer surface10.1016/j.applthermaleng.2019.114248 ↗
78. Wettability–driven synergistic resistance of scale and oil on robust superamphiphobic coating10.1016/j.cclet.2024.109623 ↗
79. Sustainable scale resistance on a bioinspired synergistic microspine coating with a collectible liquid barrier10.1039/D2MH00933A ↗
80. Scalable and robust bio–inspired organogel coating by spraying method towards dynamic anti–scaling10.1007/s40242-022-2094-x ↗
81. Effect of the microstructure on the properties of Ni–P deposits on heat transfer surface10.1016/j.surfcoat.2008.10.039 ↗
82. Effect of surface modification onanti-fouling properties of heat exchangers
83. Corrosion and fouling of different coatings in geothermal water
84. Effect of surface roughness on mixed salt crystallization fouling in pool boiling10.5004/dwt.2022.28924 ↗
85. Heat transfer characteristics of pool boiling with scalable plasma–sprayed aluminum coatings10.1021/acs.langmuir.2c03436 ↗
86. Hierarchical micro/nano structure surface fabricated by electrical discharge machining for anti–fouling application10.1016/j.jmrt.2019.06.051 ↗
87. Investigation of induction period and morphology of CaCO3 fouling on heated surface10.1016/S0009-2509(02)00007-6 ↗
88. Induction time in crystallization fouling on heat transfer surfaces10.1002/ceat.201000469 ↗