Abstract

Fe-based coatings with high V and Cr content were obtained by laser cladding using Fe-based powder with different Cr3C2 and FeV50 content. The results showed that Fe-based coatings were uniform and dense. The constituent phases were mainly composed of α-Fe solid solution with the increase of Cr3C2 and FeV50, γ-Fe and V8C7 phases were achieved. The microstructure of the coatings exhibited a typical dendrite structure. The concentration of C, V and Cr were saturated in dendritic areas, and the other alloying elements were mainly dissolved in the interdendritic areas. The hardness and wear resistance of Fe-based coatings were enhanced with the Cr3C2 and FeV50 addition. The specimen with 15% Cr3C2 and 16% FeV50 had the highest hardness of 66.1 ± 0.6 HRC, which was 1.05 times higher than the sample with 4.5% Cr3C2 and 5% FeV50, and the wear resistance of the former was three times greater than the latter.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China

Shenyang Dalu Laser Technology CO., Ltd., Shenyang 110136, China

School of Stomatology, China Medical University, Shenyang 110002, China

References (43)

Show source-provided references
1. Efficiency improvement in automobile bucket tappet/camshaft contacts by DLC coatings—Influence of engine oil, temperature and camshaft speed10.1016/j.surfcoat.2016.09.041 ↗
2. Fracture analysis of a camshaft made from nodular cast iron10.1016/j.engfailanal.2005.11.001 ↗
3. Laser cladding of NiCrSiB on Monel 400 to enhance cavitation erosion and corrosion resistance
4. He, Y.Z., Zhang, J.L., Zhang, H., and Song, G.S. (2017). Effects of different levels of boron on microstructure and hardness of CoCrFeNiAlxCu0.7Si0.1By high-entropy alloy coatings by laser cladding. Coatings, 7.10.3390/coatings7010007 ↗
5. Damm, D.D., Contin, A., Barbieri, F.C., Trava-Airoldi, V.J., Barquete, D.M., and Corat, E.J. (2017). Interlayers applied to CVD diamond deposition on steel substrate: A review. Coatings, 7.10.3390/coatings7090141 ↗
6. He, B., Zhang, N.N., Lin, D.Y., Zhang, Y., Dong, F.Y., and Li, D.Y. (2017). The phase evolution and property of FeCoCrNiAlTix high-entropy alloying coatings on Q253 via laser cladding. Coatings, 7.10.3390/coatings7100157 ↗
7. Fang, L.Y., Yan, H., Yao, Y.S., Zhang, P.L., Gao, Q.S., and Yang, Q. (2018). Reactive fabrication and effect of NbC on microstructure and tribological properties of CrS Co-based self-lubricating coatings by laser cladding. Materials, 11.10.3390/ma11010044 ↗
8. Wang, K.M., Chang, B.H., Lei, Y.P., Fu, H.G., and Lin, Y.H. (2017). Effect of cobalt on microstructure and wear resistance of Ni-based alloy coating gabricated by laser cladding. Metals, 7.10.3390/met7120551 ↗
9. Biswas, S., Alavi, S.H., and Harimkar, S.P. (2017). Effect of laser remelting and simultaneous application of ultrasonic vibrations during laser melting on the microstructural and tribological properties of laser clad Al-SiC composites. J. Compos. Sci., 1.10.3390/jcs1020013 ↗
10. Zhuang, Q.Q., Zhang, P.L., Li, M.C., Yan, H., Yu, Z.S., and Lu, Q.H. (2017). Microstructure, wear resistance and oxidation behavior of Ni-Ti-Si coatings fabricated on Ti6Al4V by laser cladding. Materials, 10.10.3390/ma10111248 ↗
11. Wang, K.M., Chang, B.H., Chen, J.S., Fu, H.G., Lin, Y.H., and Lei, Y.P. (2017). Effect of molybdenum on the microstructures and properties of stainless steel coatings by laser cladding. Appl. Sci., 7.10.3390/app7101065 ↗
12. Zhang, L., Wang, C.S., Qian, S.N., Yu, Q., and Chuang, Q. (2017). Microstructure and wear resistance of laser-clad (Co., Ni)61.2B26.2Si7.8Ta4.8 coatings. Metals, 7.10.3390/met7100419 ↗
13. Chen, Y.X., Guo, Y.B., Lu, B.F., Xu, M.J., and Xu, J.H. (2017). Microstructure and properties of the interface area in the laser cladded Ni based coatings on the 1Cr10Mo1NiWVNbN steel. Metals, 7.10.3390/met7050175 ↗
14. Multi-layer functional graded stainless steel fabricated by laser melting deposition10.1016/j.vacuum.2017.04.020 ↗
15. Yao, H.H., Zhou, Z., Wang, L., Tan, Z., He, D.Y., and Zhao, L.D. (2017). Thermal conductivity and wear behavior of HVOF-sprayed Fe-based amorphous coatings. Coatings, 7.10.3390/coatings7100173 ↗
16. Evolution of the structure and strength of steel/vanadium alloy/steel hybrid material during severe plastic deformation10.1016/j.matlet.2016.03.044 ↗
17. Li, Y.S., Zhu, L.H., Liu, C.W., and Shi, S.J. (2017). Nanoscale phase evolution during continuum decomposition of Fe-Cr alloys. Materials, 10.10.3390/ma10121431 ↗
18. Huang, C.A., Chen, J.Y., Wang, H., and Lai, P.L. (2017). Anneal-hardening behavior of Cr-Fe-C alloy deposits prepared in a Cr3+-based bath with Fe2+ ions. Materials, 10.10.3390/ma10121392 ↗
19. Magnetic properties of bulk and thin film Cr–Al–C compounds10.1179/1743294415Y.0000000103 ↗
20. Electrochemical characterization of multilayer Cr/CrN-based coatings10.3390/coatings4030508 ↗
21. Structural and mechanical properties of (Cr, Ni) N single and gradient layer coatings deposited on mild steel by magnetron sputtering
22. Research on microstructure, mechanical and tribological properties of Cr-Ti-B-N films10.3390/coatings7090137 ↗
23. Microstructure and mechanical properties of Mo2FeB2 ceramic-steels with Nb/V addition10.1080/17436753.2016.1251049 ↗
24. Influence of carbides morphology on the mechanical properties for Fe-C-V alloys10.1080/13640461.2016.1142234 ↗
25. The effect of vanadium micro-alloying on the microstructure and the tensile behavior of TWIP steel10.1016/j.msea.2017.04.083 ↗
26. Effect of a small addition of Ti on the Fe-based coating by laser cladding10.1016/j.surfcoat.2016.03.015 ↗
27. The solidification characteristics of laser surface-remelted Fe-12Cr-nC alloys10.1007/s11661-999-0180-z ↗
28. Chang, G.W. (2002). Crystal Growth and Control during Solidification of Metal, Metallurgical Industry Press. (In Chinese).
29. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
30. Calculation for grain growth rate of carbon steels by solute drag model considering segregation effect of each substitutional element10.1179/1743284710Y.0000000016 ↗
31. Decomposition modes of austenite in Cr Mo ferritic steels10.1016/S0022-3115(96)00397-2 ↗
32. Microstructural and abrasion wear characteristics of laser-clad tool steel coatings10.1080/02670844.2016.1180496 ↗
33. Laser cladding of Mg20Al80 powder on ZM5 magnesium alloy10.1179/174327807X196852 ↗
34. Mechanical properties of solid solution strengthened CGI10.1080/13640461.2015.1106781 ↗
35. Effect of particle size on wear behavior of Al–garnet composites10.1080/02726351.2014.954686 ↗
36. Mechanical properties of Cu2O thin films by nanoindentation10.3390/ma6104505 ↗
37. Hall–Petch behaviour of 316L austenitic stainless steel at room temperature10.1179/026708301125000384 ↗
38. Grain refinement and strengthening of a Cu–0.1Cr–0.06Zr alloy subjected to equal channel angular pressing10.1080/14786435.2017.1324649 ↗
39. Phase evolution and properties in laser surface alloying of FeCoCrAlCuNix high-entropy alloy on copper substrate10.1016/j.surfcoat.2017.02.068 ↗
40. Wear performance of TiC/Fe cermet electrical discharge coatings10.1016/j.wear.2018.02.007 ↗
41. Annealing effect on wear resistance of nanostructured 316L stainless steel subjected to dynamic plastic deformation10.1016/S1005-0302(12)60145-5 ↗
42. Importance and role of grain size in free surface cracking prediction of heavy forgings10.1016/j.msea.2014.12.022 ↗
43. Different aspects of the role of wear debris in fretting wear10.1016/S0043-1648(02)00044-3 ↗