High Temperature Oxidation of Enamel Coated Low-Alloyed Steel 16Mo3 in Water Vapor
Source abstract
Abstract
New types of ceramic coatings based on SiO2-Na2O-B2O3-TiO2 oxide phases were investigated as protection for boiler steel in power generation systems. Low-alloyed Cr-Mo 16Mo3 steel was coated with different compositions of enamel coatings to assess the protective potential of these coatings under water vapor at high temperatures. Oxidation at 650 °C for 50 h in Ar + water vapor was performed in a TGA apparatus to investigate the oxidation kinetics. The results indicate that the ceramic coatings provided a high degree of protection for the steel exposed to such conditions compared to the uncoated 16Mo3 steel. Furthermore, despite the formation of cracks in the coatings, no spallation from the steel surface was observed. Interconnected porosity in the coatings is suspected to provoke interfacial degradation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Laboratoire des Sciences de l’Ingénieur pour l’Environnement, Université de La Rochelle LaSIE, UMR-CNRS 7356, Avenue Michel Crépeau, CEDEX 1, 17042 La Rochelle, France
Centre for Corrosion Studies, Łukasiewicz Research Network—Krakow Institute of Technology, 73 Zakopiańska St., 30-418 Krakow, Poland
Funding
Campus France- Nawa Poland exchange program “Polonium” · Ministry of Higher Education in Poland, in the internal project in Łukasiewicz—Krakow Institute of Technology
References (35)
Show source-provided references
1. Corrosion Behavior of T24, T92, VM12, and AISI 304 Steels Exposed to KCl–NaCl–K2SO4–Na2SO4 Salt Mixtures10.1002/maco.202012139 ↗
2. Sulfidation of Ceramic-Based Coatings Deposited on Low-Alloyed Steel 16Mo3 Exposed at High Temperature10.1007/s11665-021-06070-y ↗
3. Steam Oxidation Resistance of Slurry Aluminum and Aluminum/Silicon Coatings on Steel for Ultrasupercritical Steam Turbines10.1007/s11085-017-9726-4 ↗
4. Steam Oxidation of Aluminide Coatings under High Pressure and for Long Exposures10.1016/j.corsci.2018.08.053 ↗
5. A Review of Thermal Spray Coatings for Protection of Steels from Degradation in Coal Fired Power Plants10.1515/corrrev-2020-0043 ↗
6. Combating Hot Corrosion of Boiler Tubes—A Study10.1016/j.engfailanal.2018.08.004 ↗
7. Resistance of Coatings for Boiler Components of Waste-to-Energy Plants to Salt Melts Containing Copper Compounds10.1007/s11666-013-9908-9 ↗
8. KCl-Induced High-Temperature Corrosion Behavior of HVAF-Sprayed Ni-Based Coatings in Ambient Air10.1007/s11666-017-0684-9 ↗
9. Fireside Corrosion Degradation of Ferritic Alloys at 600 °C in Oxy-Fired Conditions10.1016/j.corsci.2013.11.005 ↗
10. Beyond Traditional Coatings: A Review on Thermal-Sprayed Functional and Smart Coatings10.1007/s11666-019-00857-1 ↗
11. Ceramic Coatings for High-Temperature Protection of Steel10.6028/jres.038.014 ↗
12. Review of Ceramic Coating on Mild Steel Methods, Applications and Opportunities
13. Advanced Ceramic Coatings on Stainless Steel: A Review of Research, Methods, Materials, Applications and Opportunities
14. Laser-Induced Deposition of Alumina Ceramic Coating on Stainless Steel from Dry Thin Films for Surface Modification10.1016/j.ceramint.2013.11.067 ↗
15. Plasma-Sprayed Oxide Ceramics on Steel Substrates10.1016/S0257-8972(97)00223-5 ↗
16. Performance of Thermal Barrier Coatings in Industrial Gas Turbine Conditions10.3184/096034011X13188765758098 ↗
17. High Temperature Oxidation and Corrosion of Gas Turbine Component Materials in Burner Rig Exposures10.3184/096034011X13198126967382 ↗
18. EB-PVD Thermal Barrier Coatings for Aeroengines and Gas Turbines10.1002/1527-2648(200104)3:4<193::AID-ADEM193>3.0.CO;2-U ↗
19. The Use of APS Thermal Barrier Coatings in Corrosive Environments10.1007/s11085-017-9728-2 ↗
20. Thermal Shock Characteristics of Plasma Sprayed Mullite Coatings10.1361/105996398770350710 ↗
21. A Novel Method of Preparation of Metal Ceramic Coatings10.1016/j.jmatprotec.2008.06.017 ↗
22. Calculations of Parabolic Reaction Rate Constants10.1007/BF00667057 ↗
23. Degradation of Glass Linings and Coatings
24. Functional Corrosion-Resistant Enamel Coatings and Their Adherence Strength10.12693/APhysPolA.121.178 ↗
25. Glass Coatings on Stainless Steels for High-Temperature Oxidation Protection: Mechanisms10.1016/j.corsci.2014.01.033 ↗
26. Durability of Vitreous Enamel Coatings and Their Resistance to Abrasion, Chemicals, and Corrosion: A Review10.1007/s11998-020-00415-3 ↗
27. Prediction of Residual Stress and Deformation of Enameled Steel10.1007/s12541-015-0216-9 ↗
28. High Temperature Corrosion of Low Alloyed Steel in Air and Salt Mist Atmospheres
29. Corrosion Products and Formation Mechanism during Initial Stage of Atmospheric Corrosion of Carbon Steel10.1016/S1006-706X(08)60247-2 ↗
30. Thermodynamics of Fe Oxides: Part II. Enthalpies of Formation and Relative Stability of Goethite (α-FeOOH), Lepidocrocite (γ-FeOOH), and Maghemite (γ-Fe2O3)10.2138/am-2003-5-614 ↗
31. Study on Magnetite Oxidation Using Synchrotron X–Ray Diffraction and X–Ray Absorption Spectroscopy: Vacancy Ordering Transition in Maghemite (γ–Fe2O3)10.2465/jmps.210304 ↗
32. Corrosion Protection of 13CrMo 44 Heat-Resistant Ferritic Steel by Silicon and Cerium Ion Implantation for High-Temperature Applications
33. Ahmad, Z. (2016). Steam Oxidation of Fe-Based Materials High Temperature Corrosion, IntechOpen.
34. Mysen, B.O., and Richet, P. (2005). Silicate Glasses and Melts: Properties and Structure, Elsevier.
35. The Oxidation Behaviour of Metals and Alloys at High Temperatures in Atmospheres Containing Water Vapour: A Review10.1016/j.pmatsci.2007.11.001 ↗